You are on page 1of 1

Ast = 1% ϵc fc Pc fs Ps P Δ

L=2000mm 0 0 0 0 0 0 0
f'c = 40 MPa 0.0005 17.5 1575 100 90 1665 1
0.001 30 2700 200 180 2880 2
0.0015 37.5 3375 300 270 3645 3 Comparison of Load - Deflection Behaviour of 40 MPa and 80MPa
0.002 40 3600 400 360 3960 4 concrete in compression
0.0025 37.5 3375 500 450 3825 5
9000 40 MPa
0.003 30 2700 500 450 3150 6
0.0035 17.5 1575 500 450 2025 7 80 MPa
8000

7000

6000

Load in kN
5000

Ast = 1% ϵc fc Pc fs Ps P Δ 4000
L=2000mm 0 0 0 0 0 0 0
3000
f'c = 80 MPa 0.0005 17.56433 1580.79 100 90 1670.79 1
0.001 35.08844 3157.959 200 180 3337.959 2 2000
0.0015 52.20359 4698.323 300 270 4968.323 3
0.002 67.48978 6074.08 400 360 6434.08 4 1000

0.0025 77.81388 7003.25 500 450 7453.25 5 0


0.00283 80 7200 500 450 7650 5.66 0 1 2 3 4 5 6 7 8
0.003 74.12567 6671.31 500 450 7121.31 6 Δ in mm
0.0031 69.1275 6221.475 500 450 6671.475 6.2
0.0032 63.25241 5692.717 500 450 6142.717 6.4
0.0033 56.8202 5113.818 500 450 5563.818 6.6
0.0034 50.18075 4516.268 500 450 4966.268 6.8
0.0035 43.65773 3929.196 500 450 4379.196 7