S. No.

HARDENING Tempering Quench Flow Surface hard


Power Speed Power Speed
1 80 1400 30.75 1400 66 41-43

2 80 1500 30.5 1400 66 35-39

3 80 1450 30.5 1400 66 38-42


4 80 1400 30.5 1400 66 40-42
5 80 1400 31.25 1400 44 41-42

6 79.5 1400 31.25 1400 44 35-38

7 80 1400 32 1400 44 39-42

8 80 1400 31.25 1350 44 39-41


9 80 1400 31.75 1380 44 39-42
Residual Core HardnesRemarks

-60 370-380

-300 280-300

-190 310-340
-80
-110 390-410 Next day on same parameters, residual as well as core Hardness decreased

-230 330-360

-130 330-350

-80
-115 370-390 During production, residual decreasing gradually
ardness decreased