Metal Iron Cast Iron Grey Cast Iron

ASTM A436 Grade Type 1

Description
Related Standards

ASTM A436

Properties
Mechanical

Hardness, Brinell HB 131 - 183 [-] at 20 °C

Tensile strength Rm 0 - 172 MPa at 20 °C

Chemical properties

Element Weight % Comment

Ni 13.5 - 17.5 %

Cu 5.5 - 7.5 %

Cr 1.5 - 2.5 %

Si 1 - 2.8 %

Mn 0.5 - 1.5 %

C 0-3%

S 0 - 0.12 %

This material data has been provided by ASTM.