Fabrication of Biosilica Scaffold

Using a Salt Leaching Technique


Soraya Rahmanisa
Prinsip Dasar Metode Salt Leaching
Bahan yang dibutuhkan :
 Pelarut Polimer
 Partikel yang akan
dilarutkan
 Porogen (garam
anorganik, eg : NaCl,
gelatin, atau parafin)
The manufacturing technologies of scaffolds
(
Preparation of salt-leached biosilica scaffolds
(modification from Wang et al., 2012)
Biosilica

All the ratios of


gelatin/CMC were
Ekstrak Biosilika dari 180 G bloom in powder
dissolved in distilled water
sponge form and CMC solution
preparation at 21
milliliters

Add sodium chloride


powder (NaCl) sebanyak 7
Dipanaskan dan stirrer Soak with DI water
gram , lalu dicampurkan
pada suhu kamar

Desicator dan keringkan di


Cetakan/template Scaffold
dalam oven