MPI ACCEPTANCE CRITERIA - AWS D1.1 – Table 6.

Visual Inspection criteria is applicable for MPI as per AWS D1.1 Table 6.1.

1) Cracks

Cracks are not acceptable.

2)Fusion between Base Metal & Weld metal

Complete fusion shall exist between Weld metal & Base Metal

3)Craters

Craters(Welding termination points) shall be filled

4)Fillet Size variation

Variations are acceptable as per below table

5)Undercut

For Thickness Less than 25 mm,Undercut Shall not exceed 1 mm.

6)Porosity

The sum of the visible porosity(Dia 1mm or greater) shall not exceed 20mm in any 300 mm length of
weld.

Note-For Detailed Information refer the Below given Table 6.1