Ferritic and Martensitic

Casting Materials
material application analysis (%)
JUNKER DIN- area C Si Mn Cr Ni Mo P S
number
F29 1.4085 stainless 0.50 - 0.90 ≤ 2.0 ≤ 1.0 27.0 - 30.0 - - ≤ 0.045 ≤ 0.030
F30C 1.4086 stainless 0.90 - 1.30 ≤ 2.0 ≤ 1.0 27.0 - 30.0 - - ≤ 0.045 ≤ 0.030
F30M 1.4138 stainless 0.90 - 1.30 ≤ 2.0 ≤ 1.0 27.0 - 30.0 - 2.0 - 2.5 ≤ 0.045 ≤ 0.030
M12 1.4107 creep resistant ≤ 0.10 ≤ 0.40 0.50 - 0.80 11.5 - 12.5 0.80 - 1.50 ≤ 0.50 ≤ 0.030 ≤ 0.020
M14S 1.4008 stainless ≤ 0.10 ≤ 1.0 ≤ 1.0 12.0 - 13.5 1.0 - 2.0 0.20 - 0.50 ≤ 0.035 ≤ 0.025
M14 1.4027 stainless 0.16 - 0.23 ≤ 1.0 ≤ 1.0 12.5 - 14.5 ≤ 1.0 - ≤ 0.045 ≤ 0.030
M13N 1.4317 stainless ≤ 0.06 ≤ 1.0 ≤ 1.0 12.5 - 13.5 3.5 - 5.0 ≤ 0.70 ≤ 0.035 ≤ 0.025
M16N 1.4405 stainless ≤ 0.06 ≤ 0.8 ≤ 1.0 15.0 - 17.0 4.0 - 6.0 0.70 - 1.50 ≤ 0.035 ≤ 0.025
M13NTT 1.6982 tough at low ≤ 0.05 ≤ 0.8 ≤ 1.0 12.0 - 13.5 3.5 - 5.0 0.40 - 0.70 ≤ 0.035 ≤ 0.015
temperature
M16NTT 1.6983 tough at low ≤ 0.05 ≤ 0.8 ≤ 1.0 15.0 - 16.5 4.5 - 6.0 0.50 - 2.00 ≤ 0.035 ≤ 0.015
temperature
Small abstract of all cast alloys of Otto Junker.