You are on page 1of 1

Fabricated piping (20 questions)

1.) Best NDE for weld-o-let to pipe joint?


2.) % Flattening of cross section of fitting allowed? Ans. 5%
3.) Personal qualification for NDE film interpretation shall be minimum of level 2.
4.) After how many repair the pipe cylinder shall cut off and replaced by new pipe? Ans 2.
5.) Which leak test is most preferable for fabricated piping? A) Pneumatic test b.) Halogen Leak
test. C.) Hydrostatic test d.) NDE in place of hydrostatic test d) any of the above.
6.) For procedure qualification which standard to refer? Ans. Section IX.
7.) Weep hole shall be provided to RF pad. Ans True.
8.) Weep holes shall be plugged only by grease.
9.) Best NDE to detect lack of fusion in the welding girth?
10.) Chloride content for hydrotesting of Austenitic steel pipe spools? 50 ppm.

Additional questions shall be added later.