DESCRIPTION OF METHOD

1.

HANDY TOOL.
BOON FOR PRESENT DAY.

2.

MATERIAL REQUIRED

1.

PERMA RECRETE POWDER.


QUARTZ AGGREGATE.
WATER.

2.
3.

APPROPRIATE STEPS FOR


SFMC
1. VISUAL INSPECTION.

2. BREAKING OF PLASTER
& CONCRETE.

SUPER FLUID MICRO


CONCRETE
3. SURFACE
PREPERATION.
RUSTING & PITTING.
WIRE BRUSHING.
CLEANING.
WASHING.
APPLING ACETONE.

SUPER FLUID MICRO


CONCRETE
4. APPLICATION OF
PROTECTION COAT
POLYCON : CEMENT
1 : 1.5
BY VOLUME

SUPER FLUID MICRO


CONCRETE
5. ERECTION OF
FORMWORK
12MM THICK POST BOX TYPE
MARINE PLYWOOD FORMWORK.

SUPER FLUID MICRO


CONCRETE
6. REINSTATE THE AREA
WITH SFMC
PERMA RECRETE POWDER :1KG
QUARTZ AGGREGATE
: 0.75KG
WATER
: 180
TO
200ML

SUPER FLUID MICRO


CONCRETE
7. COMPACTION
8. REMOVATION OF FORMWORK
9. HACKING & CURING
10. APPLICATION OF SAND FACED
PLASTER

SUPER FLUID MICRO


CONCRETE

CONCRETE SURFACE
BUILT UP TO
ORIGINAL.

SUPER FLUID MICRO


CONCRETE

CHECK LIST

1.

CONCRETE SURFACE SHOULD BE DAMPENED.


SHUTTER FORMS SHOULD BE SEALED.
SIZE OF COARSE AGGREGATE SHOULD BE 510MM.
REPAIRED SURFACE SHOULD BE HACKED.
FORMWORK SHOULD BE TIGHT.
TAMPING SHOULD BE PROPER.

2.
3.
4.
5.
6.

SUPER FLUID MICRO


CONCRETE

APPROPRIATION OF SFMC

1.

VERY HIGH WORKABILITY.


VERY HIGH STRENGTH.
VERY STRONG BOND.
NO NEED OF ELABORATE CURING.
LOW MATERIAL EXPENDITURE.

2.
3.
4.
5.

SUPER FLUID MICRO


CONCRETE

CONCLUSION:

1. SFMC IS A VERSATILE TREATMENT.


2. CORROSION IS AVOIDED.
3. STRUCTURAL MEMBER REFILLED AS
PARENT CONCRETE.
4. STRENGTH & APPEARANCE AS THE
ORIGINAL ONE.