Material Soaked CBR (%)

Moorum 2.6
20

18
10% FA+90% Moorum 11.3
16
20% FA+80% Moorum 15.6
25% FA+75% Moorum 18 14
30% FA+70% Moorum 10.7

Soaked CBR (%)


12

0 2.6 10
10 11.3
8
20 15.6
25 18 6
30 10.7
4

0
0 5 10 15 20 25 30
FA (%)
Ref: TARGET CBR STRENGTH OF CEMENT
STABILIZED FLYASH-MOORUM SOIL FOR
SUB-BASE

P. Senthilkumar and S. Karthikeyan

5 20 25 30 35
FA (%)