Professional Documents
Culture Documents
PRESENTED BY : GUIDED BY :
NAME : MD IRFAN DR. MIR IQBAL FAHEEM
ROLL NO : 160319741404 PROFESSOR & HEAD OF CIVIL ENGG . DEPT
ME-CIVIL-TRANSPORTATION ENGG
1
CONTENTS
The goal of pavement design is to determine the number,
material composition and thickness of the different layers within
a pavement structure required to accommodate a given loading
regime. Pavement is most important component of highway
section. Therefore the overall functioning of highway system is
greatly relying on performance of its pavement. Pavement is a
multilayer system that distributes the vehicular loads over a
larger area. Pavement is the upper part of roadway, airport or
parking area structure. It includes all layers resting on the original
ground. It consists of all structural elements or layers, including
shoulders.
LITERATURE REVIEW
Flexible pavements are those which are surfaced with bituminous or asphalt materials.
These types of pavements are called “flexible” since the total pavement structure
“bends” or “deflects” due to traffic loads. A flexible pavement structure is generally
composed of several layers of materials which can accommodate this “flexing” Flexible
pavements comprise more than 90 percent of our paved roads.
Flexible pavements are layered systems that can be analyzed with Burmister’s layer
theory. Flexible pavements structure composed of several layers of materials which
transfers load to the sub grade without failure. These layered systems have quality
materials on the top where stresses are high and low quality materials sit in bottom. The
top layer materials which are bituminous mixes are temperature sensitive and their
properties i.e. elastic modulus and Poisson ratio change with temperature change. It
covers three of the more common types of the Hot Mixes Asphalt (HMA) mixes types
commonly used: other flexible pavements such as bituminous surface treatments (BSTs)
are considered by most agencies. HMA mix types differ from each other mainly in
maximum aggregate size, aggregate gradation and asphalt binder content or type.
It is important to account for temperature while analyzing flexible pavements with thick
bitumen mixed Indian road design are semi empirical, based on load repetitions in terms
of standard axle load (MSA) and CBR of the sub grade. The temperature considered for
pavement design is 35*C as an AAPT for whole country.
SCOPE AND OBJECTIVE OF THE PROJECT
OBJECTIVE
The main objectives of this study are as follows
To provide most economical crust suitable to the projected traffic and design
period in accordance with IRC 37-2012.
Widening the existing (3.5/5.5m) carriageway to 7m carriageway with
earthen shoulders.
SCOPE
Scope of this study is limited to
Investigation required for finding design input criteria like CBR value of soil
sub grade, existing crust thickness, present traffic, expected traffic for the
design period.
Design of crust in central carriageway as well as for the widening portion in
the specified stretch of the road.
NEED OF THE PROJECT
What is pavement ?
A structure consisting of superimposed layers of
processed materials above the natural soil sub-
grade, whose primary function is to distribute the
applied vehicle loads to the sub-grade.
7
Types of Pavement
PAVEMENT
8
Flexible pavement:
9
Load transfer:
10
Load Transfer
The wheel load acting on the pavement will be
distributed to a wider area, and the stress decreases
with the depth. Flexible pavement layers reflect the
deformation of the lower layers on to the surface
layer
11
TYPICAL LAYERS OF A FLEXIBLE PAVEMENT :
Typical layers of a conventional flexible pavement
includes seal coat, surface course, tack coat,
binder course, prime coat, base course, sub-base
course, compacted sub-grade, and natural sub-
grade.
12
TYPICAL LAYERS OF A FLEXIBLE PAVEMENT
13
TYPICAL LAYERS OF A FLEXIBLE PAVEMENT
14
TYPICAL LAYERS OF A FLEXIBLE PAVEMENT
15
FACTORS AFFECTING PAVEMENT DESIGN
16
Design Wheel Load.
17
Design Wheel Load
18
Design Wheel Load
Equivalent single wheel load
(ESWL)
19
Design Wheel Load
Repetition of loads :
1. Temperature -
Wide temperature variations may cause damaging
effects.
Pavement becomes soft in hot weather and brittle in
very cold weather.
21
Characteristic of Pavement material
1. California bearing ratio- It determines the strength
of soil sub-grade, sub-base or base and it is used for
the design of pavement.
2. Elastic modulus -It measures the materials
resistance to being deformed elastically
upon application of the wheel load.
3. Poisson Ratio – It is the ratio of lateral strain to the
axial strain caused by a load parallel axis along
axial strain.
4. Resilient modulus- The elastic modulus based on
the recoverable strain under repeated loads is
called the resilient modulus MR =σd/σr .
22
Characteristic of Pavement material
The following material properties are consider for
both flexible and rigid pavements.
When pavements are considered as linear elastic,
the elastic moduli and poisson ratio are specified.
23
Design procedures for flexible pavements:
Design Procedures
Mechanistic- Mechanistic
Empirical Design
Empirical Design Design
24
Mechanistic-empirical design
25
Failures of flexible pavements:
Different types of failure encountered in flexible
pavements are as follow.
1. Alligator cracking or Map cracking (Fatigue)
2. Consolidation of pavement layers (Rutting)
3. Shear failure cracking
4. Longitudinal cracking
5. Frost heaving
6. Lack of binding to the lower course
7. Reflection cracking
8. Formation of waves and corrugation
9. Bleeding
10. Pumping
26
1. ALLIGATOR OR MAP CRACKING
(FATIGUE CRACKING)
Followings are the primary causes of
this type of failure.
27
2. CONSOLIDATION OF PAVEMENT
LAYERS (RUTTING)
Formation of ruts falls in this
type of failure.
A rut is a depression or
groove worn into a road
by the travel of wheels.
This type of failure is caused
due to following reasons.
•Repeated application of
load along the same
wheel path resulting
longitudinal ruts.
•Wearing of the surface
course along the
wheel path resulting
shallow ruts.
28
3. SHEAR FAILURE CRACKING:
29
4. LONGITUDINAL CRACKING:
This types of cracks extents to
the full thickness of pavement.
30
5. FROST HEAVING:
Frost causes
heaving
upheaval of localized
portion a pavement.
of Theextent of frost
heaving depends upon
the ground water
and climatic condition.
table
31
6. LACK OF BINDING WITH LOWER LAYER
(POTHOLES & SLIPPAGE)
When there is lack of
binding between surface
course and underlying
layer, some portion of
surface course looses up
materials creating patches
and potholes.
Slippage cracking is one
form of this type of failure.
Lack of prime coat or tack
coat in between two layers
is the primary reason
behind this type of failure.
32
7. REFLECTION CRACKING:
This type of failure
occurs, when
bituminous surface
course is laid over the
existing cement
concrete
with some cracks.
pavement
This
crack is reflected in
the pattern on
same
bituminous surface.
33
8. FORMATION OF WAVES &
CORRUGATION :
Transverse
undulations appear
at regular intervals
due to the unstable
surface course
caused by stop-and-
go traffic.
34
9. BLEEDING:
Excess bituminous
binder occurring on the
pavement surface
causes bleeding.
Bleeding causes a shiny,
glass-like, reflective
surface that may be
tacky to the touch.
Usually found in the
wheel paths.
35
10. PUMPING:
Seeping or ejection
of water and fines
from beneath the
pavement through
cracks is called
pumping
36
FAILURES OF FLEXIBLE PAVEMENTS
DESIGN CONSIDERATION:
37
IRC METHOD OF DESIGN OF FLEXIBLE
PAVEMENTS (IRC: 37-2012)
1. IRC:37-1970
based on California Bearing Ratio (CBR) of subgrade
Traffic in terms of commercial vehicles (more than
3 tonnes laden weight)
2. IRC:37-1984
based on California Bearing Ratio (CBR) of subgrade
Design traffic was considered in terms of cumulative
number of equivalent standard axle load of 80 kN
in millions of standard axles (msa)
Design charts were provided for traffic up to 30 msa
using
an empirical approach.
.
38
3. IRC:37-2001
based on Mechanistic-Empirical method
Pavements were required to be designed for traffic as
high as 150 msa.
The limiting rutting is recommended as 20 mm in 20 per
cent of the length for design traffic
4. IRC:37-2012
based on Mechanistic-Empirical method
The limiting rutting is recommended as 20 mm in 20 per
cent of the length for design traffic up to 30 msa and
10 per cent of the length for the design traffic beyond
39
Guidelines for Design by IRC: 37: 2012
Design Traffic:
The recommended method considers design traffic
in terms of the cumulative number of standard axles
(80 kN) to be carried by the pavement during the
design life.
Only the number of commercial vehicles having
gross vehicle weight of 30 kN or more and their axle-
loading is considered for the purpose of design of
pavement.
Assessment of the present day average traffic
should be based on seven-day-24-hour count
made in accordance with IRC: 9-1972 "Traffic
Census on
36 Non-Urban Roads".
What is design ?
41
Various cases in design.
42
Data collection
Material properties :
43
Calculation of Design factor
1) Design Traffic,
2) Axle load survey,
3) Vehicle Damage Factor
4) Lane Distribution
Factor
44
Design Traffic:
45
Traffic count
Assessment of average daily traffic should be normally
based on 7 day-24hr count made in accordance with
IRC: 9 “Traffic census on non-urban roads”.
Classify traffic into different categories such as two
wheelers, three wheelers, passenger cars, trucks etc.
But only commercial vehicle with laden weight > 3 tonne
is taken into consideration of design.
Commercial vehicles are further categorised as single
axle single wheel, single axel dual wheel, Tandem axle
dual wheel and Tridem axle dual wheel.
Where no traffic count data is available, data from roads
of similar classification and importance may be used to
predict the design traffic
46
Traffic growth rate (r):
Estimated by Analyzing:
The past trends of traffic growth,
47
Design life (n)
48
Vehicle damage factor (VDF)
It is defined as equivalent number of standard axles
per commercial vehicle.
The Vehicle Damage Factor (VDF) is a multiplier to
convert the number of commercial vehicles of
different axle loads and axle configuration into the
number of repetitions of standard axle load of
magnitude 80 kN.
49
50
Vehicle Damage factor
Were sufficient information on axle loads are not
available or the small size of project does not
warrant an axle load survey the default values
of VDF may be adopted as given in the table
given
below
.
51
Example on VDF:
52
Sample Size for Axle Load Survey:
53
Axle load spectrum
Single Axle Load Tandem Axle Load Tridem Axle Load
Axle load Class Percentage of Axle load Class Percentage of Axle load Class Percentage of
(KN) Axles (KN) Axles (KN) Axles
54
Lane distribution factor
Distribution of commercial traffic in each direction
and in each lane is required for determining the total
equivalent standard axle load applications to be
considered in the design.
55
Lane distribution calculation:
1) Single-lane roads:
56
Lane distribution
Distribution of commercial traffic in each direction
and in each lane is required for determining the total
equivalent standard axle load applications to be
considered in the design.
Single lane road : Total vehicle in both direction.
Two lane single carriage way : 50% of total vehicle in
both direction.
Four lane single carriage way : 40% of total vehicle
in both direction.
Dual carriage way:Two lane 75%, Three lane 60%,
Four lane 45% of number of CV in each direction.
57
Computation of Design traffic:
The design traffic in terms of the cumulative number
of standard axles to be carried during the design
life of the road should be computed using the
following equation:
58
Sub-grade
Requirements of CBR: Sub grade is made up of in-
situ material, select soil or stabilized soil.
Compacted to a minimum of 97% of laboratory dry
density achieved with heavy compaction.
Minimum CBR of 8% for traffic > 450 CVPD
CBR can also be determined from Dynamic
Cone Penetrometer (60º cone) by ..
Log10 CBR = 2.465-1.12log10 N
Where, N = mm/blow
59
Sub-grade
Where different types of soils are used in sub grade
minimum 6 to 8 average value for each type is required.
90th percentile for high volume and 80th percentile for
other category of road is adopted as design CBR .
Maximum permissible variation
60
Effective CBR
Where there is significant difference between the
CBRs of the select sub grade and embankment
soils, the design should be based on effective CBR.
The effective CBR of the subgrade can be
determined from
Fig.
61
Lab procedure for CBR calculation:
63
Resilient Modulus:
Resilient modulus is the measure of its elastic
behavior determined from recoverable
deformation in the laboratory tests.
The modulus is an important parameter for
design and the performance of a pavement.
The relation between resilient modulus and the
effective CBR is given as:
64
The CBR of the sub-grade should be determined
as per IS: 2720 (Part 16) (36) at the most critical
moisture conditions likely to occur at site.
65
Principle of pavement design:
Pavement Model:
67
Check for Fatigue
Two fatigue equations developed based on
performance data collected during various study
are
Nf= 2.21 * 10-04x [1/εt]3.89* [1/MR]0.854 (80 %
reliability)…(a)
Nf= 0.711 * 10-04x [1/εt]3.89* [1/MR]0.854 (90 %
reliability)...(b)
Where,
Nf= fatigue life in number of standard axles,
εt= Maximum Tensile strain at the bottom of
the
bituminous layer, and
Equation for 90%modulus
MR= resilient reliability
of implies that only 10% of
the bituminous
the pavement area will have more than 20 % cracks.
layer.
63
Check for Fatigue
To consider the effect of volume of the bitumen and air
voids equation (b) is modified as follows
Nf =0.5161 * C * 10-04 x [1/ εt]3.89 * [1/MR]0.854………(c)
Va= per cent volume of air void and Vb= per cent volume
of bitumen in a given volume of bituminous mix.
Nf= fatigue life, єt= maximum tensile strain at the bottom
of DBM.
MR= Resilient modulus of bituminous mix.
For traffic < 30 msa consider equation (a); For traffic >
30msa equation (c) is recommened.
69
Check for Rutting:
Rutting is the permanent deformation in pavement
usually occurring longitudinally along the wheel
path.
Causes –
1. Deformation in sub grade /non-bituminous layer
2. Secondary compaction and shear deformation of
bituminous layer
Limiting value
20 mm in 20% length for upto 30 msa
20 mm in 10% length for > 30 msa
Rutting affects the serviceability of pavement.
70
Rutting
Based on various studies the two equation
develops are;
Where,
N = Number of cumulative standard axles, and
εv= Vertical strain in the sub-grade
71
Pavement composition as per IRC:
A flexible pavement covered in these
guidelines consists of different layers as
shown in figure;
72
SUB-BASE LAYER
UNBOUND SUB-BASE LAYER
Sub-base materials may consist of natural sand,
moorum, gravel, laterite, kankar, brick metal,
crushed stone, crushed slag
Sub-base materials passing 425 micron sieve when
tested in accordance with IS:2720 (Part 5) should
have liquid limit and plasticity index of not more than
25 and 6 respectively.
73
SUB-BASE LAYER(Unbound SB)
When coarse graded sub-base is used as a
drainage layer, Los Angeles abrasion < 40
Required permeability; fines passing 0.075
mm should be less than 2 per cent.
Sub-base is constructed in two layers, the lower
layer forms the separation/filter layer to prevent
intrusion of subgrade soil into the pavement and the
upper GSB forms the drainage layer to drain away
any water
Resilient modulus (MR) for granular sub-base
MRgsb = 0.2 h0.45 * MR subgrade
Where, h = thickness of sub-base layer in
74mm
SUB-BASE LAYER
Bound Sub base
Material for bound sub-base may consist of soil,
aggregate or soil aggregate mixture modified with
chemical stabilizers such as cement, lime-flyash.
The drainage layer of the sub-base may consist of
coarse graded aggregates bound with about 2
per cent cement while retaining the permeability.
Drainage and separation layers are essential
when water is likely to enter into pavements from
the shoulder, median or through the cracks in
surface layer.
75
SUB-BASE LAYER(Unbound SB)
Strength Parameter:
Elastic Modulus E of bound sub-
bases is
Ecgsb = 1000 * UCS
Where UCS = 28 day strength of the
cementitious granular material
76
BASE LAYER
UNBOUND BASE LAYER
Base layer may consist of wet mix macadam, water
bound macadam, crusher run macadam,
reclaimed concrete etc.
Resilient modulus of the granular base is given as..
MR granular = 0.2 * h0.45 MR subgrade
Where h = thickness of granular sub-base and base,
mm
Poisson's ratio of granular bases and sub-bases
is recommended as 0.35.
77
BASE LAYER
CEMENTITIOUS BASES :
Cemented base layers may consist of aggregates or
soils or both stabilized with chemical stabilizers, to
give a minimum strength of 4.5 to 7 MPa in 7/28
days.
Default values of modulus of rupture are
recommended for cementitious bases (MEPDG).
Cementitious stabilized aggregates 1.40 MPa
- 1.05 MPa
Lime—flyash-soil -
0.70 MPa
Soil cement -
Poisson's ration of the cemented layers may
be taken as 0.25.
78
Criteria for selecting Bitumen grade.
The recommended resilient modulus values of
the bituminous materials with different binders
are:
79
Poisson’s ratio
Poisson’s ratio µ is define as the ratio of lateral strain
(ɛl) to the axial strain (ɛa), caused by load parallel to
the axis along which ɛa is measured.
It is found that for most of the pavement structures,
the influence of µ value is normally small.
For most of cement treated materials (soil cement,
cement treated base, lean concrete and PCC),
the value of µ normally lies between 0.10 and
0.25.
Unbound granular material lie between 0.2 and 0.5
and those for bituminous mixes range from 0.35
to 0.50
80
The Poisson’s ratio of bituminous layer depends upon the
pavement temperature and a value of 0.35 is
recommended for temperature up to 35°C and value of
0.50 for higher temperatures.
Higher viscosity of bituminous binders, which can be
achieved either by using higher viscosity grade bitumen
or modified bitumen will improve both fatigue and rutting
behavior of mixes as compared to mixes with normal
bitumen.
Fatigue equation at any pavement temperature from
20°C to 40°C can be evaluated by substituting the
appropriate value of the resilient modulus of the
bituminous mix, air void and volume of bitumen.
Catalogue of designs has been worked out for a
temperature of 35°C.
81
Drainage Layer
82
Drainage Layer
Some typical drainage system is illustrated in
following Figs….
Fig.1 Pavement along a Slope
83
Drainage Layer
Fig. 2 Pavement with Filter and Drainage
Layers
84
Drainage Layer
Criteria to be satisfied:
The filter/separation layer should satisfy the
following
criteria:
85
Hydraulic gradient = [Elevation drop/ length
AD]
86
Design check
To check the suitability of pavement design
discussed above we carry out checks, which
ensure safety against the failure of designed
pavement.
The flexible pavement is checked for two types
of failures i.e. Rutting in pavement and Fatigue
in bottom layer of bituminous surfacing.
The following condition should be satisfied for the
design to be satisfactory
Design strain < Allowable
strain
Allowable strain = Obtained by fatigue model and
87 rutting model
(Decide grade by using table)
% Passing
Sieve
Grading 1 Grading 2 Grading 3 Grading 4 Grading 5 Grading 6
Opening,
Mm
20 100 100 100 100 100 100
12.5 85 84 83 81.5 79.5 75
9.5 77.5 76 74 72.5 69.5 63
4.76 58.3 56 52.5 49 43.5 32
2.36 42.5 39 34 29.5 22 5.8
2.00 39 35 30 25 17 0
0.84 26.5 22 15.5 9.8 0 0
0.42 18.2 13.3 6.3 0 0 0
0.25 13.0 7.5 0 0 0 0
0.10 6 0 0 0 0 0
0.075 0 0 0 0 0 0
Coeff. Of
permeability 3 35 100 350 850 950
m/day
88
Recommendations
Specifications should be modified according to local
condition. In wet climate wearing course should be
impermeable.
long duration and low intensity rainfall causes
more damage as compare with rainfall of small
duration and more density.
If DBM and SDBC/BC are designed properly (4%
air voids and protected shoulder) impermeably can
be ensure.
Adequate provision for sub-surface drainage prevent
pavement damage.
89
Thickness charts with BC/ SDBC are valid for
all rainfall area.
For pavement carrying heavy traffic wearing course
laid over WBM shows better performance.
For low traffic (upto 5 msa) bitumen surfacing with
two coats is found to be suitable.
90
Conclusion
Time to time revisions of code provision are needed
keeping in view changes in traffic pattern and
development of new technologies. Further with the
gain of experience in the design as well as
construction procedure of flexible pavement have
demanded certain changes.
Hence by considering the above factors IRC:
37: 2012 includes some conceptual changes in
the design of flexible pavement such as
inclusion of Resilience moduli and
consideration of strain in design.
91
This code also encourages the use IIT pave
software which is newly recommended.
Since the use of semi-mechanistic approach, the
design is not only based on the experience but it
also gives parameters (strain parameter) to
check the obtained design.
Solution to the above pavement design problem
shows that the thickness design varies with the
variation in various factors.
92
References
93
Thank you .
94