Other metals and alloys:

In addition to above information, OiLSERV have a data base on corrosion inhibitor effectiveness with CRA
materials. Information can be provided when required and additional tests can be performed in 3rd party
laboratories when requested.

Industry Acceptable Metal Loss is as follows:


Below 200 deg F: Acceptable metal loss is less than 0.02 lb/ft2,
200 - 250 deg F: Acceptable metal loss is 0.05 lb/ ft2,
Above 250 deg F: up to 0.07 lb/ft2 (The acceptable metal loss values change between operators)