WELD VISUAL IMAGES:-H SUPPORT 1)

SPATTER, POROSITY, BAD WELD VISUAL

POROSITY

2)

WELDING BALANCE

WELDING BALANCE

WELDING BALANCE

3)

POROSITY, SPATTER, BAD WELD VISUAL

POROSITY

POROSITY, SPATTER

SPATTERS, LACK OF PROPER CLEANING

INCOMPLETE WELD

POST WELD CLEANING BALANCE

Summary: Lack of improper inter run cleaning and slag removal has resulted into bad weld Visual Porosity, spatters are clearly visible Due to lack of inter run cleaning & Post weld cleaning has resulted into porosity & spatter Angle welding is not complete. Excessive spatter is seen