411 (AISI M2 Tool Steel) Composition: 0.95% C - 0.24% Mn - 0.28% Si ~ 0.018% S - 0.006% P - 4.64% Cr - 4.80% Mo - 2.45% V - 7.12% W Grain size: 9-10 Austenitized at 1280°C (2246°F) Acy = 824° ICINESH Eee om BH Hi A=" Jo vo|_| rT oe eee ude rrldaare ence 0D a EOE - me 113 (SAE 4340) Composition: 0.43% C - 0.49% Mn - 0.38% Si - 0.008% S$ - 0.02% P - 1.51% Ni - 1.10% Cr - 0.88% Mo Grain size: 9-10 Austenitized at 830°C (1526°F) for 15 min raat Bae my 1 Hore 7 a I vy 1 Tyr Tre Tl A Tay : SEL Pr 4 | +P Wil] @ Aca = 721°C I HH i § 9 i TN Th TE Nd Acg = 776°C =] rth FRA a wee seat * ee + rr eee urd 6 raualienement ete 00041 S00'C - min SAE 9840 Steel Composition: 0.43% © ~ 0.84% Mn ~ 0.25% 0.81% Cr - 0.23% Mo Grain size: 7 Austenitized at 846°C (560°F) 160% 1800 1400) 1300] 1200 tooe Gooling Curves » at Indicated Distances From Quenched End Tempercture®F A- Austenite M- Martensite Fp- Poroferrite 300} 8. Bainite Austenitized af 1550°F — Grain Size 7 200 ' es ase 810 1 2930 so OO 200) Gaoling Time From 1550°F - Seconds Type: 4340 Composition: Fe - 0.42% GC - 0.78% Mn - 1.79% Ni - 0.80% Cr - 0.33% Mo Grain size: 7-8 Austenitized at 843°C (1550°F) °c, °F, 200] 1200) 600] w 1000] © soo} = 800] & 400] © 00} so 200|- 400 tool- 200} ° 12 510 A Bo foawonessae @ 3 se aa so I-T DIAGRAM 108 TIME — SEGONDS. xlo2 105 to* TEMPER H13 Tool Steel Composition: 0.40% C - 1.089% Si - 5.0056 ‘Gr ~ 1.35% Mo - 1.10% V Austenitived at 1010°C (1850°F) oe Cp py - £ Le- #°) Guoxnere to view oe T 7 CHE } My Re { TREK [| 4) Hae} 1 Iadet secows

You might also like