Paint & Painting Defects

IMPACT DAMAGE
2

RUST SPOTTING
3

PINHOLES

PINHOLES

SOLVENT POPPING
6

CRATERING

WRINKLING
8

SOLVENT ATTACK
9

MUD CRACKING
10

SOLVENT ATTACK
11

FLOTATION

12

DRY SPRAY

13

ADHESION FAILURE
14

INCORRECT COATING SYSTEM (HOT SURFACE)


15

INCORRECT COATING SYSTEM (BITUMEN SURFACE)


16

BLISTERING
17

CISSING
18

BLISTERING

19

SEVERE BLISTERING
20

OVER THINNING (LEADS TO BUBBLING)


21

RUST NODULES
22

SURFACE CONTAMINATION PRIOR TO PAINTING


23

DELAMINATION (INTERCOAT FAILURE)


24

RUST STAINING (T.S.A)


25

CORROSION DUE TO LOW DFT


26

ADHESION FAILURE (UNTREATED GALAVANISING)


27

POOR OPACITY
28

CHECKING
29

CHALKING

30

INTERCOAT ADHESION FAILURE


31

INCOMPATIBLE PAINTING SYSTEMS


32

ADHESION FAILURE (SALT CONTAMINATION)


33

CHECKING

34

BITTINESS (ALSO CALLED SEEDYNESS, PEPPERING)


35

ADHESION FAILURE (TSA)


36

OVER APPLICATION (PINHOLES ORANGE PEEL)


37

RUNS & SAGS (OVER APPLICATION)


38

MISSES & SKIPS (LEADS TO RUST STAINING)


39

METAL CONTAMINATION OF PAINT SURFACE


40

RUST STAINING
41

BLISTERING
42

CHALKING
43

CHALKING (ULTRA VIOLET LIGHT ATTACK)


44

BLOOMING (MOISTURE ATTACK)


45

PINHOLES

46

ACID ATTACK

47

CORROSION UNDER FIRE PROTECTION


48

ORANGE PEEL (VISCOSITY & TECHNIQUE PROBLEM)


49

OVER THINNING (RUNS & SAGGING)


50

FLOCCULATION
51

GRINNING (SHOWING THROUGH, POOR OPACITY)


52

RIPPLED COATING
53

WATER SPOTTING (DURING APPLICATION)


54

SETTLEMENT
55

LOW DFT (UNEVEN COATING, HIGH PEAKS)


56