How do you increase solid content EVA in PPD solution?

Hello Everyone,
Can anyone suggest me an idea how can I increase the solid content of EVA while
dissolving into 2-ethyl-1 -Hexanol.
Previously, I successfully prepared a solution of Pour Point Depressant of EVA (
cloudy) by this procedure.
1) 10g of EVA (12% of VA) heated with 80g of 2-ethyl-1 -Hexanol at temperature 1
20C for about 1H and with speed of 750 rpm (clear solution)
2) Increase into high speed while cooling process into room temperature
This procedure has been repeated with increase the amount of EVA but the solutio
n become solid/gel while cooling.
Should I introduce any surfactant for this solution so the droplet can be stabil
ize?