Neat network polyurethane SMP samples were fabricated based on a variation
of a composition specified by Wilson et al.45 in 2007, using stoichiometric ratios
of polyol and diisocyanate monomers. Triethanolamine was added in a 2.0% excess (by mass). N,N,N,N-Tetrakis(2-hydroxypropyl)ethylenediamine (HPED, 98%) (TCI America, Portland, OR), triethanolamine (TEA 99.5%) (SigmaAldrich Co., St. Louis, MO) and hexamethylene diisocyanate (HDI, 98%) (TCI America, Portland, OR) were decanted in a precise basic controlled atmosphere glove box (LabConco Corporation, Kansas City, Missouri) under a dry air atmosphere into glass jars and were subsequently sealed.