You are on page 1of 2

3/6/2014 C20E2C / 1.

1152 - steel equivalent, mechanical properties, chemical composition

EURO PEAN ST EEL AND ALLO Y


G RADES
st eelnumber . com

Steel Steel and cast iron Alloy Equivalent Russian


Home Search About us
numbers standards standards grades steels

YOU HERE: Steel numbers -> Number 1.11XX OR Steel and cast iron standards -> / EN 10263-3

C20E2C ( 1.1152 )

Grade : C20E2C

Number: 1.1152

EN 10263 - 3 : 2001 Steel rod, bars and wire for cold heading and cold extrusion. Technical delivery
Standard:
conditions for case hardening steels

Classification: Non-alloy special steel

Equivalent grades: Go here

Che m ic a l c om pos it ion % of gr a de C2 0 E2 C ( 1 .1 1 5 2 )


C Si Mn P S Cu

0.18 - 0.22 max 0.3 0.3 - 0.6 max 0.025 max 0.025 max 0.25

M e c ha nic a l pr ope r t ie s of gr a de C2 0 E2 C ( 1 .1 1 5 2 )

Rm - Tensile strength (MPa) 450-640

Z - Reduction in cross section on fracture (%) 56-67

Equiva le nt gr a de s of gr a de C2 0 E2 C ( 1 .1 1 5 2 )
Warning! Only for reference
Russia
GOST
20
20kp

M e c ha nic a l pr ope r t ie s
M e c ha nis c he Eige ns c ha f t e n
Ca r a c t e r is t ique s m e c a nique s
R eH Minimum yield strength / Mindestwert der oberen Streckgrenze / Limite d�elasticite minimale
R m Tensile strength / Zugfestigkeit / Resistance a la traction
A Minimum elongation / Mindestwert der Bruchdehnung / Allongement minimal
J Notch impact test / Kerbschlagbiegeversuch / Essai de flexion par choc

He a t t r e a t m e nt c ondit ions
+A Soft annealed
+AC Annealed to achieve spheroidization of the carbides

http://www.steelnumber.com/en/steel_composition_eu.php?name_id=746 1/2
3/6/2014 C20E2C / 1.1152 - steel equivalent, mechanical properties, chemical composition
+AR As rolled
+AT Solution annealed
+C Cold drawn / hard
+CR Cold rolled
+FP Treated to ferrite-pearlite structure and hardness range
+I Isothermal annealing
+LC Cold drawn / soft
+M Thermo mechanical rolling
+N Normalized
+NT Normalized and tempered
+P Precipitation hardened
+PE Peeled
+QA Air quenched and tempered
+QL Liquid quenched and tempered
+QT Quenched and tempered
+S Treated to improve shearability
+SH As rolled and turned
+SR Cold drawn and stress relieved
+T Tempered
+TH Treated to hardness range
+WW Warm worked
+U Untreated

Chemical composition of C20E2C (1.1152). Equivalent grades of C20E2C (1.1152). Standards of C20E2C (1.1152).
Properties of C20E2C (1.1152). Hardness of C20E2C (1.1152). Strength of C20E2C (1.1152). Elongation of C20E2C (1.1152).

© 2011- 2014 All rights reserved. The contents from this site may not be reproduced.
The entire risk as to use of these content is assumed by you the user

http://www.steelnumber.com/en/steel_composition_eu.php?name_id=746 2/2