You are on page 1of 18

Aluminum Die Castings Surface Finished Requirements

Dimentional Tolerance

Dimension
.x one decimal
.xx two decimal
Special
angles

Tolerance
1.27 mm
0.51 mm
0.2 mm
2

(1) No burrs or sharp edges allowed anywhere on the castings.


(2) Ejector pin marks and Flash pin marks are not allowed.

(3) Cracks, cold lap, cold flow, nonfills, solder build-up and drag marks are not
acceptable.

(4) Surface Voids or Holes are not acceptable

(5) Discontinuities in Threaded Area are not acceptable.

(6) Rough and Dent surfaces are not acceptable

Surface is
not
smooth

Surface is
not
smooth
(7) Parting Lines/Gates - Voids, pinholes and breakout along the parting lines
and gates are unacceptable.

Cracks are
not
acceptable

Voids are
not
acceptable

(8) Uneven surfaces are not acceptable.

Breakout and
pinholes are not
acceptable