You are on page 1of 1

Test Report for BITURBO-200

Client:
Sample Information:
Brand Name Date of Sample received
Sample Condition
on its Receipt Date of Test completed
Date of Test Started Batch No.

Service Order No.

Test Results
Standard Test
S.No. Description Method Test Results Remarks
ASTM
1 Thickness 4.10mm
D5147

2 Peak Load 31.9 KN/m

o
Tensile Strength @ 23 C
1385 N/5cm
Longitudinal
3.1
o
Elongation @ 23 C ASTM
56.0%
Longitudinal D5147
o
Tensile Strength @ 23 C
1200 N/5cm
Transverse
3.2
o
Elongation @ 23 C
77.3%
Transverse
o
Tensile Tear Strength @ 23 C
800 N
Longitudinal ASTM
4
Tensile Tear Strength @ 23 C
o D4073
650 N
Transverse

Note: 1.0 This report shall not be reproduced, except in full, without the prior written approval of the management
2.0 The Test Results relate only to the samples tested

Tested By. _________________________ Checked By. __________________________

You might also like