Professional Documents
Culture Documents
FS-Wood Seal-B
FS-Wood Seal-B
SSP Tower3, 14 Fl. Unit A3, 88 Silom Rd., Suriyawong Bangrak Bangkok 10500
Tel: (66)2-634-4005 Fax: (66)2-634-4199 Email: sale@robergeandco.co.th www.robergeandco.co.th
EXTERIOR - If the wood surface will be exposed to water - a non- Volatility: Non-Volatile (Contains no VOC's)
flammable paint or coating* should be applied as a top coat after Water (Contains no petroleum
Wood Seal™ has dried. Solvents:
derivatives)
Bacteria
* Make sure that a paint or coating is not flammable, and does Mildly resistant
Resistance:
not negatively effect the fire resistant properties of the Flame
Seal product. Linear Shrinkage: None
Moisture
None
Absorption:
SPOT TEST SECTION: Corrosive: Mildly, none when dry
1. WOOD TO BE TESTED MUST BE UNTREATED, UNPAINTED, CLEAN AND DRY.
2. BRUSH, ROLL, OR SPRAY BOTH SIDES OF WOOD SAMPLE IF POSSIBLE. APPLY AMPLE WOOD SEAL TO SATURATE THE WOOD.
3. USE PRODUCT IN AREA WITH ADEQUATE VENTILATION.
4. ALLOW TIME TO DRY.
5. TEST BURN WITH A FLAME OR TORCH TO CHECK THAT THE WOOD DOES NOT CONTINUE TO BURN WHEN THE FLAME IS
REMOVED.
*** ( NOTE: THE CHEMICAL MUST BE USED IN ITS " UNDILUTED" STATE. ) ***
WOOD TREATMENT:
APPLY WOOD SEAL FLAME RETARDANT TO THE WOOD BY SAME METHOD AS THE SUCCESSFULLY TESTED SAMPLE.
COVERAGE RATE SHOULD BE 150 - 350 SQUARE FEET PER GALLON.
ALLOW WOOD SEAL TO DRY.
EXTERIOR - IF THE WOOD SURFACE WILL BE EXPOSED TO WATER - A NON-FLAMMABLE PAINT OR COATING SHOULD BE
APPLIED AS A TOP COAT AFTER Wood Seal™ HAS DRIED.