Professional Documents
Culture Documents
Ans-: NO/FALSE
Ans-: 1 Meter
Ans-: 90 Minutes
Ans-: 100x200x300 mm
Ans-: 35 Deg.C
Ans-: 150x300
Ans-: Yes
Q-13: Exposed below ground concrete which type of cement shall use.
Ans-: Type v
Ans-: 150 mm
Ans-: 24 Hours
Q-18: What is the minimum diameter of anchor bolts for fixing ladders.
Ans-: 16mm
Ans-: 12mm
Q-20: What is the minimum distance of anchor bolt from edge of concrete.
Ans-: 100 mm
Ans-: 90%
Ans-: 300mm
Ans-: 6 meters
Ans-: 600 mm
Ans-: 20 mm
Ans-: 70mm
Ans-: 98%
Ans-: Maximum
material.
Ans-: A material is brittle if, when subjected to stress, it breaks with little
elastic deformation and without significant plastic deformation.
Ans-: 10 mm
Civil Engineering Question & Answers
Prepared by: Mohammed Raheel Mustafa
applying?
Q-39: Hot Mix Asphalt Concrete temperature when receiving? Before applying?
concreting operations.
Ans-: SAES-A-114
Ans-: 10 or less
Q-44: Select fill compaction requirement with static load over 320 Kpa.
Q-46: Dense concrete cover of steel substrate shall not be less than 50mm,
what is min. fire resist. rating?
Ans-: 2 hours
Ans-: 370kg
Ans-: 10mm
Ans-: Isolation joints are a gap between the slabs that is typically filled with
and reductions of the adjacent sections and through which some or all of the
Ans-: Spalling is a term used to describe areas of concrete which have cracked
and delaminated from the substrate. There are a number of reasons why
spalling occurs including freeze thaw cycling, the expansive effects of Alkali
Ans-: Minimum fillet weld size shall be 3/16 inch (5 mm) for structural welds
6/22
Q-56: Who will approve if filler plate requirements greater than 1/8 inch (3
mm).
Q-57: Who will repair sags, deformations, holes, and other irregularities.
Ans-: All sags, deformations, holes, and other irregularities shall be repaired
by Erector.
Q-59: Who is responsible for the quality control of all Erector supplied
materials, installations, and workmanship.
Ans-: Erector shall be solely responsible for the quality control of all Erector
Ans-: 150mm
Civil Engineering Question & Answers
Prepared by: Mohammed Raheel Mustafa
Ans-: 20mm
Ans-: 23+-3
Ans-: 5000PSI
Ans-: 150 mm
Ans-: 75 mm
Ans-: No
Ans-: No
Ans-: No
Ans-: 300 mm
Ans-: 150x300mm
Ans-: 1m
Ans-: 1.2m
Q-80: Maximum compaction required for cohesion less material when pressure
above to 320kpa.
Ans-: 85%
Ans-: 711mm
Ans-: L/10
Ans-: 3mm/3m
Ans-: 90 minutes
Ans-: Yes
Ans-: 24 Hours
Ans-: 20mm
Ans-: 12 mm
Ans-: 100 mm
Ans-: 300 mm
Q-96: The select fill material passing through the sieve no.200.
Ans-: In a one-way slab, the main source of load transmission is the longer
Ans-: In the two-way slab, the shorter and larger sides are the main source for
directions.
Ans-104: 96 %
Ans-: 98%
Ans-: 4-7%
Ans-: 0.25L/Sq.m
Ans-: 3mm/m
Ans-: 3500PSI
Ans-: 6 meters
Ans-: 3 years
Ans-: Yes
Ans-: Hazard
Ans-: Metallurgist.
Ans-: 32 deg.
Q-124: What are Standard test methods for determining effects of large
Ans-: Mortar.
Q-129: What is minimum projection of Anchor Bolt above fully engage double
nut.
Ans-: Cement using lightweight aggregate materials rather than gravel and
compacted fill.
Ans-: 28-day compressive strength of CLSM shall be between 0.7 and 1.4 MPa
Ans-: within 3%, plus or minus, of the optimum moisture content as determined
by ASTM D1557.
Q-138: All Select Fill Material and any fill beneath and/or adjacent to
Q-139: Select Fill Material beneath and/or adjacent to foundations with static
loads over 320 kPa and foundations for vibrating or heavy machinery.
Q-141: General Fill Material Compaction requirements for areas not designated
as open or landscaped.
and ASTM D4254 for cohesionless granular soils that do not exhibit well-
defined moisture density relationship.
open or landscaped:
minimum for every 10,000 m3 where the fill material is uniform or for every
The drive-cylinder method per ASTM D2937 may only be used if the compacted
Ans-: 1. Select Fill Material under all foundations, buildings and process areas
2. Select Fill Material under roadways, railroads, area pavement and parking
areas, and lined slopes or drainage channels - one test every 200 m² of each
lift.
Backfill inches - one test for every 15 linear meters of each lift.
Ans-: Fixed reinforced concrete, for service in deeper waters far from the
shoreline.
Ans-: Below floor vapor barrier shall be in accordance with ASTM E1745,
and minimum 10 mil (250 µm) thickness unless otherwise specified in contract
documents.
Q-154: Areas subject to spills, wash water, fire water and sidewalk paved
Ans-: Areas subject to spills, wash water, fire water and sidewalk shall be
paved with a minimum thickness of 100 mm of reinforced concrete.
compressive strength.?
Civil Engineering Question & Answers
Prepared by: Mohammed Raheel Mustafa
Q-157: Concrete shall be placed in accordance with ............ for hot weather
concreting requirements.
Ans-: Concrete shall be placed in accordance with ACI 301-16, ACI 304R and
SAES-Q-001.
Ans-: ACI 301-16 and ACI 117 unless otherwise specified in the construction
Ans-: For curing shall not exceed 1,000 ppm (parts per million).
Q-160: Water curing shall be continuous until the compressive strength has
reached.?
Ans-: Compressive strength has reached 70% of the specified strength, but not
Q-161: The saturated burlaps shall be covered with a plasticized sheet vapor
comply with..........?
Ans-: The provisions of ACI 350.5 and Curing shall occur for a minimum of 14
days.
Q-163: Minimum concrete cover in sulfur pits shall not be less than?
Ans-: 75mm
Ans-: Cement using lightweight aggregate materials rather than gravel and
Q-167: Silica fume, when used as replacement for cement in concrete (binary
mix), shall not be less than 7% and shall not exceed 10% by weight of
cementitious material.
pozzolans.
Q-169: Fly ash can be used as partial replacement for cement in concrete
(binary or ternary mix) for durability purposes. The amount of fly ash shall not
be less than 25% by weight of cementitious material.
Q-170: Ground Granulated Blast Furnace Slag (GGBFS) can be used as partial
purposes. The amount of GGBFS shall not be less than 50% and shall not
exceed 70% by weight of cementitious material.
Q-171: The maximum water-soluble chloride ions in concrete shall not exceed
0.15% for reinforced concrete and 0.06% for prestressed concrete by weight
of cement. The maximum Sulfate ions as SO3 shall not exceed 4%. Tests shall
be in accordance with ASTM C1218/C1218M, BS 1881 - 124 or equivalent.
Q-173: Complete concrete mix design data shall be submitted to the Purchaser
have a target or nominal slump of 150 mm, (±40 mm) at the point of discharge
at the job site or otherwise specified.
Q-175: For self-consolidated concrete (SCC), concrete slump flow shall be....
Ans-: Concrete with Ultra High Range Superplasticizer admixtures shall have
a target or nominal slump flow of 600 mm, (±65 mm) at the point of discharge
at the job site or otherwise specified.
Ans-: Plant scales shall be calibrated no less than three times a year and shall
be certified as conforming to ASTM C94/C94M - 17a by Saudi Aramco approved
calibration agency.
Q-177: Test reports shall be submitted within .... days after tests are
completed.
Ans-: Test reports shall be submitted within 7 days after tests are completed.
Test one set of laboratory-cured specimens at 7 days and one set of specimens
at 28 days. Additional test of one set at 56 days for concrete containing natural
Test one set of field-cured specimens at 7 days and one set of specimens at
28 days. Additional test of one set at 56 days for concrete containing natural
sample per 200 m³ of aggregate to be shipped, but not less than one sample
per month.
Ans-: Coarse aggregates can be cleaned from dust in order to meet Table A by
water, vacuum suction or air blast. Total dissolved solids in the washing water
shall not exceed 3500 ppm and chlorides shall not exceed 1000 ppm
Q-181: Size of Core Test or Specimens if aggregate size is less then 9.5mm.
Ans-: 50mm/50mm
Ans-: 85%