Professional Documents
Culture Documents
Rigid Pavement
Transverse Cracking
Rigid Pavement
Transverse Cracking
Causes:
Slab longer
than 15’
Slab Curl
Curing
Rigid Pavement
Transverse Cracking
Causes:
Slab longer
than 15’
Slab Curl
Curing
Rigid Pavement
Transverse Cracking
Causes:
Slab longer
than 15’
Slab Curl
Curing
Rigid Pavement
Transverse Cracking
Cures:
Crack Sealing
Full-depth rigid
repair
Dowel bar
retrofit
Rigid Pavement
Longitudinal Cracking
Rigid Pavement
Longitudinal Cracking
Causes:
Waiting
too long to
cut center
joint
Rigid Pavement
Longitudinal Cracking
Causes:
Waiting too
long to cut
center joint
Subsoil
settlement
Rigid Pavement
Longitudinal Cracking
Causes:
Waiting too
long to cut
center joint
Subsoil
settlement
Rigid Pavement
Longitudinal Cracking
Causes:
Waiting too
long to cut
center joint
Subsoil
settlement
Meander
cracks
Rigid Pavement
Longitudinal Cracking
Cures
Joint Sealing
Full Depth
replacement
Subsurface
stabilization
Rigid Pavement
Pumping
Rigid Pavement
Pumping
Causes:
Water
Fines
Lack of load
transfer
Loading
Rigid Pavement
Pumping
Causes:
Water
Fines
Lack of load
transfer
Loading
Rigid Pavement
Pumping
Causes:
Water
Fines
Lack of load
transfer
Loading
Rigid Pavement
Pumping
Cures
Under sealing
Dowel bar
retrofit
Full depth rigid
repair
Concrete
pavement
grinding
Rigid Pavement
Faulting
Rigid Pavement
Faulting
Causes:
End-result of
pumping
Rigid Pavement
Faulting
Causes:
End-result of
pumping
Eroded subsoil
Rigid Pavement
Faulting
Causes:
End-result of
pumping
Eroded subsoil
Rigid Pavement
Faulting
Cures:
Full-depth rigid
repair
Undersealing
Dowel bar
retrofit
Grinding
Rigid Pavement
Transverse Joint Spalling
Rigid Pavement
Transverse Joint Spalling
Causes:
Improper
dowel
alignment
Rigid Pavement
Transverse Joint Spalling
Causes:
Improper
dowel
alignment
Lack of joint
seal
Rigid Pavement
Transverse Joint Spalling
Causes:
Improper
dowel
alignment
Lack of joint
seal
Incompressible
s in joint
Rigid Pavement
Transverse Joint Spalling
Cures:
Crack & Joint
Seal
Bonded
Patching
Full-depth
patching
Rigid Pavement
Wear & Polishing
Rigid Pavement
Wear & Polishing
Causes:
Traffic wears
off surface
aggregate
Rigid Pavement
Wear & Polishing
Cures:
Grinding
Asphalt
Overlay
Rigid Pavement
Scaling
Rigid Pavement
Scaling
Causes:
Non-air-
entrained
concrete
Rigid Pavement
Scaling
Causes:
Non-air-
entrained
concrete
De-icing
chemicals
Rigid Pavement
Scaling
Causes:
Non-air-
entrained
concrete
De-icing
chemicals
Improper
finishing
technique
Rigid Pavement
Scaling
Cures:
Grinding
Asphalt
overlay
Bonded
resurfacing
Partial depth
patch
Rigid Pavement
Shallow Reinforcing
Rigid Pavement
Shallow Reinforcing
Cause:
Reinforcing
Steel too close
to surface
Rigid Pavement
Shallow Reinforcing
Cause:
Reinforcing
Steel too close
to surface
Rigid Pavement
Shallow Reinforcing
Cure:
Asphalt
overlay or
patch
Replacing
steel & partial
or full depth
repair
Rigid Pavement
D-Cracking
Rigid Pavement
D-Cracking
Causes:
Poor quality
aggregate
Rigid Pavement
D-Cracking
Causes:
Poor quality
aggregate
Freeze/thaw
cycle
Rigid Pavement
D-Cracking
Cures:
Temporary:
Partial depth
asphalt patch
Permanent:
Full-depth
repair
Rigid Pavement
Corner Cracking
Rigid Pavement
Corner Cracking
Causes:
Insufficient soil
support
Rigid Pavement
Corner Cracking
Causes:
Insufficient soil
support
Temperature
related slab
movement
Rigid Pavement
Corner Cracking
Cures:
Partial or full-
depth patch
Replace slab
Stabilize
subsurface
Rigid Pavement
Blowups
Rigid Pavement
Blowups
Causes:
Expansion of
concrete
Rigid Pavement
Blowups
Causes:
Expansion of
concrete
Poorly sealed
joints
Rigid Pavement
Blowups
Causes:
Expansion of
concrete
Poorly sealed
joints
Hot weather
Rigid Pavement
Blowups
Cures:
Pressure relief
joints to
prevent
Patch or
reconstruction
after
occurrence
Rigid Pavement