Professional Documents
Culture Documents
Product Data
_______________________________________________________________________________
Form Comp. A: Epoxy Resin
Comp. B: Epoxy Hardener
Comp. C: Grey Powder
Mixed: Grey Paste
_______________________________________________________________________________
Packaging 16 Kg set (A+B+C)
_______________________________________________________________________________
Storage Condition Store in a dry area between 5°C and 35°C. Protect from sunlight.
_______________________________________________________________________________
Epocem Ferrogard 110
_______________________________________________________________________________
Shelf life 12 months minimum from production date if stored properly in
original unopened packaging in a cool, shaded area.
_______________________________________________________________________________
Technical Data
_______________________________________________________________________________
Mixing ratio Slurry: A:B:C = 1:5:10 by weight
_______________________________________________________________________________
Pot life 60 minutes (at 25°C), 30 minutes (at 40°C)
_______________________________________________________________________________
Density Fresh mixture: Approximately 2.00 Kg/Lit
_______________________________________________________________________________
Consumption Anticorrosive Caoting:
2.0 ~ 3.0 kg / m2 per two coats. Minimum of two coats are
recommended.
Bonding Agent:
Average 1.0 kg / m2 depending upon the surface roughness.
_______________________________________________________________________________
Open Time 2 hours (30°C), 4 hours (20°C), 6 hours (10°C),
8 hours (5°C)
_______________________________________________________________________________
Temperature Minimum 5°C; Maximum 40°C (substrate)
(Application)
_______________________________________________________________________________
Application Details
_______________________________________________________________________________
Mixing Stir component A and B thoroughly before pouring into a clean
mixing container. Add component C (powder) slowly while
mixing continuously. Use low speed electric mixers (max.500
rpm) for 3 minutes avoiding entrapment of air. By adding the
powder in portions, the desired application consistency can be
obtained.
_______________________________________________________________________________
Application After mixing the Epocem Ferrogard 110 thoroughly in the
specified proportion, apply the wet mixture on the cleaned
surface by brush or roller. For effective protection against
corrosion, apply the product in at least two coats.
Do not use Less than 1Kg/m² as a bonding agent
_______________________________________________________________________________
Epocem Ferrogard 110
_______________________________________________________________________________
Curing Allow the applied product to cure in air.
_______________________________________________________________________________
Cleaning Application and mixing tools should be cleaned with water while
material is still fresh. Hardened material can only be removed
mechanically.
_______________________________________________________________________________
Safety
_______________________________________________________________________________
Precautions 1.Accidental splashes to the skin must be washed off with
water and soap.
2. Accidental splashes to the eyes must be rinsed with clean
water. Seek medical attention without delay.
_______________________________________________________________________________
Toxicity Non-toxic.
_______________________________________________________________________________
Transportation Non-hazardous
_______________________________________________________________________________