You are on page 1of 1

Z-300

Li <5
Be
C 0.1-0.2%
F Quantification <3% is poor. Performance is better in He purge
Na <100
Mg <100
Al <100
Si <0.3% Maybe lower, need more standards
S 1-2%
K <100 K766+770
Ca <50
Ti <100
V
Cr <50
Mn <50
Fe <500
Ni <500
Cu <50
Zn <50
Ba <50
Pb <100

LODs assume:
6 second test over standard laser raster pattern. Averaging multiple locations may be necessary in some cases.
Pressed pellets with no surface contamination
Interference-free matrix