You are on page 1of 3
‘QW - 483 PROCEDURE QUALIFICATION RECORDS (PQR) (Record Actual Variables Used to Weld Test Coupon) Company Name: M/s SANTI FIBRE INDUSTRIES (INDIA) Procedure Qualification Record No: SF/PQR/GMAW-0001 (Org date 04/12/2022) Revision: 01 Date: 4/08/2023 WPS No. SFIWPS/01 (org date 05/12/2022) Revision: 01 Date: 4/05/2023 Welding Process (es) GMAW Typesis) (Automatic, Manual machine or Semi Auto): Manual, Horzontal position JOINTS (QW-402) See Page No. 3 of 3 | Fillet weld Joint Test Coupon (For combination qualifications, the deposited weld metal thickness shall be recorded for each filler metal or process used) |] BASE METALS (QW-403)_ | POSTWELD HEAT TREATMENT (QW-407) h IS 513 CR2 (Part 1 2016) Temperature NA E | 7 ade UNS Number. A SSSSS™S~*dCTmgs NA - ‘Group Not = Other NA = = st Coupon 1S mim TT Test Coupon (OD) NA | num Pass Thickness. = 3mm : 7 : Orner NIL GAS (QW-408) ercent Composition | Gas(es) | (Muture) | Flow Rate “FILLER METALS (QW-404): _SFA Specification ‘Shielding “railing Current OC Polarity: DCEP (Reverse Polarity) ‘Amps. 70-220 Amps. Volis 18 Tungsten Electrode type & size. _N/ | Mode of Metal Transfer for GMAW. Shor Grea | | Other NA a | x |] “Flux Type “Flux Trade Name: 5 Weld metal Thickness [TECHNIQUE (awa) Tra BL ositon of GroovelF it iF Filet horizontal position trodes’ SINGLE ELECTRODE _ Travel Speed- (Range) 60-1 Weld Progression (Uphill/ Downhill Fat String or Weave Bead String For Rook Sting for Rost Temperature: WA TA Inier pais Temperatur run nae or susequet runs i Otner Nit L —— | QW-483 (Back) POR No. SFPORIGMAW-0007 Revision: 01 Dat i 7 ____ Tensile Test (QW-150) ‘Specimen [Width Thickness Ultimate Ultimate | Type of, No (enm) (mmm) Total Load | Unit Sess | Failure & —(itPa)__| Location pele |] Bow eroken oxiste he wor Toughness Tests (QWA7O NA Specimen | Notch —] Specimen | Test Impact Valves Drop weight No. Location | Size (mm) | Temp. % Shear | Mils (in) Break(Y/N) t Comments. DYE PENETRATION TEST IN FILLET WELD & LAP WELD JOINT (QW-180): N.A. Result - Satisfactory. Penetration into Parent Metal: NA ‘visual Tests - Acceptable OTHER TESTS: Type of Test MACRO TEST (Report No - TIMET-0054/23-24, ot-24/04/2023) Witnessed by Mr. Chandan Majumder (SGS) Welder's Name: Gopal Porel Tests Conducted by : R Basu Laboratory Test No: TC759723000001170F Result SATISFACTORY We certify that the statements in this record are correct and that the test welds were prepared. welded and tested in accordance with the requirements of Section IX of ASME Boller and Pressure Vessel Code. re ALN de ere Date: 23/02/2023 Date 03.05.2023, {= Thickness of Plate = 5 mm a) Groove Angle = 90° + 5° t) Plate Thickness = 1.5 mm [SANTI FIBRE INDUSTRIES, KOLKATA, Inspection Authority Mr. Chandan Majumdar (SGS INDIA PVT. LTD.) Page 3 of |

You might also like