1. The surface to receive the waterproofing shall be cleaned off all dust, dirt, loose
materials, debris, mortar droppings, laitance, oil, grease or any other form of
foreign matter which might affect adhesion and shall be saturated by water
sprinkling in surface driedcondition.
Coving:
1. All the right angle junction between the wall and floors shall be coved with CM 1:3
using Fosroc Nitobond SBR latex @ 1 litre per bag of cement after priming the
area with cement slurry in the Ratio 1:1:3 (SBR: Water:Cement).
1. The bore packing for all the down take pipe shall be need to be properly
prepared to fill non- shrink grout compound Conbextra GP2 mixed with clean
water in the ratio 0.16 after preparing the core concrete surface and
pipecircumference.
2. Priming the concrete surface using Nitobond SBR latex mixed with cement in
slurryconsistency.
1. The slab shall be allowed for hydro testing with minimum 50mm height of water
ponding for 48 hours .
2. Construction joints, cracks and other leaking spots in the concrete surface shall
be drilled and fixed with 18mm dia heavy duty PVC pipe nozzles using Rendroc
Plug at regular intervals of 1m c/c or depending on the siteconditions.
3. It need to be ensured that the reinforcement is not damaged during drillingholes.
4. Construction joint shall be opened to size 20mm X 20mm and filled with
ConbextraGP2.
5. Cement slurry mixed with Cebex 100 free flow non-shrink cementitious
grout at the rate of 225gms per bag of cement shall be prepared to the
required consistency.
6. The prepared slurry shall be injected through the prefixed nozzles under pressure
using grout Pump to fill all possible pores and gaps left within the concretemass.
7. When the flow of grout stops, or when the grout flows out of the adjacent
nozzles, mains shallbe disconnected, nozzles shall be plugged & allowed
to set for 24 hours.
1. preparing the CM1:4 admixed with fosroc conplast wl@150ml per bag of
cement and laying the brickbat in orchid type in half bricks with Avg thickness
of 115mm at slope of (1:150) .spacing between the bricks shall be (20 to
25mm).
2. after laying the brick bats curing should be done for 24 hour and replace the
melted bricks with new bricks .
3. filling the joints with CM 1:3 admixed with conplast wl.
Protective plastering: