At the damaged spot, verify whether the steel Remove loose coating and bevel all sharp edges of
substrate is also damaged. Do not repair the the coating damage.
coating until QA/QC have inspected the damaged
steel surface and have approved coating repair.

(FOTO) (FOTO)

3 4
Roughen the surface of the plant coating around the …
damaged spot with an abrasive pad or sand paper.
Remove all contaminations.

(FOTO) (FOTO)

5 6
Degrease with isopropyl alcohol. Do not use a …
thinner.
(FOTO) (FOTO)

7 8
Depending on the size and depth of the damage,
Paste might be necessary to fill the damage. Apply
strips of Wrappingband over the damaged area with
a minimum overlap of 50mm on the factory applied
coating.

(FOTO) (FOTO)

9 10
A holiday test using a high voltage tester must be Always use approved and certified holiday test
carried out on the green STOPAQ Wrappingband equipment.
prior to the application of any Outerwrap. The test
must be carried out at a minimum of 15kV.

(FOTO) (FOTO)

11 12
Apply Outerwrap over the Wrappingband with
tension and avoid air inclusions. Start and finish with
an overlap of at least 50mm on plant coating
adjacent to the 50mm outside the Wrappingband.