Technical Information

Acronal® PS 608 ap
Polymer Dispersions for Construction
Chemical Nature Application Areas Processing

Acronal® PS 608 ap is an anionic Acronal® PS 608 ap is used to modify Should defoamer be requred in the
hydraulic binders system. Areas of formulation, FoamStar PB 2706 or
aqueous dispersion based on
application include Foamaster MO NXZ is strongly
acrylate polymer. recommended. Typical application
▪ Rigid and semi-flexible rates are within the range 0.3~1% in
waterproofing slurries and relation to the liquid component.
mortars
▪ Flexible ceramic tile adhesives To achieve proper rheology
▪ Sag-resistant repair mortars polyurethane-based thickeners can
▪ Industrial floor screeds and fine be added in liquid part, and lower
screeds viscosity MC could be used in both
▪ Other polymer modified power and liquid component as well.
cementitious mortars Superplasticizer like Meflux 2651 F is
suggested to be added in amounts of
Acronal® PS 608 ap provides 0.5~1% by weight to the cement
Technical Data excellent water impermeability in powder component to have great
cementitious waterproofing slurries workability.
and mortars.
Solids content 49 - 51 % Acroanl® PS 608 ap has a shelf life of
It has very good compatibility with six months at 10~30℃, provided due
pH value 6.5 – 8.5 various cements. attention is paid to the hygiene of
Viscosity A significant increase in the flexural tanks and storage facilities.
RVT, 23℃, 500 - 2000 mPa ∙ s strength and adhesion strength is It is strongly recommended to carry
2/10rpm observed in the repair mortar out your own trials when developing
formulation containing Acronal® PS and processing products contains
Density approx.1.02 g/cm3
608 ap. Acronal® PS 608 ap. This also
Tg approx. 10℃ Under proper polymer/cement ratio includes testing the storage stability
the performance of ceramic tile of customer’s finish product.
MFFT approx. 18℃ adhesive modified with Acronal® PS
608 could reach C2S2 standard.

Acronal® PS 608 ap provides


outstanding abrasion resistance in
modified indurstrial floor screeeds.
.

BASF East Asia Regional Headquarters The data contained in this publication are based on our current knowledge and experience. They do
Limited not constitute the agreed contractual quality of the product and, in view of the many factors that may
Dispersions & Resins Asia Pacific affect processing and application of our products, do not relieve processors from carrying out their
own investigations and tests. The agreed contractual quality of the product at the time of transfer of
45th Floor, Jardine House risk is based solely on the data in the specification data sheet. Any descriptions, drawings,
No.1 Connaught Place, photographs, data, proportions, weights, etc. given in this publication may change without prior
Central, Hong Kong information. It is the responsibility of the recipient of our product to ensure that any proprietary rights
Tel: + 852 2731 0111 and existing laws and legislation are observed.
Email: dispersions_apac@basf.com
www.dispersions.asiapacific.basf.com Edition: Aug 2016
TI/ED 2230 e