MANUAL FOR INSPECTION OF STRUCTURES (SPILLWAY, HEAD REGULATOR AND OTHER CANAL STRUCTURES)

Narmada, Water Resources, Water Supply & Kalpsar Department GOVERNMENT OF GUJARAT April 2009

Mission Statement

Harnessing the untapped waters of rivers for the survival of millions of people and environmentally sound

sustainable development of Gujarat State by providing the essence of life -- water and energy

Initial issue date: April 2009

Date of revision

Outline of changes made

ii

Preface Like any engineering work, structures i.e. dams and canal structures require continual care and maintenance, first to ensure that they remain operational and capable of performing all intended purposes and then to preclude endangering people and property. The safety of all canals is of considerable concern. Given that, the principle purpose of this Manual is to enhance the safety of dams and canal structures.The purpose is to ensure adherence to approved procedures over long periods of time and during changes in operating personnel. The Manual is prepared primarily for the use of section officers in charge of various canals and canal structures who are assigned the responsibility for the operation and maintenance of the canal. THIS MANUAL CONTAINS, AS A MINIMUM, ALL INFORMATION AND INSTRUCTIONS NECESSARY FOR SECTION OFFICERS TO PERFORM THEIR DUTIES. The instructions provided in this manual are applicable to dams & canals of all sizes and types and are useful to all. The guidance provided is generally applicable to all situations. However, it is recognised that the degree to which the methods and principles are adopted will rest with the officer in charge of the dams & canals. Manual for inspection of earthen embankments is also required to be read and operated simultaneously.

CONTENTS
Chapter PART I 1. Inspecting the structures (Spillway, HR & Canal structures) PART II 2. General Problems & Deficiencies Common Material Problems Cracks Surface defects Concrete deterioration Metal problems 3. 4. 5. 6. 7. PART III 8 Obstructions Displacement Foundation and backfill problems Seepage Poor Drainage Inspection of Structures Inspection of spillways/ wasteweirs/ escapes 9 10 11 12 13 14 Inspection of canal siphons Inspection of drainage siphon Inspection of HR (Outlet works) Inspection of cross regulators Inspection of falls Inspection of aqeducts Page

PART IV 15. PART V 16. Inspection during emergency Schedule of Routine inspection

PART I

INSPECTING THE STRUCTURES (SPILLWAY, HR & CANAL STRUCTURES)

Chapter 1

INSPECTING THE STRUCTURES (SPILLWAY, HR & OTHER CANAL STRUCTURES) 1. Purpose The purpose of inspection is to identify deficiencies that potentially affect the safety of the structure. A deficiency is a condition that might affect or interfere with the safety or operational effectiveness of the structure. 2. Reviewing data Review any available data about the structure before you begin your inspection.An important aspect of inspection is tracking conditions and potential problems to determine how and to what extent they are changing over time.Historical and design information can alert you to conditions and features that are of special concern and that should be checked and documented. Types of information that may be useful to review include: Design criteria Material data Construction records Records of operation Records of maintenance Previous inspection reports Manual of operation

3. General Guidelines When an inspection is conducted several things are required to be kept in mind: The purpose of an inspection is to gather facts. Person inspecting should probe for causes till he is satisfied. One should look for continuities or relationships among deficiencies. All features of canal as well as structure should be inspected. No shortcuts need to be taken. Enough time should be spent for inspection. Particular attention should be paid to areas where data indicate that change is occurring or where past deficiencies have been noted. Person inspecting should know his limits and should consult higher officers in case of doubt. SMPL rule should be observed for documenting conditions: S Sketch the deficiency and note its important characteristics M Measure the deficiency P Photograph the deficiency/describe its characteristics in writing L Locate the deficiency relative to some standard reference point Good notes should be taken; thorough records should be made. Findings of inspection should be reported in form of precise report immediately after the inspection is over. This would be very much useful at the time of subsequent inspections and also would help evolve plan of action.

4. Inspection tools and equipments: Following outlines the tools and equipments that will be needed for conducting inspection of canals and structures:

Binocular Camera Rock hammer Measuring tape Probe Pocket knife Shovel Bucket and timer Torch with cells Jar

For sighting along top of bank, crest For recording conditions For sounding concrete/rock For measurement For measuring width of crack at a depth For scraping rock, scraping crevices/cracks For clearing drains, manholes, pipes For measuring seepage & flow rates For looking into pipes, conduits, barrels For taking water samples, measuring turbidity

5. Spillways/ Escapes: Observe the spillway/ escapes from the crest of waste weir. Walk along the concrete sill noting any cracks, leaks, heaving or erosion etc. Check the abutment-waste weir interface for any sign of erosion. Check walls and floors as per checklist. 6. Head Regulator/ Outlets: Observe the condition of the HR/ outlets at the upstream headwall. (In order to view the outlet, it will be necessary to lower the water level in the reservoir/canal. Prior to lowering, notify downstream operators. Once the water level is lowered, the gate should be operated through its full range as narrated in the "Guidelines for Operation & Maintenance " and also in the Standing Operating Procedure issued if any, however, the gate must be closed for inspection of the waste weir.)

7. The downstream area: Walk along the bed of the downstream channel and observe any unusual conditions which may affect the performance of the dam/ canal, such as debris, vegetation, seepage, wet areas or excessive sedimentation. Observe the lining, if any, to the channel to ensure that they are intact and in good condition. The inspection checklist included in this Manual should be copied and completed every time a maintenance inspection is performed. 8. Inspecting the upstream face of structure The upstream face should be inspected from the top of the wall, abutments, Top of Bund of canal or a boat. The number of positions from which you inspect the face depends on the length and height. It is desirable that the water level in the reservoir/ canal is as low as possible when you inspect the upstream face and that is the reason why March inspection is most likely to give better chances of inspection. 9. Under water inspection In some instances it may be advisable to have a divers team inspect the upstream face at a specific location below the waterline. This is a special inspection technique that is used occasionally to determine the cause or extent of a specific problem. 10 Inspecting the downstream face of structure If leakage is occuring or if structural distress is evident, it will most likely be found on the downstream face. It is best to inspect downstram face with water in the dam/ canal at the highest waterlevel
8

possible. This will increase your chances of seeing leakage on the downstream face of the dam/ canal. Pay particular attention to the toe of the structure where the structure joins the foundation material as well as the junction of the structure with the dam/ canal embankment.Look carefully for: Seepage along the toe Cracks Alignment changes. 11. Special safety concerns when inspecting structures The following safety issues are particularly important to the inspection of spillway, HR & canal structures: Only persons who are physically fit should attempt a strenuous inspection task. Provide for communication between someone at the entrance and the person inspecting the inside of a structure. Poisonous snakes are a real threat in some parts. For an under water inspection, divers should be qualified in both diving and , if possible, diving inspection. Video may be provided while carrying out under water inspection. Divers may be made aware of the potential dangers near intake structures and entrance of HR,siphon barrels, such as cross currents, damage to diving equipment from sharp edges of metal or protruding bars When working around energy dissipators or on steep or slippery slopes, inspecting person should be secured by ropes or harnesses.Water conveyance surfaces often have algae growth that can be particularly treacherous. IMPORTANT INSPECTION TIP: If water is against the gates, make sure all control equipment has been secured from operation or clearly marked (red tagged) with warnings that personnel may be injured if the equipment is operated. Be sure that operations and inspection personnel understand the significance of red-tag procedures.

PART II

GENERAL PROBLEMS AND DEFICIENCIES

10

CHAPTER 2 COMMON MATERIAL PROBLEMS These include common problems observed in construction material like concrete, metal, PVC water stops etc.

CONCRETE PROBLEMS COMMON IN STRUCTURES 1. Condition of concrete works is generally dependent on the quality of materials used, circumstances or quality of

construction, and severity of weather exposure. Poor quality materials and deficient composition of concrete and mortar will be evidence by various forms of deterioration. Likewise, poor quality construction, such as the use of too much of water in mixes or finishing and/or permitting exposure to heat before adequate curing and hardening of concrete or mortar, will lead to early and accelerated concrete deterioration. 2. Expansion, contradiction, and construction joints and pressure relief valves may be of concern when they become "open" and permit seepage or leakage of water. Some opening or closing of joints normally occurs with temperature changes. 3. All structures experience the entire range of possible concrete problems, but conditions especially worthy of note are: Cracking Surface defects Concrete deterioration : Cavitation Concrete deterioration : erosion Leaking Joints Inadequate or damaged water stops Other joint problems

11

1. CRACKING :

4. All concrete is subject to cracking, which is usually the first visible sign of concrete distress. You will see many cracks in the course of your inspections, and not all cracks are serious. However, cracking should be monitored because cracks can provide openings in the concrete that allow other types of deficiencies to develop. Characteristics of Cracks 5. Cracks in a concrete dam can be described in terms of several characteristics: width, direction, depth, location, and trend (change). Length 6.Length is a self-evident concept. The length of a crack is established by measurement. Width
FIGURE I. DETERMINING CRACK WIDTH

(Sectional View)

12

7. The width of a crack is the amount of separation between the two concrete parts. One common mistake made by some inspectors is that they measure the width of a crack at the surface, where deterioration of the concrete may exaggerate the true dimensions of the crack. Although surface deterioration should be noted, it should not be included in an estimate of crack width. If possible, you should measure or estimate crack width at a depth below the surface deterioration by inserting a probe such as a knife blade or wire. Figure 1 illustrates how to determine the width of a crack. Direction 8. The direction, or orientation, of a crack can be described using one or more of the following terms, which are illustrated in Figure 2: Longitudinal: A longitudinal crack runs roughly parallel to the top of the member of the structure. Transverse: A transverse crack runs roughly perpendicular to the top of the member of the structure. Horizontal: A horizontal crack is one that lies at a single elevation. Vertical: A vertical crack runs up and down. Diagonal: A diagonal crack shows some inclination between horizontal and vertical

13

Cracking also can occur in random patterns (e.g., alligator pattern) over the concrete surface.

FIGURE 2. ORIENTATION OF CRACKING

Depth 9. The full depth of a crack may be difficult to determine unless the crack extends to another face or interior surface of the dam, such as a chamber wall. Trend 10. Trend is extremely important in monitoring cracking. The trend of a crack is its history of change. Studying prior reports before you begin an inspection will enable you to focus on how cracks have changed--that is, whether they have become longer, wider, or deeper, changed direction, or remained unchanged. Documenting any changes you observe will enable future inspectors to do the same thing. Location 11. Identifying the location of a given crack is vital to monitoring
14

its

trend

in

future

inspections.

Some

of

the

reference

conventions are: Left and right facing downstream Block and joint numbers Drain numbers Other reference points are also useful: Stations (measured along the axis of the structure) Lift lines Elevation (on the downstream face) Measurements from any identifiable feature of the structure (e.g.handrails, parapat)

Types of Cracks 12. Cracking in concrete structures generally falls into the following four categories: Structural cracks Cracks along joints Shrinkage cracks Thermal cracking Pattern cracking D-Cracking Other Shallow Cracking

Structural Cracks 13. A potentially serious type of crack is the structural crack -a crack that calls into question the structural integrity of an element. Structural cracks are caused by the overstressing of portions of the sytucture because of extreme loading conditions, inadequate design, poor construction techniques, or faulty materials. Often, structural cracks can be related to some feature of the
15

structure where stress concentrations occur--for example. . . The corner of an opening Areas of large temperature gradient Discontinuities in the foundation caused by material or alignment changes or by differential movement in foundation or abutments

FIGURE 3 STRUCTURAL CRACK WITH VERTICAL DISPLACEMENT (Elevation View)

14. Structural cracks are often irregular; that is, they run at an angle to the major axes of the member (say wall or column) and they may change direction abruptly. These cracks are usually wide and may be associated with noticeable displacement of the concrete adjacent to the crack. The opening may tend to increase as a result of continuous loading and creep of the concrete. Figure 3 shows an irregular structural crack with vertical displacement. Cracks Along Joints 15. Cracking may occur along joints because of structural movement, volumetric changes, or chemical reactions. Some of these cracks are intentional and occur by design. Other cracks along joints are not intentional and may pose a threat to the

16

integrity of the structure. Document any new or worsening cracks along joints, unless you are certain that these cracks are there by design. Shrinkage Cracks 16. When concrete is subjected to cycles of wetting and drying, it expands and contracts. Volume changes occur during this process and develop tensile stresses within the concrete, causing cracking. Shrinkage cracks due to drying are generally fine and show no evidence of movement. They are usually shallow, but they can be several feet long. 17. Shrinkage cracks often occur soon after construction, as the cement paste cures and shrinks. These cracks usually occur shortly after construction and usually do not penetrate deeply enough to be a threat. Thermal Cracking 18. When concrete is placed in large sections, high tensile stresses can result from the heat generated by the hydration of cement, followed by differential cooling. When tensile stresses exceed the tensile strength of the concrete, the concrete will crack. Cracking due to thermal stresses is usually orthogonal (rectangular) or blocky. Thermally induced cracks are generally much deeper than shrinkage cracks. 19. Cracks also can be caused by temperature variations not associated with construction. During cold weather, upper portions of the darn may become colder than the lower portions

17

that are in contact with the reservoir water. This temperature difference can cause cracks to form, extending from the top down each face of the strucyural member. Pattern Cracking 20 Pattern cracking is indicated by fine openings on concrete surfaces in the form of a pattern. Pattern cracking results from a decrease in volume of the material near the surface, or increase in volume of the material below the surface, or both. Figure 4 illustrates pattern cracking.

FIGURE 4

PATTERN CRACKING

21. Pattern cracks usually indicate a problem, such as freezethaw action or some type of undesirable chemical reaction occurring in the concrete. Chemical reactions will be discussed in greater detail under concrete deterioration. 22. Freeze-thaw action occurs when water enters the pores, cracks, or joints in the concrete. When the water freezes, it expands and causes the concrete to crack. Water then can enter

18

the new cracks and, when it freezes, cause the cracks to widen, or spall at the surface. D-Cracking 23. Sometimes D-cracking along joints is an early sign that freeze-thaw action has occurred. (D-cracking is the progressive formation of a series of fine cracks at close intervals, often in random D-shaped patterns along a joint.) Figure 5 illustrates Dcracking. As the cycle continues, the cracks extend farther away from the joint and become more severe. This process may lead to further disintegration of the concrete.

FIGURE 5

D-CRACKING

24. Virtually all mass concrete placed in recent years has included entrained air to reduce freeze-thaw deterioration. Other Shallow Cracking 25. Other types of shallow cracking you may notice in concrete surfaces are checking and hairline cracking. Checking refers to the developmeJ1t of shallow cracks at closely spaced but irregular intervals on the surface of mortar or concrete. Hairline cracking refers to small cracks of random pattern in an exposed
19

concrete surface.

CRACKING:

INSPECTION ACTION

26. Generally speaking, most cracks will fall into the to-bemonitored category-cracks that have been monitored in the past and should be measured and documented. A good ongoing record is necessary in order to identify a significant change or trend. New, severe, or extensive cracking and sudden changes warrant some action on your part. The followings are a few inspection guidelines. : For cracks that have been monitored and documented before, take measurements and document and changes. Based on the trend noted for a particular crack, you may wish to decrease the interval between measurements. If you observe prominent cracks or cracking over large areas measure and document them. In these cases, too, more frequent measurements may be advisable. If you observe extensive new cracking, consider initiating a crack survey to thoroughly document all cracks in the structure, their characteristics. If you observe a major new crack, or one whose characteristics have changed drastically from the previous inspection. Carry out assessment of the situation as quickly as possible. If you observe cracks indicating movement that might be detrimental to the structure or to equipment operation (e.g. Misalignment of gates that impedes gate operation and water release), get an immediate assessment done. If you find that an excessive amount of water which cannot be handled by the drainage system is flowing through a crack, recommend repairs. Identify appropriate repair procedures.
20

CRACK SURVEYS 27. A crack survey is an examination of a concrete structure for the purpose of locating, recording, and identifying cracks and of noting the relationship of the cracks with other destructive phenomena. Since cracking is often the first noticeable symptom of concrete distress, a survey is a significant part of evaluating the future serviceability of the structure. Some cracks may occur early and not progress, while others may occur later and increase in extent. Some may occur after an unusual event. A design drawing or inspection drawing is often used to record the location and extent of cracks in this type of survey. 28. A crack survey should identify Characteristics of the cracks (length, width, direction, depth, and location) Descriptions of types Descriptions of other conditions or deficiencies that may be associated with cracking Whenever feasible, external cracks should be correlated with internal cracks. Where repairs have been made to the concrete, crack surveys are difficult to perform and may be unreliable because cracks beneath the repairs may indicate deficiencies at greater depths. It is significant, however, to note whether new cracks have developed in the repair concrete. Such cracks may indicate continued structural problems.

21

INSPECTION TIP: If you are at all unsure about the severity of cracking consult Design Office so the situation can be evaluated.

Figure 6 next page shows a Crack Map.

22

Figure 6

Crack Map

23

2. SURFACE DEFECTS 29. Surface defects are concrete deficiencies that are not progressive in nature; that is they do not necessarily become more extensive with time. They may include Shallow deficiencies in the surface of the concrete. Textural defects resulting from improper construction techniques. Localized damage to the concrete surface. If you observe surface defects in the concrete, you should Record their nature and location. Note the need for prompt repair of defects that might lead to more extensive deterioration (e.g., by allowing water to enter the concrete mass). Among the most common types of surface defects are

honeycombs, stratification, evidence of from slippage, stains and impact drainage. Honeycomb: (Figure 7) 30. Honeycomb is a void that is left in the concrete when the

24

mortar fails to fill the spaces between the coarse aggregate particles effectively. Honeycomb is caused by poor construction practices, such as inadequate concrete mixing, segregation due to improper placement practices, or inadequate vibration after placement in the forms.

Stratification: (Figure8 ) 31. Stratification is the separation of overly wet or over vibrated concrete into horizontal layers, with increasingly smaller

FIGURE 8 : STRATIFICATION

material concentrated towards the top. Stratification can result in concrete of non-uniform strength, weak areas and disbonding of lift lines. Form Slippage: 32.Form slippage occurs when construction forms lack

sufficient strength to withstand the pressure resulting from placement and vibration of the concrete. When the forms slip
25

during construction, they can produce slightly off set blocks and uneven joints and surfaces. Sometimes form slippage is mistaken for misalignment of the concrete, which usually occurs well after construction. Stains: 33. Although discoloration and staining sometimes are

associated with deterioration of concrete, most stains on concrete surfaces cause only an unpleasant appearance rather than damage. Stains may have natural causes, such as deposits from runoff water of deposits from corrosion of exterior steel. They may also result from construction or maintenance accidents (e.g. oil, grease, paint, creosote or asphalt). Imapct Damage: 34. For example, the impact of a truck, boat, or crane, or rock thrown into chutes can mar or chip away a portion of the concrete surface. While such damage is localized, it can lead to other damage, such as freeze thaw action, by permitting moisture to enter the concrete. SURFACE DEFECTS : INSPECTION ACTIONS.

35. Unlike cracks, which may penetrate well into the concrete, surface defects usually are shallow and do not usually present an immediate threat to the structure. However, by erecting an opening to weather and other forces, they can lead to other more significant deterioration. If you observe surface defects in the concrete, you should ..

26

Record their nature and location (remember SMPL) Note the need for prompt repair of defects that might lead to more extensive deterioration (e.g., by allowing water to enter the concrete mass).

27

3. CONCRETE DETERIORATION 36. Deterioration is any adverse change on the surface or in the body of the concrete that is caused by separation of components of the concrete. Types of Deterioration 37. There are numerous observable conditions that can indicate concrete deterioration. Cracks, which we have discussed at some length, can be considered a specific type of deterioration, and they are often associated with other types of deterioration. The following are the most common types of concrete

deterioration that you are likely to encounter. Disintegration 38. Disintegration is deterioration of concrete into small particles, or crumbling, due to any cause. Spalling 39. Spalling is the loss of chunks of concrete from a surface, usually because of compression, impact, or abrasion. Spalling often occurs at the edges of concrete (e.g., along cracks, joints, and corners or next to embedded objects). Figure 1, presented earlier in this unit, showed a spall along a crack. Spalling may have various causes: A blow to the concrete Action of weather Internal pressure (e.g., from a corroded rebar near the surface) Expansion within the concrete mass

28

Although spalls themselves are confined to the surface of the concrete and thus may not be a serious problem, spalling can lead to secondary problems. For example, spalling may expose reinforcement, create a seepage path around an embedded waterstop at a joint, create an offset along the flow surface, or develop into a point of structural weakness. Efflorescence 40.Efflorescence is a deposit of salts from within the concrete that forms on the surface. Efflorescence is caused by water leaking through joints and cracks, leaching calcium hydroxide or carbonate from the cement, and carrying it to the exposed surface. As the water evaporates, a hard, white calcium deposit forms on the surface. As calcium is leached from the concrete around the joint, the opening may widen. This in turn leads to increased leakage and faster deterioration. It should be noted, however, that leaching also can be a self-healing process. In some cases the calcium may be deposited in such a way around the joint that it seals the opening against additional leakage. Drummy Concrete 41.Drummy concrete is concrete that has a void, separation, or other weakness within the concrete--usually a thin surface layer separated from the mass. You can check for drummy concrete by striking a hammer or "bonker" against the surface and listening for a hollow sound. Figure 9 illustrates drummy concrete.

29

FIGURE 9. DRUMMY CONCRETE

(Elevation View) Popouts 42. A popout is a small portion of the concrete surface that breaks away, due to internal pressure, leaving a shallow, conical depression. Figure 10 illustrates popouts.

FIGURE 10.

POPOUTS (Elevation View)

30

Pitting 43. Pitting is the development of relatively small cavities in the concrete surface. Pitting is caused by localized disintegration. Figure 11 illustrates pitting.

FIGURE 11.

PITTING (Elevation View)

Scaling 44. Scaling is the flaking or peeling away of the surface of the concrete or mortar. Figure 12 illustrates scaling.

FIGURE 12. SCALING (Elevation View)

Causes of Concrete Deterioration 45. In most cases cracking is both an initial cause and an effect of concrete deterioration. That is, by exposing internal surfaces
31

of the concrete to weathering, seepage, chemicals, or other elements, cracks lead to further deterioration. At the same time, cracking is often an indication that concrete deterioration is occurring. INSPECTION TIP: Whenever you observe cracking, you should be alert to the possibility of other types of concrete deterioration. 46. We have already discussed drying shrinkage, thermal stress, and freeze-thaw action as causes of concrete deterioration. Other common causes of concrete deterioration are the

following: Faulty concrete mixes Chemical attack Metal corrosion Erosion Cavitation

47. Faulty Concrete Mixes Ingredients used to make mass concrete must be carefully proportioned to produce concrete of adequate strength and durability. When concrete mixes contain improperly graded aggregates or improper cement or water content, the concrete may lack strength and be subject to disintegration. 48. Chemical Attack There are three common types of chemically induced deterioration in concrete: attack, acid attack, and alkali-aggregate reaction. 49. Sulfate Attack: Sulfate attack is a chemical and/or physical reaction between sulfates in soil or ground water and concrete. The reaction causes expansion, or growth, in the
32

concrete, which leads to disintegration. Concrete attacked by sulfate is usually light in color and falls apart easily when struck with a hammer. Other typical symptoms of sulfate i1 t tack include. . . Cracking Spalling Scaling Stains

50. Acid Attack: Acid attack is usually the result of bacterial action on the calcium hydroxide found in hydrated Portland cement, limestone, or dolomitic aggregates. In most cases, the reaction results in leaching away of water-soluble compounds. Symptoms of acid attack may include. . . Efflorescence Cracking Spalling Color change

Acidic water created by this reaction can also hasten corrosion of embedded steel reinforcement. As the steel corrodes, internal pressures develop, which may crack or spall adjacent concrete. 51. Alkali-Aggregate Reaction: An alkali-aggregate reaction is an undesirable chemical reaction between cement and aggregate that causes abnormal expansion and cracking. There are two main kinds of alkali-aggregate reaction: alkali-carbonate

reaction and alkali-silica reaction. Early indicators include. . . Pattern cracking, usually concentrated in areas that are exposed to moisture in a wet-dry cycle (e.g., piers, parapets, and the top of the structural member) Efflorescence Incrustation
33

White rings around aggregate particles A gel-like substance at pores, cracks, or openings in the concrete (only for alkali-silica reactions) Extreme alkali-aggregate reactions are characterized by closing of expansion joints, hence the term growth of concrete is sometimes used. Continued reaction can result in . . . Debonding of blocks at lift lines Binding of gates, valves, and metalwork Severe cracking Loss of strength and ultimate failure of the structure by sliding or overturning Metal Corrosion 52. Embedded reinforcing steel normally is protected by the concrete. When the concrete deteriorates, however, water can reach the steel and cause it to corrode. The oxide produced during corrosion results in an increase in volume, which causes the overlying concrete to crack and spall. The most well-known form of corrosion is rust. Indicators of rust corrosion in reinforcing steel include Cracks running in straight, parallel lines at uniform intervals corresponding to the reinforcement spacing Rust stains on the surface Spalling Exposed reinforcement

FIGURE-13. CONCRETE DETERIORATION DUE TO METAL CORROSION

34

Figure 13 shows concrete deterioration due to metal corrosion. 53. Other types of corrosion to steel reinforcement bars include: Galvanic Corrosion, which occurs at metal-to-metal

connections and contact points and may appear as corrosion in one of the metals but not the other. Pitting Corrosion, which appears as small cavities or craters on the metal and may be indicated by changes in surface texture of the metal. Stress Corrosion, which is a result of the combined action of environmental corrosion and the application of stress to the metal. This type of corrosion cannot be detected by observation alone and can result in rapid, brittle failure of the metal without warning.

CONCRETE DETERIORATION: CAVITATION 54. Concrete deterioration is any adverse change on the surface or in the body of the concrete that is caused by separation of components in the concrete. Cavitation occurs when a critical combination of the flow velocity, the flow pressure, and the vapour pressure in the water in the water is reached. An offset or irregularity on a flow surface exposed to high velocities produces turbulence. This turbulence creates negative pressures that cause water to vaporize and form bubbles, or cavities, in the water. Bubbles collapse when subjected to higher pressures downstream from the formation site.

35

Bubble collapse dynamics then create shock waves that can damage the flow surface. Popping and cracking noises

(Crepitation) accompany the collapse of the cavities. The impact of the shock waves can produce pressure up to 100,000 pounds per square inch. Repetition of these high-energy blows

eventually forms the pits or holes known as cavitation damage. 55. Common sites for cavitation are: Downstream of gates and valves In steep spillway chutes, tunnels or conduits Cavitation may occur on the floor of a chute, or on the walls or sides of a structure. Cavitation damage resembles erosion damage, but cavitation is potentially a much more serious problem, once the process begins, deterioration can occur quickly. A tiny offset or carbonate deposit may induce cavitation, leading to serious damage or failure of the concrete in a structure during heavy flows. 56. A pitted surface and/or rough holes with aggregate plucked out suggest cavitation damage. Damage upstream and

progresses downstream in a leapfrog pattern: each cavitation site triggers the deterioration of a new site downstream. 57. If cavitation is detected, try to determine what event caused the damage and to evaluate the potential for further damage. Consider the frequency of operation. Examine air vents to flow passages visually or by pouring water into them to ensure that they are not obstructed.

36

58. Cavitation effects can sometimes be mitigated by repairing the area stronger material such as steel polymer concrete. Installing aeration slots in tunnels/ conduits eliminates negative pressures by providing additional air to the affected areas. Concrete Deterioration: Erosion: 59. Erosion in concrete usually begins with wearing away of the matrix material around the aggregate, and appears as relatively uniform damage over a large surface. In a spillway, fall or escape, erosion is usually due to the movement of abrasive materials being carried by the flowing water. Aprons and stilling basins (also known as hydraulic jump basins or simply jump basins) are especially susceptible. Erosion often occurs after initially cavitation damage, and serves to increase and extend the damage. 60.Points of abrupt change in the flow channel or corners subjected to abrasive action are likely to show pronounced effects. Examples are: Bends leading from tunnels,Conduits, and chutes. Energy dissipators in stilling basins. 61. Ballmilling is a specific form of concrete erosion. Repeated rotation of debris (usually rocks) by discharging water grinds the surface, usually in a circular pattern. Stilling/hydraulic jump basins are prone to ball milling damage. If the flows continue for long time periods and if abrasive material is carried at relatively high velocities, extensive erosion damage to concrete structures results. Erosion in a

37

stilling/hydraulic

jump

basin

floor

can

excavate

enough

material to make the structure unstable. Leaking Joints 62. Joints may leak because of damage to waterstops or other joints problems. Innadequate Or Damaged Waterstops:

Figure 14 : Waterstop

63. Concrete channels and conduits & masonry spillways often include waterstops, which are continuous strips of waterproof material, usually metal, PVC, or rubber. During concrete placement, waterstops are embedded in joints between sections to prevent moisture from penetrating the joints by providing a restricted route for seepage water. If damaged waterstops no longer provide a continuous seal, extensive seepage through the joint could erode foundation material or promote freeze thaw damage to the joints. Figure 14 shows a typical waterstop.

38

Other Joint Problem:


Figure 15: Open joints in a channel

64. Joints should be inspected while dry if possible. Conduits also can be inspected just after dewatering, since water shoots back through the leaking joints, and the worst leaks can be identified. (Some leakage after dewatering is normal). Sometimes construction joint drawings and joint survey information exist, and provide useful reference when joint problems are suspected. The following points apply to inspection of joints. Soil fines oozing through a joint are evidence of seepage. Joints in concrete sections are often sealed with joint sealant, or plastic or rubber compression seals. When the sealant or seal is missing or hardened, the joint is exposed to damage. Vegetation in joints indicates damaged or missing joint sealant. INSPECTION TIP: - If the joint is located in a conduit running through the dam or canal embankment (as in case of HR at damsite, missing or defective joint sealant is cause for concern.

39

Surface Mapping 65. Surface mapping involves documenting concrete defects in a systematic manner. All types of deterioration should be included. Surface mapping can be accomplished using detailed drawings, photographs, or videotape. When photographs are used, a ruler or familiar object should be included to indicate scale. A grid is sometimes used to overlay a section of a drawing so the location of cracks and other defects can be shown easily. Figure 16 shows an example of surface mapping of concrete deterioration.
FIGURE-16. SURFACE MAPPING

CONCRETE DETERIORATION :

INSPECTION ACTIONS

66. Common sense and your organizations procedures must guide you in responding to concrete deterioration. If you observe cracking or other deterioration of concrete, you should . Use the SMPL rule to document the deterioration Sketch, measure, photograph and locate indicating direction (longitudinal, transverse, horizontal, vertical
40

or diagonal), deterioration.

size,

length,

width,

depth

of

. If surface maps exist, or if deterioration has been documented before, compare your observations with recorded date and document your findings. Be alert to other types of deterioration in the concrete that may be related to an overall problem.

Use a hammer or bonker to sound the concrete surface for drummy concrete. INSPECTION TIP : Immediately notify Executive Engineer of any deterioration that is extensive, has changed significantly since the previous inspection or appears to affect the integrity of the structure. Carry out IMMEDIATE repairs if deterioration in concrete reaches embedded reinforcement steel.

41

4. METAL PROBLEMS COMMON IN STRUCTURES Corrosion (Rust, Galvanic Action) 67. Corrosion is progressive deterioration resulting from

exposure to moisture acid and other corrosive agents, or electrolysis, and usually is marked by scaling or flaking, pitting, and color changes. Loss of paint or other protective coatings can leave a metal surface subject to corrosion, ESPECIALLY IF THE SURFACE is cycled between wet and dry. Unchecked corrosion eventually leads to failure of a metal structure. Fatigue: 68.Fatigue is loss of metal strength from repetitive loading such as being bent back and forth. Protrusions on metal components or components with moving parts are most likely to suffer fatigue. Distortions or cracked point may indicate sites where a metal structure suffers from fatigue. The process continues until the affected area cracks and/or breaks. Erosion : 69. Flow surface and areas around rivets and splice plates may be scoured by abrasive debris. Tearing and Rupture : 70. Tearing and rupture may result from impact, such as a log slamming into a steel lining. On structures, metal components are most likely to tear and rupture during storms or other occasions when flows are heavy. Tears and ruptures can cause a

42

metal structure to fail completely, or expose the structure to corrosion, cavitation, fatigue or other damage. Cavitation: 71. Cavitation of metal surfaces, such as metal conduits, can occur when high flow velocities exist on a flow surface with offsets and irregularities. The bubble collapse dynamics of cavitation cause pitting of the surface which results in progressive deterioration to the point of failure. As in concrete, the site of initial cavitation damage triggers the formation of another site downstream, so the process develops in a leapfrog pattern. Areas just downstream of gates and valves are susceptible. Cracking: 72. Cracking is usually induced by vibrations. Deformation: 73. Stress may deform metal shapes. (Egg-shaped pipe is an example.)

43

Chapter 2 OBSTRUCTIONS 1. An obstruction is an unauthorized or unplanned addition to a structure that reduces flow capacity.

Significance of Obstructions: 2. An obstructed spillway,escape or outlet works cannot perform its function properly. During a flood, if reduced flow capacity prevents the spillway or escapes from diverting enough water from the reservoir/canal or the outlet works from lowering the water level in reservoir/canal, the dam/canal embankment may be overtopped, and put in danger of failure. 3. Causes of Obstructions:

Figure 17 : Obstructions

OVERGROWN VEGETATION, Grass is the ideal cover for an earth-lined surface, shrubs, tall weeds, and trees reduce flow capacity. AQUATIC VEGETATION, Submerged aquatic plants such as water hyacinths can obstruct a submerged entrance channels to an outlet works. Algae is a problem at outlets.
44

Adjacent Slope Failure, Causes for slope failure include overly steep channel and bank slopes, drawn down of a reservoir/ canal bank in saturated bank material, and flow undercutting banks slopes due to: Unprotected soil High flow velocities Loose or deteriorated bottom and slope material Failed protective surface

Figure 18: Other Obstructions

DEBRIS, Dead trees, slide material, and other debris can form obstruction Sediment accumulation, vandalism, and beaver activity are also sources of debris. The approach channel, trash racks, and gates of an outlet works are liable to be obstructed by debris. BEAVER DAMS,: Beaver dams can obstruct channels, submerged structures, riser pipes, and box inlets. Manmade structures, Fences or boat docks sometimes are built on earth-lined spillways. Also, unauthorized flashboards sometimes are added to the control section for heading up water level. Watch for earth or concretediles or sills or wooden logs added to the crest near CR/HR to raise storage capacity. Chapter 3

45

DISPLACEMENT 1. Displacement occurs when a structure or component moves from its originally constructed position. Movements do occur as a result of seasonal temperature change or other causes. Such movements are taken into account in the design of a concrete structure. 2. Movement resulting in displacement can be caused by such factors as .. Abutment or foundation settlement or displacement. Chemical reactions in the concrete. Structural behavior of the dam. Other applied loadings of exceptional magnitude (e.g., uplift pressure, Earth-quake, extreme temperature variations).

FIGURE-19. MISALIGNMENT AND DIFFERENTIAL MOVEMENT

3. There are two main types of displacement in a concrete dam : misalignment and differential movement.

Misalignment.

46

4. Misalignment configuration.

is any variation from the original structural

Differential Movement. 5. Differential movement occurs when one part of the structure moves with respect to adjacent parts of the structure. Figure 19 presents examples of misalignment and differential movement. Detecting Displacement 6.You are most likely to detect displacement by using sighting techniques at the top of the structural member. Differential movement most often appears as deflection at joints between adjacent blocks. Other indicators of displacement include Volume change in the concrete. Closing or opening of joints. Loss of joint filler. Cracking. Debonding of lifts. Tilting, shearing, or shifting of hardware or machinery. Binding of gates. : INSPECTION ACTIONS.

DISPLACEMENT

7. Movement in and of itself is not bad. Small movements are of little concern and usually are considered in the design of the structure. Movement becomes significant when it has an adverse impact on the entire structure or on one or more of its parts. INSPECTION TIP : Significant changes either in

magnitude or in directions should be evaluated immediately consult Design Circle.

When you prepare for an inspection, you should47

Study data from previous inspection reports or derived from surveys, if available. Focus on areas of the structure where evidence of movement has been noted. When you inspect for displacement, you should Use sighting techniques along the top of the structural member to look for misalignment and differential movement. Inspect joints, hardware, and equipment for evidence of differential movement. Watch for structural cracking. Be alert for any changes in or new occurrences of displacement. For all displacement observed, record : o Location. o Extent. o Direction of displacement. o Any other evidence of movement. o Observations on date, time, and temperature. INSPECTION TIP : Make sure to record the relative water levels in the canal both upstream and downstream of the structure. Graphics or computer plots can be developed that allow you to distinguish between seasonal movement cycles and potential problems. SMALL SCALE MISALIGNMENT: Defining Small-Scale Misalignment 8. One type of small-scale misalignment, called differential movement, is localized movement of one section of a lining, wall ogee monolith, or other escape component relative to adjacent sections, Causes of differential movement include:

48

Loss of foundation or backfill Expensive clay shale foundation Poor drainage resulting in pressure behind the structure 9. Small-Scale misalignment may also result from misplacement during construction. Figure 20 shows an offset between sections of a chute. Pressures (possibly from poor drainage) have moved the sidewalls inward in the upper section of the chute). Significance of Small-Scale Misalignment: 10.Small-Scale misalignment is a significant problems because Offsets on flow surfaces can cause erosion and, in some cases, cavitation. Both can eventually cause the structure to fail. Gaps between joints allow water to penetrate and undermine foundation material, creating excessive uplift pressure, and/or allowing earth or rock material to escape. Compression across joint surfaces can result in concrete spalling metal deformation, or ruptured water stops Large-Scale Misalignment: Defining Large Scale Misalignment : 11. Large Scale Misalignment is the dislocation of entire structures from their design locations.

Causes of Large-Scale Misalignment:

49

12. One example of large-scale misalignment is a conduit that sags below its design horizontal centerline. Deformations of failures responsible for large-scale misalignment include: Over compacted backfill, excessive earth pressure, or hydrostatic pushing the structure out of position. Loss of backfill or foundation materials. Base spreading. Shear failure in foundation. Settlement of foundation. Seismic activity causing foundation collapse. 13. Large-Scale misalignment may cause a structure to fail. Landmarks, boundaries, and sighting techniques can be used to check for this problem.

Chapter 5 FOUNDATION AND BACKFILL PROBLEMS:


50

1. Foundation and backfill problems are related to many other problem conditions in spsillways and escapes both as the cause and as the result of this condition. For example, misalignment is often the result of foundation, backfill and drainage problems. (Gaps in channel joints caused by differential movement, for example expose the foundation to erosion). 2. Factors in Foundation and Backfill Problems: SEEPAGE. Seepage can move materials by piping undermining the foundation or backfill. A saturated soil base can shift or collapse EROSION: The foundation or backfill adjacent to channels or in the terminal area often suffers erosion damage. SETTLEMENT. Setting can cause misalignment. Foundation Faults. misalignment.

Foundation

faults

can

cause

Expansive Foundation. Structures built on an expansive clay or clay shale foundation are subject to heaving and misalignment across joints.

Chapter 6

51

SEEPAGE 1. Seepage is the slow percolation of water through the embankment and its foundation. What are Leakage and Seepage? 2. Some use the terms leakage and seepage interchangeably. For the purposes of this module: Leakage is the flow of water through joints, cracks, and openings in hydraulic structures. Seepage is the flow of water through the abutments or foundation of the dam. Significance of Seepage 3. Both the velocity and quality of seepage must be controlled or piping will occur. Piping is a term that describes internal erosion that begins at the downstream side of the embankment and continues at a progressive rate towards the reservoir until an internal pipe or direct conduit to the reservoir/canal has been formed. Rapid failure of the dam/ canal embankment results. Figure 21 shows one way a piping failure can occur from seepage through an outlet works.

52

4. A hole in the conduit allowed water to seep outside the conduit and move along the pipe to the toe of the dam/ canal. As the seepage water emerged from the embankment, it carried some of the embankment material with it, As the hole enlarged, seepage increased. The embankment was progressively eroded back toward the hole, forming a pipe through the embankment material. The piping failure was completed when sloughing of the embankment caused the dam/ canal to be breached.

Figure 21

EXAMPLE OF PIPING FAILURE

Characteristics of Leakage. 5. Leakage normally occurs through joints or cracks in the concrete. The main causes of leakage are the following : Cracks. Open joints. Broken seals. Leaking pipes or conduits. Deteriorated or defective concrete.

53

Evidence of leakage can vary from a moist or wet surface to a concentrated flow of water. The most common indicators of leakage in a concrete structure are: Wetness on the downstream face of the structure. Staining or buildup of sediments along joints and cracks. Water spurting or running out of joints or cracks on the downstream face. Significant flows in the drainage system, and formed drains, tail channels, river . 6. Leakage can result in an increased rate of deterioration of concrete, leaching of structural hydrostatics strength. pressure concrete, loss of mass, and reduced Leakage within can the also cause excessive leading to

structure,

overturning or sliding of blocks of the structure. Characteristics of Seepage : 7. Seepage through the foundation and abutments can be caused by the following conditions : Foundation deterioration. Inadequate grout curtain. Joints or seems in the foundation or abutment material. Evidence of seepage may include: Wet areas on the abutments or foundation downstream of the structure. Lush vegetative growth in an area downstream of the structure. Instability of the slopes (e.g., slumps and slides) downstream of the structure. Indications in instrument readings of undesirable hydrostatic pressure buildup. 8. The potential consequences of seepage include increased uplift pressure and differential movement in the structure.
54

Seepage also has the potential for solutioning soluble rock materials or instability (sliding) of the abutment or foundation and thus weakening the foundation, with potential failure as a consequence in some cases. In very basic terms, excessive leakage and seepage can lead to loss of usable water. Monitoring Leakage and Seepage. 9. All concrete structures leak and seep. The amount of leakage and seepage usually correlates with the water level in the reservoir/ canal. Generally, as the water level in the reservoir/ canal rises, the seepage flow rate increases. Temperatures also affect the amount of leakage during cold weather, concrete contracts and joints or cracks open, increasing leakage. 10. As part of your inspection, you should monitor the rate and trends of leakage and seepage. You will need to check previous records of leakage and seepage for comparable water surface elevations in the reservoir/canal so that you can compare your findings. You are looking for: Significant new leakage or seepage. Major changes in leakage / seepage pattern or flow. Turbidity in seepage. Turbidity. 11. Turbid water is cloudy, and is an indication that the foundation material may be eroding. INSPECTION TIP : Turbidity is cause for concern.

Each time seepage is measured, clarity should be evaluated.

55

Taking Measurements 12. Measure the amount of seepage and leakage and record in the Operating Log (LogBook). If previous records are not available for comparison, a program to collect flow data may need to be initiated. Dont forget to include the water level in the reservoi/ canal each time flows are measured. This will help determine the cause of a change in the amount of flow. Clarity of seepage i.e. whether clear or carrying sediment and any staining or discoloration of concrete is to be noted in the LogBook. There are various ways to take flow readings. The most common are: The use of weirs (refer to the module on instrumentation). The use of a bucket and stopwatch. Blocked Drains. 13. In monitoring leakage, increased flows are not the only cause for concern. A noticeable decrease in seepage can indicate that a drain is becoming blocked. Blocked drains can lead to deterioration of the concrete/ masonry, increased

uplift/hydrostatic pressures, and potential stability problems.

LEAKAGE AND SEEPAGE :

INSPECTION ACTIONS.

14. If you observe leakage or seepage, you should . Monitor the flow and record the following : Location and quantity or flow rate of all leakage and seepage at exit points. Occurrence of recent precipitation that may affect the appearance and quantity of seepage. Water level in the canal at the time of the observation. Check seepage for turbidity.

56

Document any suspected drain blockages. A recommendation that the drains be cleaned may be warranted. INSPECTION TIP : Consult Executive Engineer if you

observe significant new leakage or seepage, major changes in leakage / seepage pattern or flow, or turbidity in seepage.

57

Chapter 7.

POOR DRAINAGE

Weepholes and Drains 1. Structures commonly have weepholes or other means of drainage to prevent excess water pressure from developing behind a structure. When no weepholes or drainage systems exist, or when drains are plugged, excess water will accumulate. This is a problem for the following reasons: A saturated foundation has lower bearing capacity. Uplift pressure from seepage water may cause damage to a chute. Structure are designed for certain waterloads. If these hydrostatic pressures are exceeded because of defective drainage, then instability or distress can result. 2. Weepholes can become plugged by debris, infiltration of fines, iron incrustation, and carbonate deposits. An inspection sight includes probing weepholes to check for obstructions and recording depth measurements on the crack maps. Signs of poor drainage include: Ponding of water behind walls. Dampness on concrete surface, especially at cracks and joints. Moistures seeping through cracks or joints. Tilted walls or heaved slabs

58

Faulty Drainage: 3. You should-

Inspection Actions.

Observe the drain opening. Lock for deposits blocking the opening. Probe or sound drains to detect blockages. Check flow records for changes in flow rates that may indicate faulty drainage. Walk the gallery system and note the condition of gutters. Report gutter blockages and recommend prompt cleaning. Check pressure gauges.

59

PART III INSPECTION OF STRUCTURES

60

Chapter 8 INSPECTION OF SPILLWAYS, WASTEWEIRS & ESCAPES

1. Spillways, Wsateweirs and Escapes are constructed to release water in excess of the storage space in a dam/ canal. These are important to the safety of dams/ canals, and maintenance to allow proper functioning is essential. These usually are located to discharge away from the embankment in order to preclude erosion of the embankment when spilling. Regulated spillways/ escapes employ gates of various types to control the rate of flow through the structure. Structural instability is evidenced by deep cracks in slabs or walls, slab removal, foundation piping, tilting of walls, and misalignment of walls. Obstructions including debris, trash, trees, brush, and sediment diminish the flow capacities of escape structures, stilling basins, and inflow and outlet channels and may also produce undesirable erosionproducing currents. Weep holes and drainage openings are usually installed in the walls and floors of escape structures, and these often become clogged with sediment and may be occupied by animals or birds.

INSPECTION ACTION: Inspect Annually the escape structure and channel for instability, deterioration, obstructions, and erosion. Evidence of structural instability should be reported immediately, through Superintending Engineer in charge of the work to Design Circle who can assess significance and suggest appropriate action to be taken.

61

Structural deterioration that is progressive and endangering the structural integrity of the canal should be repaired. Obstructions including debris, trash, dead and live trees, and brush and sediment deposits should be removed. (Debris, trash, trees, and brush should be disposed of in accordance with forest and environmental regulations) 2. General inspection required as outlined vide Part II shall apply for all the components of spillways/wasteweirs/escapes. Following gives further details for inspection to be carried out. Checklist for inspection of spillways/wasteweirs/escapes is provided at the end of this chapter. Control Section: 3. The control section is a particularly critical portion of a spillway/wasteweir/ escape, as it receives flow of water from the reservoir/canal and passes on to river/ tail channel via energy dissipation system. It may also be in the form of a weir with crest (or sill level) raised above ground/canal bed level. The spillway/wasteweir/escape must begin releasing water as

intended by design, whether the flow is triggered, when canal water level reaches a predetermined level or through the operation of gates or the removal/failure of stoplogs. The most serious danger posed by the inability of the control section to operate properly is that the water level in reservoir/canal may rise and overtop the banks. Problems typical to the escape control section include: Deterioration of surface materials:Check the following points for deterioration in the control section:

62

Look at surfaces in areas of concentrated and high velocity flows, such as near gates, for erosion. Check areas near large gates for cracking in concrete, and tearing, rupture, and fatigue in metal. Examine the upstream edges of weirs for damage from battering by debris. A boat may be used to inspect the upstream side of a weir immediately adjacent to the water level. INSPECTION TIP : High velocity flow over a concrete surface containing abnormalities can initiate cavitation damage. Check surfaces carefully for offsets, small holes and calcium carbonate deposits. The bearing surfaces where gates rest and areas immediately downstream of gate slots, liner plates and air vents should be examined with special care.

Obstructions: 4. Besides general types of obstructions already discussed, check for the following obstructions to control sections: Check for unauthorized equipment added to the control section. Backfill and Foundation Deficiencies: 5. Points to remember when inspecting the control section for backfill and foundation deficiencies are: Foundation in the control section often must bear the stress of heavy equipment. Check carefully for displacements that may indicate settling foundation shifts, or undermining. Check for voids under concrete channel walls and floors. It is critical that gaps in joints do not expose foundation or backfill material where escape extends through the
63

embankment section, and that water stops, sealants and compressive joint fillers are intact and in good condition. Check for clogged weep holes and foundation drains if present and watch for seepage and other signs of problems with the drainage system. Operating Bridge And Pier Problems: 6. Deficiencies in the operating bridge, piers, decks, or other access structures on the spillway/wasteweir/escape could make gates and other controls unworkable in an emergency, and collapse of the supporting structure could obstruct the spillway/wasteweir /escape. 7. Check for the following deficiencies. On concrete bridges, check joints and water runoff points for exposed metal and corrosion of reinforcement steel. Check for peeling or missing paint On steel flashing over joints inspect for break down of welds or mechanical connectors, couplings, and flanges. Look for loose or insecurely anchored guardrails. Check the condition of previously repaired areas. Check & clear bridge drains every quarter 8. Check bridge support as follows. On concrete bridge supports look for stress cracking. Check the bearing supports at the abutments for condition and evidence of movement. Look for misalignment or damage at sliding joints.

64

Problems With Gates, Stoplogs: 9. When inspecting the control section of a spillway/wasteweir/escape, your primary concern is to ensure that the operation of gates and other

reservoir/canal evacuation equipment is not impaired by adjacent and supporting structures. 10. When inspecting, stoplogs and structures adjacent to and supporting gates check the following points. Look for displacement of structural elements or concrete deterioration that may be jamming or misalignment gates. Have the equipment operated if possible, to detect jamming, or gates not seated properly on the crest. During operations, look for deterioration of material on the underside of the gates. Note excessive leakage. Watch for misalignment of gate stems and other signs of strain from holding water or from debris or over tightening. Mechanical Equipment 11. All accessible parts of mechanical and associated electrical equipment should be inspected visually every year for damaged, deteriorated, corroded, cavitated, loose, worn, or broken parts.

12. Mechanical and electrical equipment should be lubricated at periodic intervals. The service and maintenance procedures prescribed by the manufacturer should be followed for pumps, motors, and other commercial components, where available.

65

Proper lubrication reduces the friction and wears between sliding parts, protects against corrosion, and carries away contaminants. For electrical equipment, the use of desiccants is helpful to increase equipment life and reduce trouble.

13. All mechanical and electrical equipment with moving parts should be exercised by operating through the full travel range under actual operating conditions, if possible, and at regular intervals. A log of such operations should be maintained. Periodic operation of equipment removes foreign material from sliding surfaces, distributes lubricants, and flexes packing and seals.

14. AlI exposed metal surfaces (not in sliding contact), other than corrosion resistant materials, should be properly protected or painted to prevent deterioration. Operating instructions should be posted within protective coverings, such as clear plastics, near associated equipment so that equipment can be operated as intended. Each operating device should be

permanently and clearly marked for easy identification.

15. Adequate physical security should be provided to preclude unauthorized tampering with and operating of equipment. Such security may include chaining and locking outside gate

operators and constructing and locking adequately restrictive barriers, covers, or enclosures.

66

Inspection of Gates and valves (annual). (1) Visual inspection. When water conditions permit, inspect the downstream surfaces of the guard gate leaves and bodies, the upstream and downstream surfaces of regulating gate leaves and bodies, and outlet pipes. Particular attention should be given to signs of cavitations damage to waterway surfaces downstream from gate or valve leaves and flanged joints. Inspect neoprene or rubber gate seals for deterioration, cracking, wear, foreign material deposits, and leakage. Inspect valve and gates metal seats or seals for wear, scratches, foreign material deposits, and leakage. Repairs should be made as necessary to keep the equipment in a safe and reliable operating condition. (2) Exercising After lubrication, operate each valve and gate through a full cycle while under actual operating conditions, if possible. During operation, listen for unusual noises and check for binding or vibration. Inspection of Hydraulic and manual operators and control systems for gates and valves (annual) (1) Visual inspection Check hydraulic oil in the tank for proper fluid level (take into account displacement of the gate stem), water, and foreign materia1. Check all pipe joints, cylinder flanges, packing, and hydraulic equipment for leaks.

67

Check oil filters and strainers and change or clean if required. Check hydraulic hoist piston stem for rusting and foreign deposits. Remove deposits and rough areas on stems to prevent damage to packing or seals. (2)Exercising Operate hydraulic control and manual operator systems and check for unusual noises or vibrations. Check motors and hydraulic fluids for overheating, and check pressure switches, pressure gages, and limit switches for proper operation according to operating instructions. Clean manual operators of dirt and foreign material and lubricate as appropriate. 16. Physical security - The physical security should be inspected for adequacy and repairs and improvements made, as necessary, to avoid unauthorized operation and ensure the safety of the equipment.

Inspection of Traveling crane, hoist, and tracks (annual) (1) Visual inspection Examine hoist, crane, and tracks for broken, bent, misaligned, worn, or loose parts and corrosion and deterioration of protective coatings. (2)Exercising After lubrication, operate crane and hoist throughout all functions and check for unusual noises, binding, and vibration during operation.

68

ENERGY DISSIPATION SECTION: 17. Use these general guidelines during your inspection of the energy dissipation section of a spillway/wasteweir/escape or HR/outlet works: First and foremost, know how the structures are supposed to function. Make close observations of the structures when in use. Note unusual water currents, eddies and swirls, especially return currents that would carry rock and debris into the structure from downstream. Look for Sand boils which result from the upward flow of seepage under pressure and are characterized by a boiling action of the surface seepage. A sand boil is often accompanied by a cone of material around the boil which develops from the deposition of foundation or embankment material varied by the seepage. If possible, dewater the pool to inspect surfaces for damage. To inspect a large pool that cannot be dewatered, plan a boat inspection and record soundings made A plumb bob/ surveying equipment may be needed to determine the location of subsurface damage. Underwater inspections by divers are recommended if problems are suspected. As with any underwater inspection, a detailed inspection, a plan and a good communication system are important considerations for logging damaged areas. Typical Problems With Energy Dissipation Section: 18. Damage can occur to all elements of an energy dissipation section because these structures reduce the velocity and dissipate the energy of a flow. If the energy dissipation structure

69

fails to operate properly the main structure can be eroded at the down stream end, causing a loss of foundation support. Problems typical to the energy dissipation section include the following: Deteriaration of Materials: 19. Follow the actions described in Table-1 Inspection of Energy Dissipation materials to check for deterioration of materials. TABLE 1 INSPECTION OF ENERGY DISSIPATION MATERIALS Concrete Check for signs of cavitation. The sides of chute blocks baffles. And dentates are exposed to considerable turbulence, and any offsets or irregularities can trigger cavitation. Look for erosion damage from abrasion of wasteweir aprons, the top surfaces and undersides of buckets, and the floors, walls chute blocks and dentates of stilling basins. See if ball milling has ground circular patterns in the floor or apron of stilling / hydraulic jump basins. Check joints for spells or settlement on one side. See if joint sealant or compressive joint filler is cracked missing, moved, or deteriorated. Look for broken waterstops. Watch for corroded and damaged reinforcement resulting from erosion and cavitation damage. Concrete

70

terminal structures reinforced.

are

always

Inspect the submerged portions of plunge pools and stilling / hydraulic jump basins while dewatered, if possible or use divers. (An underwater camera or a remotely operated vehicle (ROV) might be used before divers.) Riprap/Pitching Make sure that riprap/pitching is not displaced or lost and that foundation material is protected. Look for piping or voids beneath riprap/pitching. Check riprap or gabion plunge pools and downstream channels for exposed geotextiles, which typically should not be exposed to direct flow or sunlight.

Geotextiles

20. Obstructions: Check energy dissipation sections for the following obstruction: Debris clogging baffles Plunge pools, stilling / hydraulic jump basins, and areas down stream of flip buckets filling with debris (often rocks and other objects thrown by people) Return currents bringing downstream materials into the structure Heavy vegetative growth (such as thick grasses) in plunge pools. If you see material blocking flow note the type of material dimensions and depth, and location relative to a side or an end. A boat can be used to perform a hydrographic survey of a large pool bottom to check for obstructions or damage.
71

21. Damaged Or Missing Baffles: Baffles may be cracked severely eroded loose or missing. 22. Misalignment Of Walls Or Baffles: deflect the portion of terminal structures. Check for vertically, and sight along the top of a sill for alignment deviation. Check instrumentation data to measure deflections. Offsets may occur as a result of misalignment, and cavitation can developed downstream of such offsets. 23. Malfunctioning Drains: Check for clogged drains in the energy dissipation area. Determine whether water flowing from drains is clear or contains sediment or fine materials. 24. Backfill And Foundation Deficiencies: Check the following points when inspecting the energy dissipation section for backfill and foundation deficiencies: Inspect plunge pools, hydraulic jump basins, and ripraplined dissipators carefully for foundation and crack fill problems. Look for settlement and cracks in backfill. Measure the size and distance of problem areas measure settlement depth and probe for voids and erosion channels. Watch especially for erosion of backfill behind the downstream portion of a stilling / hydraulic jump basins cutoff walls and reinforcement should not be visible. Settlement or improper elevation or length may change the jump location is stilling / hydraulic jump basins. Check that jump within the structure occurs at design locations (If the spillway/wasteweir/escape or HR/outlet works is
72

The force of flows may

not operating, water stains on the walls will indicate where the jump is actually occurring). Look for misaligned dry walls, cracks in the basin, and cracked backfill for evidence that a jump basin is settling. Check a riprap plunge pool for undermining by loss of underlying soil or lack of filter action. If a plunge pool lining is sand or gravel, check for piping. TAIL CHANNEL 25. The tail channel discharges the flow from

spillway/wasteweir/escape into nearby river or nalla or even drain. If it fails, excess discharge is likely to erode the lower portion of the spillway/wasteweir/escape control section or energy dissipation system, the groin and toe areas of

embankment or areas downstream of the spillway/wasteweir/ escape. Tail channel is subject to the same general problems with structure and material as Approach channel of the drainage siphon, with additional concerns described below: Erosion: Discharge entering the tail channel is generally at a higher velocity than flows through the approach channel.The tail channel is very susceptible to erosion if not properly sized, aligned and protected from excess velocity. Look for erosion gullies that may indicate improper compaction, overtopping because of downstream obstructions or poor vegetative cover. Inadequate Length: The tail channel should extend far enough downstream to ensure that flows will not damage the embankment groin and toe areas. If damage is occuring, it is extremely important to note the deficiency.

73

CHECKLIST FOR EXAMINATION OF SILLWAY/WASTEWEIR/ESCAPE ______________________ dam/ canal Chainage _______________

Date of Examination _________________

Signature Completed _________________________

Operational Status at Time of Examination Water Surface-Elevation Releases: Escape Outlet Works for irrigation Water supply __________ m3/s __________ m3/s __________ m3/s __________ M

Examination Participants Name Affiliation

_____________________________________________________________ _____________________________________________________________ _____________________________________________________________ _____________________________________________________________

GLACIS OF WASTE WEIR/SPILLWAY Debris Crest Surface condition(Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) _________________ General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) __________________ Cracks or areas of distress Sign of movement ______________________ ______________________ ______________________

Training Walls Surface condition(Observe Cracks / Honey comb / stratification /

74

Form slippage / Stains / Bar Projection) ____________________ General condition of concrete (Observe Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ Signs of Movement (offsets/Misalignment/Differential movement) ________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Cracks or areas of distress(Measure location/extent) ______________________

Condition of backfill (watch for seepage/erosion/settlement) _____________________ Functioning of weep holes(Whether clean/choked) Seepage(Record stains at joints/ turbidity) Debris( If present at at joints/lift joints) ______________________ ______________________ ______________________

Floor/apron/cistern Surface condition (Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ______________________ General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ Signs of Movement (offsets/Misalignment/Differential movement) ________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Seepage(Record stains at joints/ turbidity) Amount of flow Location of seeping drains Endsill alignment(Watch for Damage/ distortion) ______________________ ______________________ ______________________ ______________________

Backfill beyond endsill (Watch for erosion/Reinforcement visibility) _______________ TAIL CHANNEL Slope protection Stability of side slopes Vegetation or other obstructions Any other deficiency GATES Description ______________________ (Scour, Retrogression) ______________________ ______________________ ______________________ ______________________

General Condition(watch for corrosion/fatigue/rupture/cavitations of metal &position of welds) Protective coating ______________________ ______________________

75

Leakage (In closed condition at seal/through concrete) Condition of rubber seals

______________________ ______________________

Alignment of gate stem Exercising frequency Operation during inspection (Raise & lower fully

______________________ ______________________

if loss of water is not a problem) ___________________ CONTROLS FOR GATES Mechanical Hoists(watch for wear of brakeshoe lining / key-bolts are tightened/ handcranks in locked position ) Wire ropes( watch for rusting/ breakage/reduction in diameter/ condition of socket--clamps) Protective coatings(watch if peeling/missing) ______________________ ______________________ ______________________

Condition of hoist platform (Watch for rusting/ loss of weld/bending/ misalignment/movement) Guard rails(Watch for damage/ loss of sleeves/coupling /check anchors) Change of oil (Gear box) Condition of Gear teeth (Check for damage/wear/cracks) Lubrication ( Of ropes/bearing points/Pinions/Hinges/ Spin gear/Chains) Electrical Power supply Standby power Operation instructions STOPLOGS General condition Protective coating(watch if peeling/missing) Seals BRIDGE Condition of piers (Leaks / Staining / Projection) ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

76

Surface of roadway slab Water Spouts (whether choked) Condition of parapet/Guard rails (watch for misalignment/ differential settlement)

______________________ ______________________

______________________

Structural condition of slab and beams (watch for Deflection / Cracks) ______________________ Bridge bearings ______________________ Overall condition OTHER POINTS ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

77

Chapter 9 INSPECTION OF CANAL SIPHON 1. Canal siphons consist of gated or ungated conduits (RCC barrels or pipes ) with upstream and downstream transitions. General inspection required as outlined vide Part II shall apply for all the components of canal siphon. Following gives further details for inspection to be carried out. Checklist for inspection of canal siphon is provided at the end of this chapter. Barrels / Pipes (Conduits) 2. A conduit is a pipe or box structure constructed by joining sections.All outlets, HRs, canal siphons and drainage siphons can generally be termed as conduits.

External Inspection Procedures for Conduits: 3. Evidence of potential conduit problems may BE found by examining external features of the conduit (if it is exposed) or the embankment. If the material is reaching its life expectancy, it may be possible to dig down to expose all sides of the conduit at a point where the surrounding soil is still damp. Examine the outside of the conduit for signs of deterioration. The condition of the outside of the conduit could be significantly different from the interior. In some cases the soil protects the exterior from oxygen-induced corrosion. On the other hand local site conditions may have accelerated the deterioration of the exterior. Consider the outside of the conduit to be just one indicator. ** Look for signs of infiltration of soil into the conduit:

78

Sinkholes and piping cavities that exit the surface. Holes taken over by animals may not be easily recognized as sinkholes or piping cavities. Holes that appear to be in a line. These may be an indication that piping or settlement is occurring. Fines in the discharged water. ** Look for seepage or indications that seepage is sometimes present. (This is best done while the conduit is full). Indications of seepage are: Wet spots Increased vegetation or the presence of plants that thrive in wet ground. ** Watch for water flow when all intakes are closed. If any is observed, double-check to see if intakes are leaking. If not document where water is entering the waterway, and examine the water for fines. ** Look for piping related erosion around the conduit near the downstream end. Check for seepage adjacent to the structure. The situation may be especially serious if the seepage is carrying sediment. ** With exposed conduit, check the support for settlement of movement of the joints. Internal Inspection Procedures for Conduits: 4. To attempting to inspect conduit interiors, you may experience the following difficulties: ** Dewatering difficulties: You cannot inspect a conduit comprehensively unless it has been dewatered. However, dewatering may be impractical or impossible for one or more of the following reasons. The need to limit maximum drawdown

79

The need to maintain water flows. Structural inadequacy of the conduit to withstand hydrostatic pressure in a dewatering condition.

To assess the probable condition of the conduit interior, it may be necessary to rely on results of the exterior inspection. ** Inaccessibility of conduit interior- The conduit may be too dangerous for internal inspection by a person. One possibility is to use remotely operated video equipment. If that is not feasible, the inspection must be based on: - The condition of the exposed portion of the conduit or the embankment above it. The internal inspection of accessible portions of the conduit. (some details can be observed from the downstream end of the conduit with the aid of a strong light and possibly a mirror).

INSPECTION TIP : One indication of settlement related problems that may be observed from the downstream end of a conduit is the pending of water in certain reaches of pipe. 5. A deficiency commonly encountered in the internal inspection of conduit is cracking. Be aware of previously reported cracks and note any new cracks, using a crack map or similar reporting method. Figure --- shows one page of a crack map prepared by an inspection team. Cracks should be documented as fully as possible, with measurements and/or sketches drawn to scale showing the length and position of each crack. The crack map in figure includes measurements of the depth of weep holes, which were probed during the inspection.

80

6. To get some indication of whether cracks are continuous through a concrete structure, use a geologists' pick or other hammer to tap the concrete. More comprehensive studies of the concrete using dye tests and sonic methods may be necessary if there are indications that the crack extends any distance into the structure. 7. When inspecting the interior of a conduit, document the following: ** Cavitation damage downstream, from gates and at sharp bends, joints or other discontinuities. Corrosion of metal conduit or liner. Cracking: Use crack maps, Describe position, length and orientation (Transverse, longitudinal, or diagonal) Estimate the depth of the crack. Damaged coating or lining materials. (Cracking or buckling is a sign of structural stress Missing chunks can cause cavitation). Debris impact. Deformation of the conduit shape. Efflorescent or gel on the concrete. (Indicates possible chemical deterioration of the concrete). Erosion, especially in areas of high-velocity flow. Joint separation, compression, or deterioration. Mention any unsound welds, rivets, or flanges. Leakage from the conduit, or seepage entering the conduit. Misalignment of sections of the conduit.

** **

**

** ** **

** **

** **

81

** **

Plugged drain holes. Voids behind the conduit near any observed cracks, misalignments or other areas of possible seepage.

8. Problems with conduits occur most often at joints, and special attention should be given to them during inspection. Open joints can permit erosion of envelope material or cause leakage of water into the embankment during pressure flow. Joints in conduits should be inspected in dry conditions, if possible. Inspection just after a conduit is dewatered may reveal the locations of leaks, because water sometimes spurts through affected joints. 9. Typically, conduit joints pull apart under the lowest part of siphon and are under compression at the end. When inspecting conduit joints be sure to: ** ** ** ** Examine joints for leaks Examine the joints between adjacent sections of conduit for leaks and for ruptured water stops. Look for compression spalling of concrete. Check for misalignment of sections due to differential settlement.

82

Figure shows a conduit joint which has opened along the bottom due to localized settlement along the conduit. Operating Bridge And Pier Problems: 10. Deficiencies in the operating bridge, piers, decks, or other access structures on the siphon could make gates and other controls unworkable in an emergency, and collapse of the supporting structure could obstruct the escape. 11.Check for the following deficiencies. On concrete bridges, check joints and water runoff points for exposed metal and corrosion of reinforcement steel. Check for peeling or missing paint On steel flashing over joints inspect for break down of welds or mechanical connectors, couplings, and flanges. Look for loose or insecurely anchored guardrails. Check the condition of previously repaired areas. 12. Check bridge support as follows. On concrete bridge supports look for stress cracking. Check the bearing supports at the abutments for condition and evidence of movement. Look for misalignment or damage at sliding joints. Problems With Gates, Stoplogs: 13. When inspecting the control section of a siphon, your primary concern is to ensure that the operation of gates and other canal evacuation equipment is not impaired by adjacent and supporting structures.

83

When inspecting, stoplogs and structures supporting gates check the following points.

adjacent to and

Look for displacement of structural elements or concrete deterioration that may be jamming or misalignment gates. Have the equipment operated if possible, to detect jamming, or gates not seated properly on the crest. During operations, look for deterioration of material on the underside of the gates. Note excessive leakage. Watch for misalignment of gate stems and other signs of strain from holding water or from debris or over tightening. Inspection of Gates and valves (annual). (3) Visual inspection. When water conditions permit, inspect the downstream surfaces of the guard gate leaves and bodies, the upstream and downstream surfaces of regulating gate leaves and bodies, and outlet pipes. Particular attention should be given to signs of cavitations damage to waterway surfaces downstream from gate or valve leaves and flanged joints. Inspect neoprene or rubber gate seals for deterioration, cracking, wear, foreign material deposits, and leakage. Inspect valve and gates metal seats or seals for wear, scratches, foreign material deposits, and leakage. Repairs should be made as necessary to keep the equipment in a safe and reliable operating condition. (4) Exercising After lubrication, operate each valve and gate through a full cycle while under actual operating conditions, if possible.
84

During operation, listen for unusual noises and check for binding or vibration. Inspection of Hydraulic and manual operators and control systems for gates and valves (annual) (1) Visual inspection Check hydraulic oil in the tank for proper fluid level (take into account displacement of the gate stem), water, and foreign materia1. Check all pipe joints, cylinder flanges, packing, and hydraulic equipment for leaks. Check oil filters and strainers and change or clean if required. Check hydraulic hoist piston stem for rusting and foreign deposits. Remove deposits and rough areas on stems to prevent damage to packing or seals. (2)Exercising Operate hydraulic control and manual operator systems and check for unusual noises or vibrations. Check motors and hydraulic fluids for overheating, and check pressure switches, pressure gages, and limit switches for proper operation according to operating instructions. Clean manual operators of dirt and foreign material and lubricate as appropriate. 14. Physical security - The physical security should be inspected for adequacy and repairs and improvements made, as necessary, to avoid unauthorized operation and ensure the safety of the equipment.

85

Inspection of Traveling crane, hoist, and tracks (annual) (2) Visual inspection Examine hoist, crane, and tracks for broken, bent, misaligned, worn, or loose parts and corrosion and deterioration of protective coatings. (2)Exercising After lubrication, operate crane and hoist throughout all functions and check for unusual noises, binding, and vibration during operation. Energy Dissipation Section: 15. Use these general guidelines during the your inspection of the energy dissipation section of a canal siphon: First and foremost, know how the structures are supposed to function. Make close observations of the structures when in use. Note unusual water currents, eddies and swirls, especially return currents that would carry rock and debris into the structure from downstream. Look for Sand boils which result from the upward flow of seepage under pressure and are characterized by a boiling action of the surface seepage. A sand boil is often accompanied by a cone of material around the boil which develops from the deposition of foundation or embankment material varied by the seepage. If possible, dewater the pool to inspect surfaces for damage. Underwater inspections by divers are recommended if problems are suspected. As with any underwater inspection, a detailed inspection, a plan and a good

86

communication system are important considerations for logging damaged areas. Typical Problems With Energy Dissipation Section: 16. Damage can occur to all elements of an energy dissipation section because these structures reduce the velocity and dissipate the energy of a flow. If the energy dissipation structure fails to operate properly the main structure can be eroded at the down stream end, causing a loss of foundation support. 17. Problems typical to the energy dissipation section include the following: Deteriaration of Materials: 18. Follow the actions described in Table--2 Inspection of Energy Dissipation materials to check for deterioration of materials. TABLE 2 INSPECTION OF ENERGY DISSIPATION MATERIALS Concrete Check for signs of cavitation. The sides of chute blocks baffles. And dentates are exposed to considerable turbulence, and any offsets or irregularities can trigger cavitation. Look for erosion damage from abrasion of wasteweir aprons, the top surfaces and undersides of buckets, and the floors, walls chute blocks and dentates of stilling basins.

87

See if ball milling has ground circular patterns in the floor or apron of stilling / hydraulic jump basins. Check joints for spells or settlement on one side. See if joint sealant or compressive joint filler is cracked missing, moved, or deteriorated. Look for broken waterstops. Watch for corroded and damaged reinforcement resulting from erosion and cavitation damage. Concrete terminal structures are always reinforced. Inspect the submerged portions of plunge pools and stilling / hydraulic jump basins while dewatered, if possible or use divers. (An underwater camera or a remotely operated vehicle (ROV) might be used before divers.) Riprap/Pitching Make sure that riprap/pitching is not displaced or lost and that foundation material is protected. Look for piping or voids beneath riprap/pitching. Check riprap or gabion plunge pools and downstream channels for exposed geotextiles, which typically should not be exposed to direct flow or sunlight.

Geotextiles

19. Obstructions: Check energy dissipation sections for the following obstruction: Debris clogging baffles Plunge pools, stilling / hydraulic jump basins, and areas down stream of flip buckets filling with debris (often rocks and other objects thrown by people)

88

Return currents bringing downstream materials into the structure Heavy vegetative growth (such as thick grasses) in plunge pools. If you see material blocking flow note the type of material dimensions and depth, and location relative to a side or an end. A boat can be used to perform a hydrographic survey of a large pool bottom to check for obstructions or damage. 20. Damaged Or Missing Baffles: Baffles may be cracked severely eroded loose or missing. 21. Misalignment Of Walls Or Baffles: deflect the portion of terminal structures. Check for vertically, and sight along the top of a sill for alignment deviation. Check instrumentation data to measure deflections. Offsets may occur as a result of misalignment, and cavitation can developed downstream of such offsets. 22. Malfunctioning Drains: Check for clogged drains in the energy dissipation area. Determine whether water flowing from drains is clear or contains sediment or fine materials. 23. Backfill And Foundation Deficiencies: Check the following points when inspecting the energy dissipation section for backfill and foundation deficiencies: The force of flows may

89

Inspect plunge pools, hydraulic jump basins, and ripraplined dissipators carefully for foundation and crack fill problems. Look for settlement and cracks in backfill. Measure the size and distance of problem areas measure settlement depth and probe for voids and erosion channels. Watch especially for erosion of backfill behind the downstream portion of a stilling / hydraulic jump basins cutoff walls and reinforcement should not be visible. Settlement or improper elevation or length may change the jump location is stilling / hydraulic jump basins. Check that jump within the structure occurs at design locations (If the escape or outlet works is not operating, water stains on the walls will indicate where the jump is actually occurring). Look for misaligned dry walls, cracks in the basin, and cracked backfill for evidence that a jump basis is settling. Check a riprap plunge pool for undermining by loss of underlying soil or lack of filter action. If a plunge pool lining is sand or gravel, check for piping.

90

CHECKLIST FOR EXAMINATION OF CANAL SIPHON _____________________Canal offtaking from ______________________ canal

Chainage _______________ to _________________

Date of Examination _________________

Signature Completed _________________________

Operational Status at Time of Examination Canal Water Surface-Elevation Releases: Escape Outlet Works for irrigation Water supply __________ m3/s __________ m3/s __________ m3/s __________ M

Examination Participants Name Affiliation

_____________________________________________________________ _____________________________________________________________ _____________________________________________________________ _____________________________________________________________

APPROACH CHANNEL General condition (Siltation/Debris) Vegetation (trees, willows etc.) Slides above channel (Deep / Shallow) Channel side slope stability ______________________ ______________________ ______________________ ______________________

Slope protection(Adequacy / Degradation / Displacement) ______________________ BARREL Entrance transition Debris (Watch if coming out from joints) Surface condition (Cracks / Honey comb / stratification / 91 ______________________

Form slippage/ Stains/Bar Projection) ______________________ General condition (Disintegration / Spalling / Drummy Concrete /Pop out / Pitting / Sealing) Settlement Joints(If washed out/crack/differential movement /vegetation growth) Cracks/Area of distress (Measure location/extent) Seepage(Record stains a tjoints / turbidity ) Walls Surface condition(Observe Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ____________________ General condition of concrete (Observe Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Cracks or areas of distress(Measure location/extent) ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

Condition of backfill (watch for seepage/erosion/settlement) _____________________ Seepage(Record stains at joints/ turbidity) Debris( If present at at joints/lift joints) Floor Surface condition (Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ______________________ ______________________ ______________________

General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ Signs of Movement (offsets/Misalignment/Differential movement) ________________ Joints(If washed out /crack/differential movement /vegetation growth) _____________ Seepage(Record stains at joints/ turbidity) Amount of flow Location of seeping drains Endsill alignment(Watch for Damage/ distortion) ______________________ ______________________ ______________________ ______________________

Backfill beyond endsill (Watch for erosion/Reinforcement visibility) _______________ BRIDGE Condition of piers (Leaks / Staining / Projection) ______________________ 92

Surface of roadway slab Water Spouts (whether choked) Condition of parapet/Guard rails (watch for misalignment/ differential settlement)

______________________ ______________________

______________________

Structural condition of slab and beams (watch for Deflection / Cracks) _____________________ Bridge bearings ______________________ Overall condition TAIL CHANNEL Slope protection Stability of side slopes Vegetation or other obstructions Any other deficiency GATES Description ______________________ (Scour, Retrogression) ______________________ ______________________ ______________________ ______________________ ______________________

General Condition(watch for corrosion/fatigue/rupture/cavitations of metal &position of welds) Protective coating Leakage (In closed condition at seal/through concrete) Condition of rubber seals ______________________ ______________________ ______________________ ______________________

Alignment of gate stem Exercising frequency

______________________ ______________________

Operation during inspection (Raise & lower fully if loss of water is not a problem) ____________________ CONTROLS FOR GATES Mechanical Hoists(watch for wear of brakeshoe lining / key-bolts are tightened/ handcranks in locked position ) Wire ropes( watch for rusting/ breakage/reduction in diameter/ condition of socket--clamps) Protective coatings(watch if peeling/missing) ______________________ ______________________ ______________________

Condition of hoist platform (Watch for rusting/ loss of weld/bending/ 93

misalignment/movement) Guard rails(Watch for damage/ loss of sleeves/coupling /check anchors) Change of oil (Gear box) Condition of Gear teeth (Check for damage/wear/cracks) Lubrication ( Of ropes/bearing points/Pinions/Hinges/ Spin gear/Chains) Electrical Power supply Standby power Operation instructions STOPLOGS General condition Protective coating (watch if peeling/missing) Seals TRASH RACKS OTHER ______________________ ______________________

______________________

______________________ ______________________ ______________________

______________________

______________________ ______________________ ______________________

______________________ ______________________ ______________________ ______________________

______________________ ______________________

94

Chapter 10.

INSPECTION OF DRAINAGE SIPHON

1. Drainage siphons consist of conduits (RCC barrels or pipes ) with upstream and downstream transitions, approach and tail channel. General inspection required as outlined vide Part II shall apply for all the components of drainage siphon. Following gives further details for inspection to be carried out. Checklist for inspection of drainage siphon is provided at the end of this chapter. Approach Channel : Typical Problems

2. Failure of the approach channel may block flow to the drainage siphon entirely, greatly reduce the flow capacity, or cause flow irregularities that imprnage upon or overtop channel walls. As a result, the water surface in the drain may be raised above safe levels, and the canal bank may even be overtopped. 3. Approach channels may be affected by: Deterioration of Materials. Slope and wall failure may result when surface materials deteriorate. To inspect for deterioration of surface materials perform the actions listed in Table : 2 Inspecting approach channel Materials.

95

TABLE

2 INSPECTING APPROACH CHANNEL MATERIALS

INSPECTION POINT Check concrete linings for cracks, displacement, and erosion Sight along the walls to make sure that they have not moved. RCC, Shotcrete Check for cracks and erosion Aaphaltic Concrete Check for cracks, erosion, and disintegration Earth Note any severe erosion gullies Rock Look for excessive deterioration of rock in natural rock channels Check riprap for weathering deterioration of stone, and slides in sides walls. GABIONS Note signs of gabion settling or rock deterioration. Check baskets for rusted, broken, cut, or deform wires. NOTE :- Gabions are wire cages filled with rocks that can be piled up for slope stabilization. 4. OBSTRUCTIONS. Approach channels may be obstructed by: Vegetation Debris Sediment Fallen rocks Trees Manmade structures

MATERIAL Concrete

To inspect for obstructions in the approach channel, take these actions: Check the channels for debris. Record the type, location and extent of any obstruction.

96

5. Slope And Wall Failure. While inspecting the approach channel for slope and wall failure, do the following: Examine the side slopes or walls for slides, movement, cracked or wet spots. Check for foundation undermining by flow from springs. Look at the topography above the channel for signs of instability, such as sinkholes or slumps behind the walls. If you see soil loss with seepage, look for an exit points. Check for indications of poor drainage, such as seepage and clogged weepholes or drains. 6. Poor Floor Condition or Stability. Check these points when examining the entrance channel floor. If the channel is unlined: o Look at the toe of the channel slope for wet areas. o Check for erosion sinkholes and lack of vegetation. Check foundation foe signs of undermining by clow from springs. Look for signs of poor drainage, such as seepage and clogged weepholes or drains, Inspect for voids under a concrete floor, using a bunker or a hammer. (Another device that may be used is a Chain drag which is a series of chains fastened to a bar. Concrete is sounded by dragging the chains over a surface. This device is used to test large areas).
7. Concrete Deteriaration From Wetting/Drying. Concrete

deteriorates from wetting and drying as the water level rises and falls. The waterline of the approach channel needs to be checked for cracking, scaling and crumbing of the concrete surface.

97

8. Wave Erosion.

Check side slopes or pitching for beaching

from wave erosion. The overly-steep channel slope above the beach may fail.

9. Insufficient Capacity. If you see evidence of overtopping and a flow restriction does nor appear to be contributing factor, recommended that a hydrologic study be conducted to see whether the approach channel can satisfy operational

requirements. Tail Channel 10 The tail channel discharges the flow from the conduit(s) of drainage siphon into nearby river or nalla or even drain. If it fails, excess discharge is likely to erode the downstream portion of the drainage siphon or energy dissipation system, the groin and toe areas of canal emabankment or areas further

downstream of the drainage siphon. Tail channel is subject to the same general problrms with structure and material as Approach channel of the drainage siphon, with additional concerns described below: Erosion: Discharge entering the tail channel is generally at a higher velocity than flows through the approach channel.The tail channel is very susceptible to erosion if not properly sized, aligned and protected from excess velocity. Look for erosion gullies that may indicate improper compaction, overtopping because of downstream obstructions or poor vegetative cover. Inadequate Length: The tail channel should extend far enough downstream to ensure that flows will not damage the embankment groin and toe areas. If damage
98

is occuring, it is extremely important to note the deficiency. Barrels (Conduits)

11. A conduit is a pipe or box structure constructed by joining sections.All outlets, HRs, canal siphons and drainage siphons can generally be termed as conduits. External Inspection Procedures for Conduits: 12. Evidence of potential conduit problems may be found by examining external features of the conduit (if it is exposed) or the embankment. If the material is reaching its life expectancy, it may be possible to dig down to expose all sides of the conduit at a point where the surrounding soil is still damp. Examine the outside of the conduit for signs of deterioration. The condition of the outside of the conduit could be significantly different from the interior. In some cases the soil protects the exterior from oxygen-induced corrosion. On the other hand local site conditions may have accelerated the deterioration of the exterior. Consider the outside of the conduit to be just one indicator. ** Look for signs of infiltration of soil into the conduit: Depression of the embankment along the centerline of the conduit. Sinkholes and piping cavities that exit the surface. Holes taken over by animals may not be easily recognized as sinkholes or piping cavities. Holes that appear to be in a line. These may be an indication that piping or settlement is occurring.

99

Fines in the discharged water.

** Look for seepage or indications that seepage is sometimes present. (This is best done while the conduit is full). Indications of seepage are: Wet spots Increased vegetation or the presence of plants that thrive in wet ground. ** Watch for water flow when there is no flow in the conduit. If any is observed, document from where water is entering the waterway, and examine the water for fines. ** Look for piping related erosion around the conduit near the downstream end. Check the embankment slope above the conduit outfall carefully for voids or erosion that may indicate piping. Check for seepage adjacent to the structure. The situation may be especially serious if the seepage is carrying sediment. ** With exposed conduit, check the support for settlement of movement of the joints. Internal Inspection Procedures for Conduits: 13. To attempting to inspect conduit interiors, you may experience the following difficulties: ** Dewatering difficulties: You cannot inspect a conduit comprehensively unless it has been dewatered. However, dewatering may be impractical or impossible due to structural inadequacy of the conduit to withstand hydrostatic pressure in a dewatering condition. To assess the probable condition of the conduit interior, it may be necessary to rely on results of the exterior inspection.

100

**

Inaccessibility of conduit interior- The conduit may be too small or too dangerous for internal inspection by a person. One possibility is to use remotely operated video equipment. If that is not feasible, the inspection must be based on: - The condition of the exposed portion of the conduit or the embankment above it. The internal inspection of accessible portions of the conduit. (some details can be observed from the downstream end of the conduit with the aid of a strong light and possibly a mirror).

INSPECTION TIP : One indication of settlement related problems that may be be observed from the downstream end of a conduit is the ponding of water in certain reaches of pipe. 14. A deficiency commonly encountered in the internal

inspection of conduit is cracking. Be aware of previously reported cracks and note any new cracks, using a crack map or similar reporting method. Figure -6- shows one page of a crack map prepared by an inspection team. Cracks should be documented as fully as possible, with measurements and/or sketches drawn to scale showing the length and position of each crack. The crack map in figure includes measurements of the depth of weep holes, which were probed during the inspection. 15. To get some indication of whether cracks are continuous through a concrete structure, use a geologists' pick or other hammer to tap the concrete. More comprehensive studies of the concrete using dye tests and sonic methods may be necessary if

101

there are indications that the crack extends any distance into the structure. 16. When inspecting the interior of a conduit, document the following: ** Cavitation damage downstream, at sharp bends, joints or other discontinuities. Corrosion of metal conduit or liner. Cracking: Use crack maps, Describe position, length and orientation (Transverse, longitudinal, or diagonal) Estimate the depth of the crack. Damaged coating or lining materials. (Cracking or buckling is a sign of structural stress Missing chunks can cause cavitation). Debris impact. Deformation of the conduit shape. Efflorescent or gel on the concrete. (Indicates possible chemical deterioration of the concrete). ** ** Erosion, especially in areas of high-velocity flow. Joint separation, compression, or deterioration. Mention any unsound welds, rivets, or flanges. Leakage from the conduit, or seepage entering the conduit. Misalignment of sections of the conduit. Plugged drain holes. Voids behind the conduit near any observed cracks, misalignments or other areas of possible seepage.

** **

**

** ** **

** ** ** **

102

17. Problems with conduits occur most often at joints, and special attention should be given to them during inspection. Open joints can permit erosion of envelope material or cause leakage of water into the embankment during pressure flow. Joints in conduits should be inspected in dry conditions, if possible. Inspection just after a conduit is dewatered may reveal the locations of leaks, because water sometimes spurts through affected joints. 18. Typically, conduit joints pull apart under the highest part of an embankment and are under compression at the end of the waterway. When inspecting conduit joints be sure to: ** ** ** ** Examine joints for leaks Examine the joints between adjacent sections of conduit for leaks and for ruptured water stops. Look for compassion spelling of concrete. Check for misalignment of sections due to differential settlement.

103

Figure shown a conduit joint which has opened along the bottom due to localized settlement along the conduit. Energy Dissipation Section: 19. Use these general guidelines during the your inspection of the energy dissipation section of a drainage siphon: First and foremost, know how the structures are supposed to function. Make close observations of the structures when in use. Note unusual water currents, eddies and swirls, especially return currents that would carry rock and debris into the structure from downstream. Look for Sand boils which result from the upward flow of seepage under pressure and are characterized by a boiling action of the surface seepage. A sand boil is often accompanied by a cone of material around the boil which develops from the deposition of foundation or embankment material varied by the seepage. If possible, dewater the pool to inspect surfaces for damage. To inspect a large pool that cannot be dewatered, plan a boat inspection and record soundings made A plumb bob/ surveying equipment may be needed to determine the location of subsurface damage. Underwater inspections by divers are recommended if problems are suspected. As with any underwater inspection, a detailed inspection, a plan and a good communication system are important considerations for logging damaged areas.

104

Typical Problems With Energy Dissipation Section: 20. Damage can occur to all elements of an energy dissipation section because these structures reduce the velocity and dissipate the energy of a flow. If the energy dissipation structure fails to operate properly the main structure can be eroded at the down stream end, causing a loss of foundation support. 21. Problems typical to the energy dissipation section include the following: Deteriaration of Materials: 22. Follow the actions described in Table--4 Inspection of Energy Dissipation materials to check for deterioration of materials. TABLE 4 INSPECTION OF ENERGY DISSIPATION MATERIALS Concrete Check for signs of cavitation. The sides of chute blocks baffles. And dentates are exposed to considerable turbulence, and any offsets or irregularities can trigger cavitation. Look for erosion damage from abrasion of wasteweir aprons, the top surfaces and undersides of buckets, and the floors, walls chute blocks and dentates of stilling basins. See if ball milling has ground circular patterns in the floor or apron of stilling / hydraulic jump basins.

105

Check joints for spells or settlement on one side. See if joint sealant or compressive joint filler is cracked missing, moved, or deteriorated. Look for broken waterstops. Watch for corroded and damaged reinforcement resulting from erosion and cavitation damage. Concrete terminal structures are always reinforced. Inspect the submerged portions of plunge pools and stilling / hydraulic jump basins while dewatered, if possible or use divers. (An underwater camera or a remotely operated vehicle (ROV) might be used before divers.) Riprap/Pitching Make sure that riprap/pitching is not displaced or lost and that foundation material is protected. Look for piping or voids beneath riprap/pitching. Check riprap or gabion plunge pools and downstream channels for exposed geotextiles, which typically should not be exposed to direct flow or sunlight.

Geotextiles

23. Obstructions: Check energy dissipation sections for the following obstruction: Debris clogging baffles Plunge pools, stilling / hydraulic jump basins, and areas down stream of flip buckets filling with debris (often rocks and other objects thrown by people) Return currents bringing downstream materials into the structure

106

Heavy vegetative growth (such as thick grasses) in plunge pools. If you see material blocking flow note the type of material dimensions and depth, and location relative to a side or an end. A boat can be used to perform a hydrographic survey of a large pool bottom to check for obstructions or damage. 24. Damaged Or Missing Baffles: Baffles may be cracked severely eroded loose or missing. 25. Misalignment Of Walls Or Baffles: deflect the portion of terminal structures. Check for vertically, and sight along the top of a sill for alignment deviation. Check instrumentation data to measure deflections. Offsets may occur as a result of misalignment, and cavitation can developed downstream of such offsets. 26. Malfunctioning Drains: Check for clogged drains in the energy dissipation area. Determine whether water flowing from drains is clear or contains sediment or fine materials. 27. Backfill And Foundation Deficiencies: Check the following points when inspecting the energy dissipation section for backfill and foundation deficiencies: Inspect plunge pools, hydraulic jump basins, and ripraplined dissipators carefully for foundation and crack fill problems. Look for settlement and cracks in backfill. The force of flows may

107

Measure the size and distance of problem areas measure settlement depth and probe for voids and erosion channels. Watch especially for erosion of backfill behind the downstream portion of a stilling / hydraulic jump basins cutoff walls and reinforcement should not be visible. Settlement or improper elevation or length may change the jump location is stilling / hydraulic jump basins. Check that jump within the structure occurs at design locations (If the escape or outlet works is not operating, water stains on the walls will indicate where the jump is actually occurring). Look for misaligned dry walls, cracks in the basin, and cracked backfill for evidence that a jump basis is settling. Check a riprap plunge pool for undermining by loss of underlying soil or lack of filter action. If a plunge pool lining is sand or gravel, check for piping.

108

CHECKLIST FOR EXAMINATION OF DRAINAGE SIPHON _____________________Canal offtaking from ______________________ canal Chainage _______________ to _________________

Date of Examination _________________

Signature Completed _________________________

Operational Status at Time of Examination Canal Water Surface-Elevation Releases: Escape Outlet Works for irrigation Water supply __________ m3/s __________ m3/s __________ m3/s __________ M

Examination Participants Name Affiliation

_____________________________________________________________ _____________________________________________________________ _____________________________________________________________ _____________________________________________________________

APPROACH CHANNEL General condition (Siltation/Debris) Vegetation (trees, willows etc.) Slides above channel (Deep / Shallow) Channel side slope stability ______________________ ______________________ ______________________ ______________________

Slope protection (Adequacy / Degradation / Displacement) ______________________ BARREL Walls Surface condition(Observe Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ____________________ General condition of concrete (Observe Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ 109

Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Cracks or areas of distress(Measure location/extent) ______________________

Condition of backfill (watch for seepage/erosion/settlement) _____________________ Functioning of weep holes(Whether clean/choked) Seepage(Record stains at joints/ turbidity) Debris( If present at at joints/lift joints) Floor Surface condition (Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ______________________ General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) _________________ Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Seepage(Record stains at joints/ turbidity) Amount of flow Location of seeping drains Endsill alignment(Watch for Damage/ distortion) ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

Backfill beyond endsill (Watch for erosion/Reinforcement visibility) _______________

TAIL CHANNEL Slope protection Stability of side slopes Vegetation or other obstructions Any other deficiency OTHER ______________________ ______________________ ______________________ ______________________ (Scour, Retrogression) ______________________ ______________________ ______________________ ______________________

110

Chapter

11

INSPECTION OF OUTLET WORKS (HEAD REGULATOR)

1.

Outlet

works

are

conduits

through

or

around

an

embankment used for releasing water. Regulated outlets use gates or valves for controlling the rate of flow. At unregulated conduits, the rate of flow is controlled by the size of the conduit and the height of the water in the canal above the invert, or floor, of the conduit. Conduits at embankments usually have regulating gates or valves within the upstream portion of the conduit so that flows can be shut off to prevent water from eroding the embankment in the event of failure or leakage through the conduit. Outlet works gates are susceptible to Thus, it is

plugging with debris and sediment deposition.

important that any trash racks in front of the gates be cleaned whenever possible and that the gates be opened periodically to flush debris and sediment. INSPECTION ACTION: Semiannual1y inspect the end of each outlet. Inspect the outlet end of the conduit for breaks in the conduit, erosion of the downstream toe of the embankment or undercutting of the outlet end of the conduit. Operate each gate sufficiently to ensure that it is fully operable and debris and sediment are flushed out. Inspect gate stems to the waterline, and correct any misalignment that interferes with operation. Inspect downstream cistern of the outlets and get removed debris/vegetation.

111

Inspect Annually and also after unusually high discharges, the channel downstream from the outlet works for erosion, obstructions, and undercutting of the outlet structure or the toe of the embankment. Inspect every 3 years, conduits internally. The inspection should be for the purpose of determining the existence of breaks, leaks, cavitations, or other damage. 2. General inspection required as outlined vide Part II shall apply for all the components of Head Regulator/ Outlet. Following gives further details for inspection to be carried out. Checklist for inspection of Head Regulator/ Outlet and Cross regulators is provided at the end of the chapter on Cross regulators. Problems Common To all Types of Intake structure 3. Listed below are some general problems associated with all types of intake structures. Specific issues related to individual intake structure elements are detailed in the paragraphs that follow. Deterioration Of Materials Intake structures that extend above the water surface may be subjected to accelerated deterioration from wetting and drying as the water level rises and falls. If an intake is constructed of coated metal, look for rust holes, especially at the ground line. Crack maps should be used or prepared while inspecting a concrete intake structure. Indications of new or worsened conditions should be noted. There is a sample crack map later in this section. Structural damage to an intake structure Structural damage may be indicated by a flow of water that continues into a conduit even when the water level is below the opening of the intake structure, or when the gate is closed.
112

Misalignment of an intake structure - Misalignment may indicate movement of the abutments or other serious structure problem affecting the integrity of the canal. 4. In the paragraphs that follow, descriptions of the elements of an intake structure are accompanied by specific points to check during your inspection and recommendations to make in your report. Shaped Entrances: 5. Entrance in to or within intake structures are usually rounded or otherwise specially shaped to streamline the flow of water and minimize hydraulic. Even so, localized zones of negative pressure resulting from rapid change in direction or discontinuities can cause vibration and/or cavitation damage. Look for damaged concrete and exposed reinforcing steel. Barrels, Outlet Pipes (Conduits) 6. A conduit is a pipe or box structure constructed by joining sections.All outlets, HRs, canal siphons and drainage siphons can generally be termed as conduits. External Inspection Procedures for Conduits: 7. Evidence of potential conduit problems may be found by examining external features of the conduit (if it is exposed) or the embankment. If the material is reaching its life expectancy, it may be possible to dig down to expose all sides of the conduit at a point where the surrounding soil is still damp. Examine the outside of the conduit for signs of deterioration. The condition of the outside of the conduit could be significantly different from the interior. In some cases the soil protects the exterior from oxygen-induced corrosion.

113

On the other hand local site conditions may have accelerated the deterioration of the exterior. Consider the outside of the conduit to be just one indicator. ** Look for signs of infiltration of soil into the conduit: Depression of the embankment along the centerline of the conduit. Sinkholes and piping cavities that exit the surface. Holes taken over by animals may not be easily recognized as sinkholes or piping cavities. Holes that appear to be in a line. These may be an indication that piping or settlement is occurring. Fines in the discharged water. ** Look for seepage or indications that seepage is sometimes present. (This is best done while the conduit is full). Indications of seepage are: Wet spots Increased vegetation or the presence of plants that thrive in wet ground. ** Watch for water flow when all intakes are closed. If any is observed, double-check to see if intakes are leaking. If not document where water is entering the waterway, and examine the water for fines. ** Look for piping related erosion around the conduit near the downstream end. Check the embankment slope above the conduit outfall carefully for voids or erosion that may indicate piping. Check for seepage adjacent to the structure. The situation may be especially serious if the seepage is carrying sediment. ** With exposed conduit, check the support for settlement of movement of the joints.

114

** Check the concrete anchors of exposed steel conduit for cracking, weathering, and/or chemical deterioration. Internal Inspection Procedures for Conduits: 8. To attempting to inspect conduit interiors, you may experience the following difficulties: ** Dewatering difficulties: You cannot inspect a conduit comprehensively unless it has been dewatered. However, dewatering may be impractical or impossible for one or more of the following reasons. Lack of a bulkhead or other closure device. The need to limit maximum drawdown The need to maintain water flows. Structural inadequacy of the conduit to withstand hydrostatic pressure in a dewatering condition.

To assess the probable condition of the conduit interior, it may be necessary to rely on results of the exterior inspection. ** Inaccessibility of conduit interior- The conduit may betoo small or too dangerous for internal inspection by a person. One possibility is to use remotely operated video equipment. If that is not feasible, the inspection must be based on: - The condition of the exposed portion of the conduit or the embankment above it. The internal inspection of accessible portions of the conduit. (some details can be observed from the downstream end of the conduit with the aid of a strong light and possibly a mirror). INSPECTION TIP : One indication of settlement related problems that may be observed from the downstream end if a conduit is the ponding of water in certain reaches of pipe.
115

9. A deficiency commonly encountered in the internal inspection of conduit is cracking. Be aware of previously reported cracks and note any new cracks, using a crack map or similar reporting method. Figure 6 shows one page of a crack map prepared by an inspection team. Cracks should be documented as fully as possible, with measurements and/or sketches drawn to scale showing the length and position of each crack. The crack map in figure includes measurements of the depth of weep holes, which were probed during the inspection. 10. To get some indication of whether cracks are continuous through a concrete structure, use a geologists' pick or other hammer to tap the concrete. More comprehensive studies of the concrete using dye tests and sonic methods may be necessary if there are indications that the crack extends any distance into the structure. 11. When inspecting the interior of a conduit, document the following: ** Cavitation damage downstream, from gates and valves and at sharp bends, joints or other discontinuities. Corrosion of metal conduit or liner. Cracking: Use crack maps, Describe position, length and orientation (Transverse, longitudinal, or diagonal) Estimate the depth of the crack. Damaged coating or lining materials. (Cracking or buckling is a sign of structural stress Missing ### can cause cavitation). Debris impact.

** **

**

**

116

** **

Deformation of the conduit shape. Efflorescent or gel on the concrete. (Indicates possible chemical deterioration of the concrete). Erosion, especially in areas of high-velocity flow. Joint separation, compression, or deterioration. Mention any unsound welds, rivets, or flanges. Leakage from the conduit, or seepage entering the conduit. Misalignment of sections of the conduit. Plugged drain holes. Voids behind the conduit near any observed cracks, misalignments or other areas of possible seepage.

** **

** ** ** **

12. Problems with conduits occur most often at joints, and special attention should be given to them during inspection. Open joints can permit erosion of envelope material or cause leakage of water into the embankment during pressure flow. Joints in conduits should be inspected in dry conditions, if possible. Inspection just after a conduit is dewatered may reveal the locations of leaks, because water sometimes spurts through affected joints. 13. Typically, conduit joints pull apart under the highest part of an embankment and are under compression at the end of the waterway. When inspecting conduit joints be sure to: ** ** Examine joints for leaks Examine the joints between adjacent sections of conduit for leaks and for ruptured water stops. Look for compassion spelling of concrete.

**

117

**

Check for misalignment of sections due to differential settlement.

Figure shown a conduit joint which has opened along the bottom due to localized settlement along the conduit. Operating Bridge And Pier Problems: 14. Deficiencies in the operating bridge, piers, decks, or other access structures on the Head Regulator could make gates and other controls unworkable in an emergency, and collapse of the supporting structure could obstruct the Head Regulator. 15. Check for the following deficiencies. On concrete bridges, check joints and water runoff points for exposed metal and corrosion of reinforcement steel. Check for peeling or missing paint On steel flashing over joints inspect for break down of welds or mechanical connectors, couplings, and flanges. Look for loose or insecurely anchored guardrails.
118

Check the condition of previously repaired areas. 16. Check bridge support as follows. On concrete bridge supports look for stress cracking. Check the bearing supports at the abutments for condition and evidence of movement. Look for misalignment or damage at sliding joints. Problems With Gates, Stoplogs: 17. When inspecting the control section of a Head Regulator/ Outlet, your primary concern is to ensure that the operation of gates and other canal evacuation equipment is not impaired by adjacent and supporting structures. 18. When inspecting, stoplogs and structures adjacent to and supporting gates check the following points. Look for displacement of structural elements or concrete deterioration that may be jamming or misalignment gates. Have the equipment operated if possible, to detect jamming, or gates not seated properly on the crest. During operations, look for deterioration of material on the underside of the gates. Note excessive leakage. Watch for misalignment of gate stems and other signs of strain from holding water or from debris or over tightening. Inspection of Gates and valves (annual). (1) Visual inspection. When water conditions permit, inspect the downstream surfaces of the guard gate leaves and bodies, the

119

upstream and downstream surfaces of regulating gate leaves and bodies, and outlet pipes. Particular attention should be given to signs of cavitations damage to waterway surfaces downstream from gate or valve leaves and flanged joints. Inspect neoprene or rubber gate seals for deterioration, cracking, wear, foreign material deposits, and leakage. Inspect valve and gates metal seats or seals for wear, scratches, foreign material deposits, and leakage. Repairs should be made as necessary to keep the equipment in a safe and reliable operating condition. (2) Exercising After lubrication, operate each valve and gate through a full cycle while under actual operating conditions, if possible. During operation, listen for unusual noises and check for binding or vibration. Inspection of Hydraulic and manual operators and control systems for gates and valves (annual) (1) Visual inspection Check hydraulic oil in the tank for proper fluid level (take into account displacement of the gate stem), water, and foreign materia1. Check all pipe joints, cylinder flanges, packing, and hydraulic equipment for leaks. Check oil filters and strainers and change or clean if required. Check hydraulic hoist piston stem for rusting and foreign deposits. Remove deposits and rough areas on stems to prevent damage to packing or seals.

120

(2)Exercising Operate hydraulic control and manual operator systems and check for unusual noises or vibrations. Check motors and hydraulic fluids for overheating, and check pressure switches, pressure gages, and limit switches for proper operation according to operating instructions. Clean manual operators of dirt and foreign material and lubricate as appropriate. 20. Physical security - The physical security should be inspected for adequacy and repairs and improvements made, as necessary, to avoid unauthorized operation and ensure the safety of the equipment. Inspection of Traveling crane, hoist, and tracks (annual) (3) a. Visual inspection Examine hoist, crane, and tracks for broken, bent, misaligned, worn, or loose parts and corrosion and deterioration of protective coatings.

(2)Exercising b. After lubrication, operate crane and hoist throughout all functions and check for unusual noises, binding, and vibration during operation.

121

Chapter 12 INSPECTION OF CROSS REGULATOR

1. General inspection required as outlined vide Part II shall apply for all the components of cross regulator. Following gives further details for inspection to be carried out. Checklist for inspection of cross regulator is provided at the end of this chapter.

Operating Bridge And Pier Problems: 2. Deficiencies in the operating bridge, piers, decks, or other access structures on the cross regulator could make gates and other controls unworkable in an emergency, and collapse of the supporting structure could obstruct the canal. 3. Check for the following deficiencies. On concrete bridges, check joints and water runoff points for exposed metal and corrosion of reinforcement steel. Check for peeling or missing paint On steel flashing over joints inspect for break down of welds or mechanical connectors, couplings, and flanges. Look for loose or insecurely anchored guardrails. Check the condition of previously repaired areas.

4.Check bridge support as follows. On concrete bridge supports look for stress cracking.

122

Check the bearing supports at the abutments for condition and evidence of movement. Look for misalignment or damage at sliding joints. Problems With Gates, Stoplogs: 5.When inspecting the control section of an cross regulator, your primary concern is to ensure that the operation of gates is not impaired by adjacent and supporting structures. 6. When inspecting, stoplogs and structures adjacent to and supporting gates check the following points. Look for displacement of structural elements or concrete deterioration that may be jamming or misalignment gates. Have the equipment operated if possible, to detect jamming, or gates not seated properly on the crest. During operations, look for deterioration of material on the underside of the gates. Note excessive leakage. Watch for misalignment of gate stems and other signs of strain from holding water or from debris or over tightening. Inspection of Gates and valves (annual). (1)Visual inspection. a When water conditions permit, inspect the downstream surfaces of the guard gate leaves and bodies, the upstream and downstream surfaces of regulating gate leaves and bodies, and outlet pipes Particular attention should be given to signs of cavitations damage to waterway surfaces downstream from gate or valve leaves and flanged joints.

123

c.

Inspect neoprene or rubber gate seals for deterioration, cracking, wear, foreign material deposits, and leakage. Inspect valve and gates metal seats or seals for wear, scratches, foreign material deposits, and leakage. Repairs should be made as necessary to keep the equipment in a safe and reliable operating condition.

d.

e.

(2) Exercising After lubrication, operate each valve and gate through a full cycle while under actual operating conditions, if possible. During operation, listen for unusual noises and check for binding or vibration. Inspection of Hydraulic and manual operators and control systems for gates and valves (annual) (1) Visual inspection Check hydraulic oil in the tank for proper fluid level (take into account displacement of the gate stem), water, and foreign materia1. Check all pipe joints, cylinder flanges, packing, and hydraulic equipment for leaks. Check oil filters and strainers and change or clean if required. Check hydraulic hoist piston stem for rusting and foreign deposits. Remove deposits and rough areas on stems to prevent damage to packing or seals. (2)Exercising Operate hydraulic control and manual operator systems and check for unusual noises or vibrations.

124

Check motors and hydraulic fluids for overheating, and check pressure switches, pressure gages, and limit switches for proper operation according to operating instructions. Clean manual operators of dirt and foreign material and lubricate as appropriate. 7. Physical security - The physical security should be inspected for adequacy and repairs and improvements made, as necessary, to avoid unauthorized operation and ensure the safety of the equipment.

Inspection of Traveling crane, hoist, and tracks (annual) (1) a. Visual inspection Examine hoist, crane, and tracks for broken, bent, misaligned, worn, or loose parts and corrosion and deterioration of protective coatings.

(2)Exercising b. After lubrication, operate crane and hoist throughout all functions and check for unusual noises, binding, and vibration during operation.

125

CHECKLIST FOR EXAMINATION OF OUTLET WORKS (H.R. & C.R.) _____________________Canal offtaking from ______________________ canal Chainage _______________ to _________________

Date of Examination _________________

Signature Completed _________________________

Operational Status at Time of Examination Canal Water Surface-Elevation Releases: Escape Outlet Works for irrigation Water supply __________ m3/s __________ m3/s __________ m3/s __________ M

Examination Participants Name Affiliation

_____________________________________________________________ _____________________________________________________________ _____________________________________________________________ _____________________________________________________________

Trashracks Trashracks concrete structure SERVICE CONTROL FACILITY GATES Description

______________________ ______________________

______________________

General Condition(watch for corrosion/fatigue/rupture/cavitations of metal &position of welds) ______________________ Protective coating Leakage (In closed condition at seal/through concrete) Condition of rubber seals ______________________ ______________________ ______________________

126

Alignment of gate stem Exercising frequency

______________________ ______________________

Operation during inspection (Raise & lower fully if loss of water is not a problem) ___________________ CONTROLS FOR GATES Mechanical Hoists(watch for wear of brakeshoe lining / key-bolts are tightened/ handcranks in locked position ) Wire ropes( watch for rusting/ breakage/reduction in diameter/ condition of socket--clamps) Protective coatings(watch if peeling/missing) ______________________ ______________________ ______________________

Condition of hoist platform (Watch for rusting/ loss of weld/bending/ misalignment/movement) Guard rails(Watch for damage/ loss of sleeves/coupling /check anchors) Change of oil (Gear box) Condition of Gear teeth (Check for damage/wear/cracks) Lubrication ( Of ropes/bearing points/Pinions/Hinges/ Spin gear/Chains) Electrical Power supply Standby power Operation instructions STOPLOGS General condition Protective coating (watch if peeling/missing) Seals Valve(s) (IF PROVIDED) General condition Protective coatings Cavitations Leakage (closed) Creep ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

127

Exercising frequency Operation of valves at time of examination Control system for valves Mechanical Electrical Operating instructions GATE CIVIL WORKS (including Access Bridge) Walls

______________________ ______________________

______________________ ______________________ ______________________

Surface condition(Observe Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ____________________ General condition of concrete (Observe Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Cracks or areas of distress(Measure location/extent) ______________________

Condition of backfill (watch for seepage/erosion/settlement) _____________________ Functioning of weep holes(Whether clean/choked) Seepage(Record stains at joints/ turbidity) Debris( If present at at joints/lift joints) Floor Surface condition (Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ______________________ ______________________ ______________________ ______________________

General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) _________________ Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Seepage(Record stains at joints/ turbidity) Amount of flow Location of seeping drains Endsill alignment(Watch for Damage/ distortion) ______________________ ______________________ ______________________ ______________________

Backfill beyond endsill (Watch for erosion/Reinforcement visibility) _______________

128

Chapter 13

.INSPECTION OF FALL

1. General inspection required as outlined vide Part II shall apply for all the components of canal fall. Following gives further details for inspection to be carried out. Checklist for inspection of canal fall is provided at the end of this chapter.

CONTROL SECTION: 2. The control section is a particularly critical portion of a canal fall as it receives flow of water from upstream and passes on further downstream via energy dissipation system. It may be in the form of a weir with crest (or sill level) raised above canal bed level. 3. Problems typical to the canal fall control section include: Deterioration of surface materials:Check the following points for deterioration in the control section: Look at surfaces in areas of concentrated and high velocity flows, such as near gates,(in case of fall cum Cross regulator) for erosion. Check areas near large gates for cracking in concrete, and tearing, rupture, and fatigue in metal. Examine the upstream edges of weirs for damage from battering by debris. INSPECTION TIP : High velocity flow over a concrete surface containing abnormalities can initiate cavitation damage. Check surfaces carefully for offsets, small holes and calcium carbonate deposits. The bearing surfaces

129

where gates rest and areas immediately downstream of gate slots, liner plates should be examined with special care. Obstructions: Besides general types of obstructions already discussed, check for the following obstructions to control sections: Check for unauthorized equipment added to the control section. Operating Bridge And Pier Problems:Deficiencies in the operating bridge, piers, decks, or other access structures on the escape could make gates and other controls unworkable and collapse of the supporting structure could obstruct the canal. Check for the following deficiencies. On concrete bridges, check joints and water runoff points for exposed metal and corrosion of reinforcement steel. Check for peeling or missing paint On steel flashing over joints inspect for break down of welds or mechanical connectors, couplings, and flanges. Look for loose or insecurely anchored guardrails. Check the condition of previously repaired areas. Check bridge support as follows. On concrete bridge supports look for stress cracking. Check the bearing supports at the abutments for condition and evidence of movement. Look for misalignment or damage at sliding joints. Problems With Gates, Stoplogs: When inspecting the control section of a fall cum Cross regulator, your primary concern is to ensure that the
130

operation of gates is not impaired by adjacent and supporting structures. When inspecting, stoplogs and structures adjacent to and supporting gates check the following points. Look for displacement of structural elements or concrete deterioration that may be jamming or misalignment gates. Have the equipment operated if possible, to detect jamming, or gates not seated properly on the crest. During operations, look for deterioration of material on the underside of the gates. Note excessive leakage. Watch for misalignment of gate stems and other signs of strain from holding water or from debris or over tightening. Backfill and Foundation Deficiencies: Points to remember when inspecting the control section for backfill and foundation deficiencies are: Foundation in the control section often must bear the stress of heavy equipment. Check carefully for displacements that may indicate settling foundation shifts, or undermining. Check for voids under concrete channel walls and floors. It is critical that gaps in joints do not expose foundation or backfill material where escape extends through the embankment section, and that water stops, sealants and compressive joint fillers are intact and in good condition. Check for clogged weep holes and foundation drains if present and watch for seepage and other signs of problems with the drainage system.

131

Energy Dissipation Section: 4. Use these general guidelines during the your inspection of the energy dissipation section of a canal fall: First and foremost, know how the structures are supposed to function. Make close observations of the structures when in use. Note unusual water currents, eddies and swirls, especially return currents that would carry rock and debris into the structure from downstream. Look for Sand boils which result from the upward flow of seepage under pressure and are characterized by a boiling action of the surface seepage. A sand boil is often accompanied by a cone of material around the boil which develops from the deposition of foundation or embankment material varied by the seepage. If possible, dewater the pool to inspect surfaces for damage. To inspect a large pool that cannot be dewatered, plan a boat inspection and record soundings made A plumb bob/ surveying equipment may be needed to determine the location of subsurface damage. Underwater inspections by divers are recommended if problems are suspected. As with any underwater inspection, a detailed inspection, a plan and a good communication system are important considerations for logging damaged areas. Typical Problems With Energy Dissipation Section: 5. Damage can occur to all elements of an energy dissipation section because these structures reduce the velocity and dissipate the energy of a flow. If the energy dissipation structure

132

fails to operate properly the main structure can be eroded at the down stream end, causing a loss of foundation support. 6. Problems typical to the energy dissipation section include the following: Deteriaration of Materials: 7. Follow the actions described in Table--5- Inspection of Energy Dissipation materials to check for deterioration of materials. TABLE 5 INSPECTION OF ENERGY DISSIPATION MATERIALS Concrete Check for signs of cavitation. The sides of chute blocks baffles. And dentates are exposed to considerable turbulence, and any offsets or irregularities can trigger cavitation. Look for erosion damage from abrasion of wasteweir aprons, the top surfaces and undersides of buckets, and the floors, walls chute blocks and dentates of stilling basins. See if ball milling has ground circular patterns in the floor or apron of stilling / hydraulic jump basins. Check joints for spells or settlement on one side. See if joint sealant or compressive joint filler is cracked missing, moved, or deteriorated. Look for broken waterstops. Watch for corroded and damaged reinforcement resulting from erosion and cavitation damage. Concrete

133

terminal structures reinforced.

are

always

Inspect the submerged portions of plunge pools and stilling / hydraulic jump basins while dewatered, if possible or use divers. (An underwater camera or a remotely operated vehicle (ROV) might be used before divers.) Riprap/Pitching Make sure that riprap/pitching is not displaced or lost and that foundation material is protected. Look for piping or voids beneath riprap/pitching. Check riprap or gabion plunge pools and downstream channels for exposed geotextiles, which typically should not be exposed to direct flow or sunlight.

Geotextiles

8. Obstructions: Check energy dissipation sections for the following obstruction: Debris clogging baffles Plunge pools, stilling / hydraulic jump basins, and areas down stream of flip buckets filling with debris (often rocks and other objects thrown by people) Return currents bringing downstream materials into the structure Heavy vegetative growth (such as thick grasses) in plunge pools. If you see material blocking flow note the type of material dimensions and depth, and location relative to a side or an end. A boat can be used to perform a hydrographic survey of a large pool bottom to check for obstructions or damage.
134

9. Damaged Or Missing Baffles: Baffles may be cracked severely eroded loose or missing. 10. Misalignment Of Walls Or Baffles: deflect the portion of terminal structures. Check for vertically, and sight along the top of a sill for alignment deviation. Check instrumentation data to measure deflections. Offsets may occur as a result of misalignment, and cavitation can developed downstream of such offsets. 11. Malfunctioning Drains: Check for clogged drains in the energy dissipation area. Determine whether water flowing from drains is clear or contains sediment or fine materials. 12. Backfill And Foundation Deficiencies: Check the following points when inspecting the energy dissipation section for backfill and foundation deficiencies: Inspect plunge pools, hydraulic jump basins, and ripraplined dissipators carefully for foundation and crack fill problems. Look for settlement and cracks in backfill. Measure the size and distance of problem areas measure settlement depth and probe for voids and erosion channels. Watch especially for erosion of backfill behind the downstream portion of a stilling / hydraulic jump basins cutoff walls and reinforcement should not be visible. Settlement or improper elevation or length may change the jump location is stilling / hydraulic jump basins. Check that jump within the structure occurs at design locations (If the escape or outlet works is not operating, water stains
135

The force of flows may

on the walls will indicate where the jump is actually occurring). Look for misaligned dry walls, cracks in the basin, and cracked backfill for evidence that a jump basis is settling. Check a riprap plunge pool for undermining by loss of underlying soil or lack of filter action. If a plunge pool lining is sand or gravel, check for piping.

136

CHECKLIST FOR EXAMINATION OF CANAL FALL STRUCTURE _____________________Canal offtaking from ______________________ canal Chainage _______________ to _________________

Date of Examination _________________

Signature Completed _________________________

Operational Status at Time of Examination Canal Water Surface-Elevation Releases: Escape Outlet Works for irrigation Water supply __________ m3/s __________ m3/s __________ m3/s __________ M

Examination Participants Name Affiliation

_____________________________________________________________ _____________________________________________________________ _____________________________________________________________ _____________________________________________________________

GLACIS OF WASTE WEIR/SPILLWAY Debris Crest Surface condition(Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ________________ General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) __________________ Cracks or areas of distress Sign of movement Training Walls Surface condition(Observe Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ___________________ 137 ______________________ ______________________ ______________________

General condition of concrete (Observe Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) _______________ Signs of Movement (offsets/Misalignment/Differential movement) ________________ Joints(If washed out /crack/differential movement /vegetation growth) _____________ Cracks or areas of distress(Measure location/extent) ______________________

Condition of backfill (watch for seepage/erosion/settlement) _____________________ Functioning of weep holes(Whether clean/choked) Seepage(Record stains at joints/ turbidity) Debris( If present at at joints/lift joints) Floor/apron/cistern Surface condition (Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ______________________ General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Seepage(Record stains at joints/ turbidity) Amount of flow Location of seeping drains Endsill alignment(Watch for Damage/ distortion) ______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

Backfill beyond endsill (Watch for erosion/Reinforcement visibility) _______________

138

Chapter 14

INSPECTION OF AQEDUCTS

1. General inspection required as outlined vide Part II shall apply for all the components of canal aqueduct. Following gives further details for inspection to be carried out. Checklist for inspection of canal aqueduct is provided at the end of this chapter.

2. Operating Bridge And Pier Problems:Deficiencies in the operating bridge, piers, decks, or other access structures on the escape could make gates and other controls unworkable and collapse of the supporting structure could obstruct the canal. Check for the following deficiencies. On concrete bridges, check joints and water runoff points for exposed metal and corrosion of reinforcement steel. Check for peeling or missing paint On steel flashing over joints inspect for break down of welds or mechanical connectors, couplings, and flanges. Look for loose or insecurely anchored guardrails. Check the condition of previously repaired areas. Check bridge support as follows. On concrete bridge supports look for stress cracking. Check the bearing supports at the abutments for condition and evidence of movement. Look for misalignment or damage at sliding joints.

139

Problems With Gates, Stoplogs: 3. When inspecting the control section of a fall cum Cross regulator, your primary concern is to ensure that the operation of gates is not impaired by adjacent and supporting structures. 4. When inspecting, stoplogs and structures supporting gates check the following points. Look for displacement of structural elements or concrete deterioration that may be jamming or misalignment gates. Have the equipment operated if possible, to detect jamming, or gates not seated properly on the crest. During operations, look for deterioration of material on the underside of the gates. Note excessive leakage. Watch for misalignment of gate stems and other signs of strain from holding water or from debris or over tightening. Backfill and Foundation Deficiencies: 5. Points to remember when inspecting the control section for backfill and foundation deficiencies are: Foundation in the control section often must bear the stress of heavy equipment. Check carefully for displacements that may indicate settling foundation shifts, or undermining. Check for voids under concrete channel walls and floors. It is critical that gaps in joints do not expose foundation or backfill material where escape extends through the embankment section, and that water stops, sealants and compressive joint fillers are intact and in good condition. adjacent to and

140

Check for clogged weep holes and foundation drains if present and watch for seepage and other signs of problems with the drainage system. Inspection of Aqueduct Barrels:

External Inspection Procedures: 6. Evidence of potential problems may be found by examining external features of the barrels. Examine the outside of the barrel for signs of deterioration. The condition of the outside of the barrel could be significantly different from the interior e.g. local site conditions might have accelerated the deterioration of the exterior. Consider the outside of the conduit to be just one indicator. ** Look for seepage or indications that seepage is sometimes present. (This is best done while the barrel is full). Indications of seepage are: Wet spots Increased vegetation or the presence of plants that thrive in wet ground. ** Watch for water flow when all intakes are closed. If any is observed, double-check to see if intakes are leaking. If not document where water is entering the barrel, and examine the water for fines. ** Check for seepage adjacent to the structure. The situation may be especially serious if the seepage is carrying sediment. ** With exposed conduit, check the support for settlement of movement of the joints. ** Check the concrete anchors of exposed steel conduit for cracking, weathering, and/or chemical deterioration.

141

Internal Inspection Procedures: 7. To attempting to inspect barrel interiors, you may experience the following difficulties: ** Dewatering difficulties: You cannot inspect a barrel comprehensively unless it has been dewatered. However, dewatering may be impractical or impossible for one or more of the following reasons. The need to limit maximum drawdown The need to maintain water flows. Structural inadequacy of the barrel to withstand hydrostatic pressure in a dewatering condition.

To assess the probable condition of the barrel interior, it may be necessary to rely on results of the exterior inspection. ** Inaccessibility of conduit interior- The conduit may be too dangerous for internal inspection by a person. One possibility is to use remotely operated video equipment. If that is not feasible, the inspection must be based on: - The condition of the exposed portion of the barrel The internal inspection of accessible portions of the barrel. (some details can be observed from the downstream end of the barrel with the aid of a strong light and possibly a mirror).

INSPECTION TIP : One indication of settlement related problems that may be observed from the downstream end if a conduit is the ponding of water in certain reaches of barrel. 8. A deficiency commonly encountered in the internal inspection of barrel is cracking. Be aware of previously reported cracks and

142

note any new cracks, using a crack map or similar reporting method. Figure -6 shows one page of a crack map prepared by an inspection team. Cracks should be documented as fully as possible, with measurements and/or sketches drawn to scale showing the length and position of each crack. The crack map in figure includes measurements of the depth of weep holes, which were probed during the inspection. 9. To get some indication of whether cracks are continuous through a concrete structure, use a geologists' pick or other hammer to tap the concrete. More comprehensive studies of the concrete using dye tests and sonic methods may be necessary if there are indications that the crack extends any distance into the structure. 10 When inspecting the interior of a barrel, document the following: ** Cavitation damage discontinuities. downstream, at joints or other

** **

Corrosion of metal conduit or liner. Cracking: Use crack maps, Describe position, length and orientation (Transverse, longitudinal, or diagonal) Estimate the depth of the crack. Debris impact. Deformation of the barrel shape. Efflorescent or gel on the concrete. (Indicates possible chemical deterioration of the concrete). Erosion, especially in areas of high-velocity flow.

** ** **

**

143

**

Joint separation, compression, or deterioration. Mention any unsound welds, rivets, or flanges. Leakage from the barrel, Misalignment of sections of the barrel.

** **

11. Problems with barrel occur most often at joints, and special attention should be given to them during inspection. Open joints can permit erosion of envelope material or cause leakage of water into the embankment during pressure flow. Joints in barrel should be inspected in dry conditions, if possible. Inspection just after a barrel is dewatered may reveal the locations of leaks, because water sometimes spurts through affected joints. 12. Typically, barrel joints pull apart under the highest part of an embankment and are under compression at the end of the waterway. When inspecting barrel joints be sure to: ** ** Examine joints for leaks Examine the joints between adjacent sections of barrel for leaks and for ruptured waterstops. Look for compression spalling of concrete. Check for misalignment of sections due to differential

** **

144

settlement. Figure shows a barrel joint which has opened along the bottom due to localized settlement along the barrel.

145

CHECKLIST FOR EXAMINATION OF AQUEDUCT _____________________Canal offtaking from ______________________ canal Chainage _______________ to _________________

Date of Examination _________________

Signature Completed _________________________

Operational Status at Time of Examination Canal Water Surface-Elevation Releases: Escape Outlet Works for irrigation Water supply __________ m3/s __________ m3/s __________ m3/s __________ M

Examination Participants Name Affiliation

_____________________________________________________________ _____________________________________________________________ _____________________________________________________________ _____________________________________________________________

BRIDGE General condition Vegetation at abutments and piers Bridge supports Foundations Substructures-piers Bridge bearings Moving parts

______________________ ______________________ ______________________

______________________ ______________________ ______________________ ______________________

146

Accumulation of birds, nests etc. Visual examination of scour protection Protective coatings Main supporting members Deteriorated and/or damaged members(SLABS/BEAMS) Protective coatings Bridge deck General condition Surface of roadway slab Drainage Water spouts Expansion joints Guardrails/Parapats Signage BARREL Walls

______________________ ______________________ ______________________

______________________ ______________________

______________________ ______________________ ______________________ ______________________ ______________________ ______________________ ______________________

Surface condition(Observe Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ____________________ General condition of concrete (Observe Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) _______________ Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Cracks or areas of distress(Measure location/extent) ______________________

Condition of backfill (watch for seepage/erosion/settlement) _____________________ Functioning of weep holes(Whether clean/choked) Seepage(Record stains at joints/ turbidity) Debris( If present at at joints/lift joints) Floor Surface condition (Cracks / Honey comb / stratification / Form slippage / Stains / Bar Projection) ______________________ General condition of concrete(Disintegration / Spalling / Drummy Concrete / Pop out / Pitting / Sealing) ________________ ______________________ ______________________ ______________________

147

Signs of Movement (offsets/Misalignment/Differential movement) _________________ Joints(If washed out /crack/differential movement /vegetation growth) ______________ Seepage(Record stains at joints/ turbidity) Amount of flow Location of seeping drains Endsill alignment(Watch for Damage/ distortion) ______________________ ______________________ ______________________ ______________________

Backfill beyond endsill (Watch for erosion/Reinforcement visibility) _______________

148

PART IV

SCHEDULE OF ROUTINE INSPECTION

149

Chapter 15

SCHEDULE OF ROUTINE INSPECTION

1. Operation of the dam/canal during normal conditions shall be the responsibility of the section officer in charge of the canal. It shall be ensured that unauthorized encroachments do not occur, that existing or potential conditions do not lead to public criticism or injury to the public and that nothing is done which conflicts with the primary purpose of the project. Following gives schedule of duties to be performed by the Section officer: Daily 1. Record water surface elevation in reservoir/canal 2. Record discharge released into various canals/ direct outlets offtaking from the canal within his jurisdiction 3. Record releases from escapes/wasteweirs/spillways 4. Check security and safety devices 5. Make required changes in gate openings 6. Record pertinent information in Operating Log 7. Check escape tail channel for debris Monthly 1. Check condition of : Downstream cisterns 2. Run generators for minimum one hour 3. Keep batteries charged 4. Replace light bulbs if required 5.Check signs that warn public of hazards near falls, escapes, Head regulators and siphons 6. Check fence conditions and caution signs Quarterly 1. 2. 3. 4. Operating instructions--uptodate & legible Clean gate control switchboxes Check & clear bridge drains Clean inside of motor control cabinet
150

Semiannually 1. Inspect approach and tail channels of structures for trees, vegetation, shrubs, bush growth and remove deep rooted vegetation and shrubs. 2. Inspect for erosion in and around structures 3. Inspect and record quality and clarity of seepage and corresponding water level in canal. 4. Lubricate gate rollers 5. Lubricate hoist cables 6. Replace grease in gear case of hoist 7. Change oil in generator 8. Check hydraulic oil lines 9. Check oil reservoir level in hydraulic gate system 10. Check rubber seals and seal clamps 11. Check paint on gates 12. Check mechanical hoist bearings and flexible coupling bearings 13. Spur gear units and gear motors Annually 1. 2. 3. 4. 5. Check and repaint metal works of bridge, gates, fence Review Standing Operating Procedure Exercise gates and valves Check condition of exterior and interior of siphon barrels Examine approach and tail channels of siphons, tail channels of escapes, apron, downstream cistern of escapes, falls & outlets 6. Check electrical pull boxes, conduits & switches 7. Inspect ends of drainage pipes at or near upstream toe of embankment and clean out debris / material that might choke that drain. After Heavy Rains 1.Inpect and repair escapes/spillways and drainage structures Every three years 1.Inspect and repair conduits/ barrels having more than 60 cm diameter
151

2. Following officers shall carry out inspection as per the frequency shown against their designation: Designation Of inspecting officer Deputy Executive Engineer Executive Engineer Superintending Engineer Chief Engineer Inspection to be carried out during month of March, October April October MidMay MidNovember May lastfortnight November last fortnight Note

Vulnerable area At Random

152

PART V

INSPECTION DURING EMERGENCY

153

Chapter 16

INSPECTION DURING EMERGENCY

Detailed guidelines are under preparation for inspection and operation during emergency situations. These form part of Standing Operating Procedures of each of the dams.

154