COROZION CLASSES

Category of corrosion
C 1 = Internal dry
C 2 = Continental rural areas
C 3 = Continental or temperate coastal urban areas
C 4 = Continental and coastal urban industrial areas
C 5 = Industrial areas with high humidity or high salinity coastal areas.

CLASE DE COROZIVITATE

CATEGORII DE COROZIVITATE
C 1 = Interior uscat
C 2 = Interior condensare ocazionala. Exterior: rural
C 3 = Interior umiditate ridicata, usoara poluare a aerului. Exterior: mediu urban de uscat,
sau in apropierea coastei marine
C 4 = Interior: bazine cu apa, uzine chimice. Exterior: zone industriale de uscat sau coaste
marine
C 5 = Exterior: zone industriale cu umiditate crescuta sau sau coaste marine cu salinitate
ridicata
ON CLASSES

The average loss in thickness of zinc (μm / year)


Up to 0,1
From 0,1 to 0,7
From 0,7 to 2
From 2 to 4
From 4 to 8

COROZIVITATE

VITEZA MEDIE ANUALA DE COROZIUNE A


ZINCULUI (μm / an)
< 0,1
0,1 la 0,7

0,7 la 2

2 la 4

4 la 8