You are on page 1of 1

I.

1) MATERIAL

- CONCRETE (composed of aggregates, water, cement,


admixture(optional))
- GROUT
- REINFORCING STEEL
 Prestressing Steel
o Wires
o Strands
o Tendons
o Bars
 Non-Prestressing Steel (Conventional)
o Addition to prestressing steel for:
 Flexural capacity (optional)
 Shear Capacity
 Temperature and Shrinkage requirement

I.1.1) CONCRETE

- Minimum Compressive Strength: 28Mpa (CLASS P)

- Maximum Aggregate Size: 20mm

I.1.2) REINFORCING STEEL

I.1.2.1) PRESTRESSING STEEL

- Uncoated, stress-relieved or low-relaxation, seven


wire strands

- Uncoated or deformed, high strength bars

Shall conform the following material standard:

STRANDS: AASHTO M203/M203M [ASTM A416/A416M]

BARS: AASHTO M275/M275M [ASTM A722/A722M]