Kovar is an alloy composed primarily of iron and nickel, with additions of manganese, cobalt, and silicon. It has a density of 8.359 g/cc and melts at 1450°C. The document provides various thermal, electrical, mechanical and magnetic properties of Kovar.
Kovar is an alloy composed primarily of iron and nickel, with additions of manganese, cobalt, and silicon. It has a density of 8.359 g/cc and melts at 1450°C. The document provides various thermal, electrical, mechanical and magnetic properties of Kovar.
Copyright:
Attribution Non-Commercial (BY-NC)
Available Formats
Download as DOC, PDF, TXT or read online from Scribd
Kovar is an alloy composed primarily of iron and nickel, with additions of manganese, cobalt, and silicon. It has a density of 8.359 g/cc and melts at 1450°C. The document provides various thermal, electrical, mechanical and magnetic properties of Kovar.
Copyright:
Attribution Non-Commercial (BY-NC)
Available Formats
Download as DOC, PDF, TXT or read online from Scribd
Density 8.359g/cc Melting point 1450°C Thermal conductivity 0.0395cal/sec/cm/°C at 30°C 0.0485 cal/sec/cm/°C at 300°C Specific heat 0.105 cal/g/°C at 0°C 0.155 cal/g/°C at 430°C Curie point 435°C Linear thermal expansion 6.19 in/in/°C Electrical Resistivity 49 μΩcm Maximum elongation 35.4% Modulus of elasticity 20*10-6Psi Tensile strength 77500Psi (21°C) Yield strength 59500 Psi (21°C) Magnetic permeability 3700 max at 7000 gauss Vapour pressure -