Topcoat Hempel Paints (Saudi Arabia) W.L.L. Hempels Silvium 51570 1000196402
1.
2.
Mixing 2.1 2.2 2.3 No. of Components Mixing Ratio Thinner SAMS S/N 2.4 2.5 2.6 Thinning Requirements Induction Time Pot Life : : : : : : : 1 N/A N/A N/A Nil N/A N/A
3.
Application 3.1 3.2 3.3 3.4 Maximum Allowable Substrate Temperature Typical Wet Film Thickness Per Coat Typical Dry Film Thickness Per Coat Theoretical Coverage @ 25 Micrometers Dry Film Thickness Minimum Number of Coats : : : : 50C 65 micrometers 25 micrometers 15.2 m/l
3.5
Manufacturer - Approved Saudi Aramco Data Sheet APCS-4 Topcoat Hempels Silvium 51570 (Cont'd)
3.6
Drying Time Substrate Temperature 10C 30C 50C Recoat Interval Minimum Maximum 18 hours 5 hours 2 hours None None None
3.7
Recommended Equipment Airless Spray : Tip size: 0.017 inch Fluid pressure: 1.500 psi N/A For touch up only
Conventional Spray Brush 4. Technical Properties 4.1 4.2 4.3 4.4 4.5 Volume Solids Product Weight Viscosity Flash Point Gloss (ASTM D2697) (ASTM D1475) (ASTM D562) (ASTM D93 or D56) (ASTM D523)
: :
: : : : :