Professional Documents
Culture Documents
Report
VESSEL: DATE:
HOLD:
Rating Structure 3)
NOTES, e.g.
Deformation
Inspection 1)
Corrosion 5)
Area
* Evaluation of deficencies
Item
Fractures
Coating 4)
* Affected area (e.g. From frame x to
y,)
Tank top
Structure (incl. plates frames,stiffen.,girders,stringers etc.)
Ventilation Pipes
Fire extinguishing piping
Air & Sounding piping
Steam piping (heating)
GEN. COND. OF
COATING 2) Master:
GOOD
FAIR Ch. Officer:
POOR
REMARKS
1) Mark as follows: Y: Inspected / N: Not inspected / NA: Not applicable
2) Mark with X
3) Mark with X if found and give explanation in Notes
4) Mark Rating as follows: (see Assessment scale on next page)
1-Coating breakdown <=0.1% (GOOD)
2-Coating breakdown 0.1%<2% (GOOD)
3-Overall coating breakdown 2%<20% Or local coating breakdown at the edges of stiffeners and weld
connections >=20% but less as defined for poor condition (FAIR)
4-Overall coating breakdown 20%<50% (POOR)
5-Overall coating breakdown >50% (POOR)
5) Mark Rating as follows: (see Assessment scale on next page)
1- Minor spot rust <=0.1%
2- Light rust 0.1%<2%
3- Light rust 2%<20% and hard scale <10%
4- Hard scale >10%
5- Hard scale >20%
Page 1 of 5