JOINTS (a) Secondary bonded joints for Class I vessels may be made by adhesive bonding or laminate overlay. Secondary bonded joints for Class II vessels shall be made by laminate overlay only. (b) Secondary bonded joints of Class I vessels shall be designed to withstand a minimum of six times the design pressure of the vessel without leakage. The adequacy of bonded joints shall be determined in accord- ance with the requirements of RD-160. (c) Secondary bonded joints of Class II vessels shall employ laminate overlays that are calculated in accord- ance with Articles RD-11 and RD-12 and pass the Acceptance Test criteria of Article RT-6. (d) Parts to be joined by secondary bonding shall be surface prepared as specified in the Procedure Speci- fication to enhance bond strength and reduce stress intensifications caused by structural discontinuities.