You are on page 1of 1

PT. MULTI FABRINDO GEMILANG DOCUMENT NO.

PROCEDURE MANUAL MFG-DOC-3500


REPAIR NOZZLE PROCEDURE PAGE REVISION
1 OF A

1. SCOPE

1.1. This procedure describes step of repair nozzle miss tolerance.

2. REFERENCE
2.1 ASME Section IX 2019 Edition
2.2 Fabrication procedure

3 TOOLS
3.1 Water pass.
3.2 Tape
3.3 Rose Head Burner
3.4 Tempered Stick
3.5 IR Gun (If Available)

4 PROCEDURE
4.1 Carbon Steel
4.1.1 Check dimensional of nozzle, how far and orientation of nozzle out of
tolerance.
4.1.2 Burn using Rose head burner at the other side of tilted nozzle orientation.
4.1.3 Fitter must control the temperature using tempered stick or IR Gun.
4.1.4 After Burn for a while, re-check the dimensional.
4.1.5 Repeat step 3.2 and 3.4 until the Nozzle orientation fit the tolerance

4.2 Stainless Steel


4.2.1 For stainless steel avoid using burner for a miss direction more than 5
mm (≥5 mm)
4.2.2 For intolerance more than 5 mm (≥5 mm), perform re weld to fix the
intolerance.