Professional Documents
Culture Documents
99 Blok R.8, Jalan Raya Salembaran Tangerang
Pergudangan 99 Blok R.8, Jalan Raya Salembaran Tangerang
Telp : 021 ‐ 22550092 / 021‐22550079 Fax. : 021 ‐ 22550077
email : diwanbudiperkasa@gmail.com
DESIGN CALCULATION
MECH. CALCULATION
FRP EQUAL TEE
ASME NM 2 ‐ 2018
3. Design For FRP Equal Tee
Thickness design By HLU methode With 10 BarG Internal Pressure
h k h h l
PD R Reffer ASME NM 2 ‐ 2018 Page 14
t = m
2S
Where :
‐ Inside Diameter of Main Run Structur Wall, DR = (Di + 2c)
‐ Pressure Stress multiplier for integral tees, m
0.25
m = 1.4λZ
‐ Design Pressure, P = 10 BarG = 1 Mpa
‐ Hoop Tansile Stranght, S = 20.68 Mpa AWWA 950 Table 10 Page 18 ( 3000 Psi)
Tabel.2 Summary Thickness of FRP Equal Tee
y q
P S L Min. Thick Use thicknes
No Pipe Dia c DR λZ m
Di(mm) (mm) (mm) (Mpa) (Mpa) (mm) t (mm) t + C (mm)
1 350 3 356 8.48 1.86 1 20.68 556 16.0 19.0
2 300 3 306 10.20 1.94 1 20.68 506 14.4 17.4
3 25 3 31 1.19 1.14 1 20.68 231 0.9 7
Note :
‐ the use of thicknes has been adjusted to what is offered
‐ Use laminate type 2