Powder Metallurgy Process for

Manufacturing Core Projectile


Experiment Method
Material
Pb coarse (purity 99.8%).
Sn (purity 99.8%).
zinc stearate as lubricant.
Manufacturing Process Core
Projectile
Raw Material

At 100, 150, and 200C for 1, 2,


and 3 hours
10% weight of Sn The sample result was
89.75% weight of Pb cylindrical compacted mixture
Pb Powder 900 microns 0.25% Zinc stearate with
Lubricant 14 mm in diameter and 14 mm
Sn Powder 150 microns in height.
Microstructure/ Material
Properties
Characterization of Tin and Lead Sinter Density and Porosity
Powder
Tin Powder (Sn)

Lead (Pb) Powder


Characterization of Projectile
Result