Professional Documents
Culture Documents
DEPARTMENT BANGKOK
OF CIVIL Project : -
CBR TEST (ASTM D1883) Test by : GROUP 5 Date : 22-03-2565 Sample : Laterite
Load Scale, K lb/div
SWELLING RESULTS Height of Sample,Ho mm Piston Area in²
Mould No. 1 2 3 Penetration Rate in/min
PENETRATION RESULTS
No. of Layer 5 5 5 Mould No. 1 2 3
Blows per Layer 12 25 56 Blows per Layer 12 25 56
Surcharge (lb) 10 10 10
Surcharge kg(lb) 10 10 10
Force Force Force
Swelling Swelling Swelling Penetration Pressure Pressure Pressure
% % % Gauge Gauge Gauge
Date Time x 0.01 x 0.01 x 0.01 in lb/in² lb/in² lb/in²
Swelling Swelling Swelling Reading Reading Reading
mm mm mm 0.000 0 0 0 0 0 0
0.025 32 49.70 39 61.34 16 23.08
0.050 64 102.93 87 141.20 54 86.30
0.075 99 161.16 157 257.65 118 192.77
0.100 133 217.72 224 369.11 270 445.63
0.150 197 324.19 361 597.02 384 635.28
0.200 248 409.03 513 849.89 465 770.03
0.250 299 493.88 675 1119.39 676 1121.05
0.300 342 565.41 830 1377.25 886 1470.41
0.400 435 720.13 1113 1848.04 1054 1749.89
0.500 533 883.16 1371 2277.25 1580 2624.94