211 82.1668 0.42657 13.40449 718.7215 3.129142 24 0.8784 0.001803 85.

48408
220 98.8 0.492854 12.00982 576.9431 2.727866 12 0.8413 0.001803 28.64731

The volume fraction of retained austenite was calculated using the formula:

1 𝐼ϒ 1 𝐼 1 𝐼ϒ
𝑉ϒ = /[ + ]
𝑝 𝑅ϒ 𝑞 𝑅 𝑝 𝑅ϒ

The volume fraction of retained austenite before and after inter-critical


annealing was estimated to be 0 0.06063 and 0.406494.

13.Conclusion:

With the rapid increase in the number of motor vehicles worldwide and the

associated environmental impact, automobile light weighing has become an

urgent global initiative. TRIP (Transformation-Induced- Plasticity)-aided steel

has receive much attention due to their outstanding combination of strength and

ductility. The present review introduces medium Mn steel , which is a candidate

3rd –G AHSS, and the effect of inter-critical annealing in the microstructure of

medium manganese steel. The microstructure of hot rolled alloy before and after

inter-critical annealing was investigated. Before inter-critical annealing the hot


19 | P a g e