Professional Documents
Culture Documents
DMA
56 x 13 x 3 mm
TENSILE
250 X 25 X 3
IZOD
64 x 12.7 x 3.2 mm
FLEXURAL
3.2 mm x 12.7 mm
ilss
ASTM D2344 testing determines the apparent interlaminar shear strength of parallel
fiber reinforced plastics. This test method specifies using a 6.35 mm (0.250 in.)
diameter loading nose to apply a force downwards on the center of the specimen
until fracture. It does this at a rate of 1.3 mm (0.05 in./min.)