Inspection Cretira for SS316 Backing Ring

(1) All inside and outside surfaces must be checked 100% before shipment.
(2) All the casting surface must be free of yellowish stain left by washing liquid after
machining.
(3) Porosity holes must not be bigger than 0.5 mm. we will follow Table 1.0 for inspection of
porosity holes.

(4) Other part of the enclosure surface will be inspected with our surface finish guide.
(5) The following are the examples of Acceptable and reject samples.

Fig. 2 - Accepted
because dent is
at the corner.
Fig. 1 - Accepted
because Porosity
like holes are very
small and shallow.

Fig.3 - Accepted
because a small
bump.

Fig.4 - Accepted because only


one dent and other areas are
perfect.

Fig. 5 -Accepted because only a


bump and other areas are
perfect.

Fig.6 -Accepted
because only one
material excess at
the corner.

Fig.8 Rejected
because dent line
is too long.

Fig.9 Rejected
because too many
small dents and
looks ugly.

Fig.10 Rejected because


More than one porosity
holes, porosity holes are
bigger than 0.5 mm.