Master Data Sheet
Job order No.:- Date:-
Sample Description:-TMT Steel
S. Test Test Method Test Result Requirement
No. IS 1786:2008
Grade Fe-500D
(A) Chemical Test
1. Carbon, % IS 228(P-I):1987 0.25 Max.
2. Sulphur, % IS 228:(P- 0.040 Max.
IX):1989
3. Phosphorus, % IS 228(P-III):1987 0.040Max.
4. Sulphur + Phosphorus, % IS 1786:2008 0.075 Max.
(B) Physical Test
1. Yield Stress, N/mm2 IS 1608(Pt-1):2018 500 Min.
2. Tensile Strength, N/mm2 IS 1608(Pt-1):2018 Not Less than 565
3. TS/YS Ratio IS 1608(Pt-1):2018 1.10 Min.
4. Elongation, % IS 1608(Pt-1):2018 16.0 Min.
(On gauge length 5.65√ A, where
A= Cross Sectional Area)
5. Total Elongation at Maximum IS 1608(Pt-1):2018 5.0 Min.
Force
6. Bend Test IS 1599:2012 There is no rupture
or cracks visible on
the bent portion.
7. Rebend Test IS 1786:2008 There is no rupture
or cracks visible on
the rebent portion.
8. Nominal Mass, Kg/mtr. IS 1786:2008 3.85±3%
Remarks:
**End of Report**
Analyst Lab In-Charge