API 650 Requirements:

 All plates shall be manufactured by the open-hearth, electric-furnace, or basic oxygen


process.

 Fully killed plates shall be heat treated to produce grain refinement by either normalizing
or heating uniformly for hot forming.

 The tensile tests shall be performed on each plate as heat treated.

 Carbon equivalent shall be with in code acceptable limits.

 Must meet the impact test requirements of API 650 (if applicable for material thickness)
QE SPECIFICATION ES.5.06.0006 REQUIREMENTS: FOR ANNULAR & SHALL PLATES OF
TANKS WITH TOTAL VOLUME LESS THAN 15000 M3.

 The steel shall contain not more than 0.23% carbon, 0.05% sulphur and 0.05%
phosphorus, as determined by ladle analysis.

 The steel shall have a guaranteed minimum ultimate tensile strength of at least 363 MPa
and a maximum ultimate tensile strength of not more than 510 MPa.

 The steel shall have a guaranteed yield strength of at least 206 MPa.

 The steel shall have an elongation not less than 22%.

General Requirements:
Material certification shall be 3.2