Figure 5 : Comparison of elongation flakiness index for different kinds of

aggregate samples.

Figure 5 shows the comparison diagram regarding elongation index in percentage


for five different sample of aggregate as 29.31% , 16.66% , 18.51% , 38.93% &
72 %respectively.
Top View

Side View

Figure 3 : Metal Length Gauge

Figure 3 represents the metal thickness gauge used for the determination of
aggregates elongation index. A metal length gauge indicates the standard length
for a specific material for the purpose of determining the elongation index of the
particular material.
Figure 2 : Aggregate Sample

Figure 2 represents the aggregate sample used for determination of aggregate


elongation index by group 1.
Figure 4 : Mechanical Sieve Shaker

Figure 4 represents the mechanical sieve shaker with BS test sieve , arranged in
descending order as 50.0 mm, 37.5mm, 28mm , 20mm, 14mm, 10mm, 6.3mm
respectively. Generally, typical sieve shaker separates particles by passing them
through a series of chambers with mesh filters and agitating the sample in order
to obtain complete separation.