Carried out by adding a soluble initiator to pure monomer The mixture is constantly agitated & heated to polymerization temperature Once the reaction starts, heating is stopped as the reaction is exothermic Adopted to produce polystyrene, polyvinyl chloride, polymethyl methacrylate