EN24 Steel Properties

EN24 / 817m40. EN24 is usually supplied in the T condition with a tensile strength of 850/1000 N/mm2.

EN24 is a popular grade of through-hardening alloy steel due to its excellent machinability in the "T"
condition. EN24T is used in components such as gears, shafts, studs and bolts. EN24T can be further surface-
hardened to create components with enhanced wear resistance by induction or nitriding processing.

International Steel Specification Comparison (EN24T)

BS 970:1955 EN24T
BS 970:1991 817M40T
German / DIN 34CrNiMo6
French AFNOR 35NCD6
American AISI / SAE 4340
German Werkstoff No. 1.6582
European Standard EN10277-5

817M40T - EN24T is a high tensile alloy steel renown for its wear resistance properties and also where high
strength properties are required.

Typical chemical composition of En24


C SI MN S P Cr Mo Ni

0.36/0.44 0.10/0.35 0.45/0.70 0.040 max 0.035 max 1.00/1.40 0.20/0.35 1.30/1.70

817M40T / EN24T Mechanical Properties

Tensile Yield
Size Impact Impact Hardness
Strength Stress Elongation
mm Izod J KCV J HB
N/mm² N/mm²

63 to 150 850-1000 680 Min 13% 54 50 248/302

150 to 250 850-1000 654 Min 13% 40 35 248/302

Convert hardness to Rockwell B, Rockwell C or Vickers.


EN24 is available from stock in round and flat bar and in plate.

Disclaimer:
The information presented here are typical or average values and are not a guarantee of maximum or minimum values.
Uses described are made only for the purpose of illustration to enable the reader to make their own evaluation and are
not intended as warranties, either express or implied, of fitness for these or other purposes.

ALAM STEEL

You might also like