You are on page 1of 3

PRODUCT DATA SHEET PRINCIPAL APPLICATIONS REGULATORY APPROVALS

Nitrate Removal French Health Ministry Approval for


Potable Water Treatment
Purolite® Kosher Certified
Certified by the WQA to NSF/ANSI-61
A520E Standard
Drinking Water Inspectorate Approved
Polystyrenic Macroporous,
Quaternary Ammonium Strong Base for Use in Public Water Supply in the
Anion Resin, Chloride form, Potable UK
Water Grade Water Regulations Advisory Scheme
Approved

TYPICAL PACKAGING
1 ft³ Sack
25 L Sack
5 ft³ Drum (Fiber)
1 m³ Supersack
42 ft³ Supersack

TYPICAL PHYSICAL & CHEMICAL CHARACTERISTICS:

Polymer Structure Macroporous polystyrene crosslinked with divinylbenzene

Appearance Spherical Beads

Functional Group Quaternary Ammonium

Ionic Form Cl- form

Total Capacity (min.) 0.9 eq/L (19.7 Kgr/ft³) (Cl- form)

Moisture Retention 50 - 56 % (Cl- form)

Particle Size Range 300 - 1200 µm

< 300 µm (max.) 1%

Uniformity Coefficient (max.) 1.7

Specific Gravity 1.07

Shipping Weight (approx.) 675 - 705 g/L (42.2 - 44.1 lb/ft³)

Temperature Limit 100 °C (212.0 °F) (Cl- form)

2022 Purolite www.purolite.com July 22, 2022 | Page 1 of 3


All rights reserved.
Hydraulic Characteristics
PRESSURE DROP BACKWASH

The pressure drop across a bed of ion exchange resin depends During up-flow backwash, the resin bed should be expanded in
on the particle size distribution, bed depth, and voids volume of volume between 50 and 70% for at least 10 to 15 minutes. This
the exchange material, as well as on the flow rate and viscosity of operation will free particulate matter, clear the bed of bubbles and
the influent solution. Factors affecting any of these parameters— voids, and reclassify the resin particles ensuring minimum
such as the presence of particulate matter filtered out by the bed, resistance to flow. When first putting into service, approximately
abnormal compressibility of the resin, or the incomplete 30 minutes of expansion is usually sufficient to properly classify
classification of the bed—will have an adverse effect, and result the bed. It is important to note that bed expansion increases with
in an increased head loss. Depending on the quality of the flow rate and decreases with influent fluid temperature. Caution
influent water, the application and the design of the plant, service must be taken to avoid loss of resin through the top of the vessel
flow rates may vary from 10 to 40 BV/h. by over expansion of the bed.

PRESSURE DROP ACROSS RESIN BED BACKWASH EXPANSION OF RESIN BED

2022 Purolite www.purolite.com July 22, 2022 | Page 2 of 3


All rights reserved.
Algeria India Mexico Spain
Australia Indonesia Morocco Taiwan
Bahrain Israel New Zealand Tunisia
Brazil Italy Poland Turkey
Canada Japan Romania UK
China Jordan Russia Ukraine
Czech Republic Kazakhstan Singapore USA
France Korea Slovak Republic Uzbekistan
Germany Malaysia South Africa

Americas EMEA FSU Asia Pacific


Purolite Purolite Ltd. Purolite Ltd. Purolite China Co. Ltd.
2201 Renaissance Blvd. Unit D Office 6-1 Room 707, C Section
King of Prussia, PA 19406 Llantrisant Business Park 36 Lyusinovskaya Str. Huanglong Century Plaza
T +1 800 343 1500 Llantrisant, Wales, UK Moscow, Russia No.3 Hangda Road
T +1 610 668 9090 CF72 8LF 115093 Hangzhou, Zhejiang, China 310007
F +1 800 260 1065 T +44 1443 229334 T +7 495 363 5056 T +86 571 876 31382
americas@purolite.com F +44 1443 227073 F +7 495 564 8121 F +86 571 876 31385
emea@purolite.com fsu@purolite.com asiapacific@purolite.com

The statements, technical information and recommendations contained herein are believed to be accurate as of the date hereof. Since the conditions and methods of
use of the product and of the information referred to herein are beyond our control, Purolite expressly disclaims any and all liability as to any results obtained or arising
from any use of the product or reliance on such information; NO WARRANTY OF FITNESS FOR ANY PARTICULAR PURPOSE, WARRANTY OF MERCHANTABILITY
OR ANY OTHER WARRANTY, EXPRESSED OR IMPLIED, IS MADE CONCERNING THE GOODS DESCRIBED OR THE INFORMATION PROVIDED HEREIN. The
information provided herein relates only to the specific product designated and may not be applicable when such product is used in combination with other materials or
in any process. Nothing contained herein constitutes a license to practice under any patent and it should not be construed as an inducement to infringe any patent and
the user is advised to take appropriate steps to be sure that any proposed use of the product will not result in patent infringement.

2022 Purolite www.purolite.com July 22, 2022 | Page 3 of 3


All rights reserved.

You might also like