0% found this document useful (0 votes)
318 views1 page

Material Chart

This document provides standards for various materials used in pipes, forgings, castings, fittings, plates, bolts, and nuts. It lists the appropriate ASTM standard for 13 material types including carbon steel, low temperature carbon steel, alloy steel, stainless steel, inconel, titanium, aluminium, monel, hastelloy B, hastelloy C, nickel, alloy 20, and bronze. It also lists general material certification requirements regarding melting method, practice, deoxidation, quality, and heat treatment.

Uploaded by

Nirmal Parmar
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as XLS, PDF, TXT or read online on Scribd
0% found this document useful (0 votes)
318 views1 page

Material Chart

This document provides standards for various materials used in pipes, forgings, castings, fittings, plates, bolts, and nuts. It lists the appropriate ASTM standard for 13 material types including carbon steel, low temperature carbon steel, alloy steel, stainless steel, inconel, titanium, aluminium, monel, hastelloy B, hastelloy C, nickel, alloy 20, and bronze. It also lists general material certification requirements regarding melting method, practice, deoxidation, quality, and heat treatment.

Uploaded by

Nirmal Parmar
Copyright
© © All Rights Reserved
We take content rights seriously. If you suspect this is your content, claim it here.
Available Formats
Download as XLS, PDF, TXT or read online on Scribd

STANDARD FOR MATERIAL

Sl.No Material Description PIPE FORGING CASTING FITTING PLATE BOLTS & STUDS / NUTS

1.0 CARBON STEEL ASTM A 106 Gr.B ASTM A 105 ASTM A 216 Gr. WCB ASTM A 234 Gr. WPB ASTM A 515 Gr. 60 ASTM A 193 Gr. B7 / ASTM A 194 Gr. 2H
API 5L
IS1239

2.0 LOW TEMP. ASTM A 333 Gr. 3 & 6 ASTM A 350 Gr. LF1 & LF2 ASTM A 352 Gr. LCB ASTM A 420 Gr. WPL 3 & 6 ASTM A 516 Gr. 60 & 70 ASTM A 320 Gr. L7 / ASTM A 194 Gr. 4
CARBON STEEL

3.0 ALLOY STEEL ASTM A 335 Gr.P1, P22 etc. ASTM A 182 Gr.F1, F22 etc. ASTM A 217 Gr. WC1, ASTM A 234 Gr. WP1, WP22 ASTM A 204 Gr.B & ASTM A 193 Gr. B5 / ASTM A 194 Gr. 3
WC9 ASTM A 387 Gr. 11, 22

4.0 STAINLESS STEEL ASTM A 312 TP 304 / TP 316 ASTM A 182 Gr. F304 / F316 ASTM A 351 CF8 / CF8M ASTM A 403 TP 304 / 316 ASTM A 240 Gr. 304 / 316 ASTM A 320 Gr. B8 / ASTM A 194 Gr. 8

5.0 STAINLESS STEEL ASTM A 312 TP 304 / TP 316 ASTM A 182 Gr. F304L / F316L ASTM A 351 CF3 / CF3M ASTM A 403 TP 304L / 316L ASTM A 240 Gr. 304L / 316L -

6.0 INCONEL - ASTM B 166 - - - -

7.0 TITANIUM - ASTM B 381 ASTM A 367 - - -

8.0 ALUMINIUM - ASTM B 247 ASTM B 26 - - -

9.0 MONEL - - ASTM A 296 M 35 - - -

10.0 HASTELLOY B - - ASTM A 296 N 12 M 1 - - -

11.0 HASTELLOY C - - ASTM A 494 CW 12 M 1 - - -

12.0 NICKEL - - ASTM A 296 CZ 100 - - -

13.0 ALLOY 20 - - ASTM A 296 CN 7 M - - -

14.0 BRONZE - - ASTM B 61 & B 62 - - -

1 Material Certification Requirements :


1.1 Melting method
1.2 Melting practice
1.3 Deoxidation
1.4 Quality
1.5 Heat treatment