When manual metal arc welding low carbon steel, which electrode covering will give the
greatest degree of penetration?
a. Iron powder.
b. Rutile.
c. Cellulosic.
d. Low hydrogen
Tig
When TIG welding austenitic stainless steel pipe, argon gas backing is called for. This is to:
a. Prevent oxidation
b. Prevent underbead cracking
c. Prevent porosity
d. Control the penetration bead shape
. Inherent rectification of the electrical output is produced in the arc when TIG welding using:
a. AC with a suppressor
b. AC without a suppressor
c. DC with reverse polarity
d. DC with straight polarity
Which defect would you expect to get in TIG welds in non-deoxidised steel?
a. Undercut.
b. Porosity.
c. Tungsten inclusions.
d. Linear misalignment.
Argon purging on the root side is necessary in the TIG welding of stainless steel to:
a. Obtain full penetration.
b. Obtain full fusion.
c. Avoid porosity in the root.
d. Obtain a satisfactory weld surface finish.
When TIG welding austenitic stainless steel pipe, argon gas backing is called for. This is to:
a. Prevent oxidation
b. Prevent underbead cracking
c. Prevent porosity